Abstract

Abstract There is disclosed an aqueous medium comprising water to which has been added a water thickening amount of a water thickening polymer which is prepared by polymerizing at least one alkyl acrylate monomer and at least one carboxylic polymerizable monomer selected from the group consisting of acrylic acid and methacrylic acid which are present from 20 to 95 parts by weight per hundred parts of total monomer being polymerized and utilizing, as an ionic emulsifier, an emulsifier selected from the group consisting of disodium or diammonium nonylphenoxy polyethoxy sulfosuccinate having the general formula: CH.sub.3 (CH.sub.2).sub.8 C.sub.6 H.sub.4 O(CH.sub.2 CH.sub.2 O).sub.8-16 COCH 2 CH(COOM)SO 3 Q wherein Q is sodium or ammonium and a sodium or ammonium lauryl polyethoxysulfate having the general formula: CH.sub.2 (CH.sub.2).sub.11 O(CH.sub.2 CH.sub.2 O).sub.8-16 SO.sub.3 Q wherein Q is sodium or ammonium, said polymer in latex form being neutralized to a pH ranging between a pH of 5.5 to 11.5. Such polymers may also be gelled with water soluble polyvalent compounds such as sodium dichromate and water soluble reducing agents such as sodium hydrosulfite. The aqueous gels are employed in enhanced oil recovery.

Inventors

  • 👤 Daniel F. Klemmensen
  • 👤 Richard G. Bauer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 00:47
CPC Classifications
C; C09; C09K; C09K8/00; C09K8/60; C09K8/84; C09K8/86; C09K8/88; C09K8/887; C08; C08F; C08F220/00; C08F220/02; C08F220/04; C08F220/10; C08F220/12; C09K8/50; C09K8/504; C09K8/506; C09K8/508; C09K8/512; C09K8/58; C09K8/588; Y; Y10; Y10S; Y10S507/00; Y10S507/935; Y10S507/936; Y10S524/00; Y10S524/914

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 149 words
An aqueous medium comprising water to which has been added a water thickening amount of a water thickening polymer which is prepared by polymerizing at least one alkyl acrylate monomer and at least one carboxylic polymerizable monomer selected from the group consisting of acrylic acid and methacrylic acid which are present from 20 to 95 parts by weight per hundred parts of total monomer being polymerized and utilizing, as an ionic emulsifier, an emulsifier selected from the group consisting of disodium or diammonium nonylphenoxy polyethoxy sulfosuccinate having the general formula: CH.sub.3 (CH.sub.2).sub.8 C.sub.6 H.sub.4 O (CH.sub.2 CH.sub.2 O).sub.8-16 COCH.sub.2 CH(COOM)SO.sub.3 Q wherein Q is sodium or ammonium and a sodium or ammonium lauryl polyethoxysulfate having the general formula: CH.sub.2 (CH.sub.2).sub.11 O(CH.sub.2 CH.sub.2 O).sub.8-16 SO.sub.3 Q wherein Q is sodium or ammonium, said polymer in latex form being neutralized to a pH ranging between a pH of 5.5 to 11.5.
Claim 2
Dependent Claim 149 words
An aqueous medium comprising water to which has been added a water thickening amount of a water thickening polymer which is prepared by polymerizing at least one alkyl acrylate monomer and at least one carboxylic polymerizable monomer selected from the group consisting of acrylic acid and methacrylic acid which are present from 20 to 95 parts by weight per hundred parts of total monomer being polymerized and utilizing, as an ionic emulsifier, an emulsifier selected from the group consisting of disodium or diammonium nonylphenoxy polyethoxy sulfosuccinate having the general formula: CH.sub.3 (CH.sub.2).sub.8 C.sub.6 H.sub.4 O (CH.sub.2 CH.sub.2 O).sub.8-16 COCH.sub.2 CH(COOM)SO.sub.3 Q wherein Q is sodium or ammonium and a sodium or ammonium lauryl polyethoxysulfate having the general formula: CH.sub.2 (CH.sub.2).sub.11 O(CH.sub.2 CH.sub.2 O).sub.8-16 SO.sub.3 Q wherein Q is sodium or ammonium, said polymer in latex form being neutralized to a pH ranging between a pH of 5.5 to 11.5.
Claim 3
Dependent Claim 32 words
An aqueous medium according to claim 1 in which the water thickening polymer is employed in amounts ranging from 0.05 to about 2% by weight based on the weight of the water.
Claim 4
Dependent Claim 41 words
An aqueous medium according to claim 1 in which the acrylic acid or methacrylic acid are present in the water thickening polymer in an amount varying from about 55 to about 75 parts per hundred parts of total monomer being polymerized.
Claim 5
Dependent Claim 25 words
An aqueous medium according to claim 1 in which said polymer has been neutralized to a pH ranging between a pH of 6.5 to 8.5.
Claim 6
Dependent Claim 32 words
An aqueous medium according to claim 2 in which the amount of water thickening polymer ranges from about 0.1 to about 0.5 percent by weight based on the weight of the water.
Claim 7
Dependent Claim 262 words
An aqueous medium comprising water to which has been added a water thickening amount of a water thickening polymer which is prepared by polymerizing at least one alkyl acrylate monomer and at least one carboxylic polymerizable monomer selected from the group consisting of acrylic acid and methacrylic acid which are present from 20 to 95 parts by weight per hundred parts of total monomer being polymerized and utilizing, as an ionic emulsifier, an emulsifier selected from the group consisting of disodium or diammonium nonylphenoxy polyethoxy sulfosuccinate having the general formula: CH.sub.3 (CH.sub.2).sub.8 C.sub.6 H.sub.4 O(CH.sub.2 CH.sub.2 O).sub.8-16 COCH.sub.2 CH(COOM)SO.sub.3 Q wherein Q is sodium or ammonium and a sodium or ammonium lauryl polyethoxysulfate having the general formula: CH.sub.2 (CH.sub.2).sub.11 O(CH.sub.2 CH.sub.2 O).sub.8-16 SO.sub.3 Q wherein Q is sodium or ammonium, said polymer in latex form being neutralized to a pH ranging between a pH of 5.5 to 11.5 and containing from about 1 to about 200 weight percent of a water soluble compound of a polyvalent metal selected from the group consisting of chromium compounds in which the chromium has a valence of +6 which is capable of being reduced to a lower valent state of +3 and manganese compounds in which the manganese has a valence of +7 and which is capable of being reduced to a lower valent state of +4 and from about 1 to about 200 weight percent of a water soluble reducing agent, based on the weight of said polymer, which is effective to reduce at least a portion of said metal to said lower valent state.
Claim 8
Dependent Claim 262 words
An aqueous medium comprising water to which has been added a water thickening amount of a water thickening polymer which is prepared by polymerizing at least one alkyl acrylate monomer and at least one carboxylic polymerizable monomer selected from the group consisting of acrylic acid and methacrylic acid which are present from 20 to 95 parts by weight per hundred parts of total monomer being polymerized and utilizing, as an ionic emulsifier, an emulsifier selected from the group consisting of disodium or diammonium nonylphenoxy polyethoxy sulfosuccinate having the general formula: CH.sub.3 (CH.sub.2).sub.8 C.sub.6 H.sub.4 O(CH.sub.2 CH.sub.2 O).sub.8-16 COCH.sub.2 CH(COOM)SO.sub.3 Q wherein Q is sodium or ammonium and a sodium or ammonium lauryl polyethoxysulfate having the general formula: CH.sub.2 (CH.sub.2).sub.11 O(CH.sub.2 CH.sub.2 O).sub.8-16 SO.sub.3 Q wherein Q is sodium or ammonium, said polymer in latex form being neutralized to a pH ranging between a pH of 5.5 to 11.5 and containing from about 1 to about 200 weight percent of a water soluble compound of a polyvalent metal selected from the group consisting of chromium compounds in which the chromium has a valence of +6 which is capable of being reduced to a lower valent state of +3 and manganese compounds in which the manganese has a valence of +7 and which is capable of being reduced to a lower valent state of +4 and from about 1 to about 200 weight percent of a water soluble reducing agent, based on the weight of said polymer, which is effective to reduce at least a portion of said metal to said lower valent state.
Claim 9
Dependent Claim 32 words
An aqueous medium according to claim 6 in which the water thickening polymer is employed in amounts ranging from 0.05 to about 2% by weight based on the weight of the water.
Claim 10
Dependent Claim 41 words
An aqueous medium according to claim 6 in which the acrylic acid or methacrylic acid are present in the water thickening polymer in an amount varying from about 55 to about 75 parts per hundred parts of total monomer being polymerized.
Claim 11
Dependent Claim 25 words
An aqueous medium according to claim 6 in which said polymer has been neutralized to a pH ranging between a pH of 6.5 to 8.5.
Claim 12
Dependent Claim 32 words
An aqueous medium according to claim 7 in which the amount of water thickening polymer ranges from about 0.1 to about 0.5 percent by weight based on the weight of the water.
Claim 13
Dependent Claim 46 words
An aqueous medium according to claim 6 in which the water soluble compound of a polyvalent metal ranges from 3 to 100% by weight and the water soluble reducing agent ranges from 3 to 100% by weight, both being based on the weight of said polymer.
Claim 14
Dependent Claim 37 words
The aqueous medium according to claim 6 in which the water soluble compound of a polyvalent metal is sodium dichromate or potassium dichromate and in which the water soluble reducing agent is sodium hydrosulphite or potassium hydrosulphite.

References Cited (Backward Citations)

US2842492A Cited
US3649581A Cited
US3724547A Cited
US3909423A Cited
US3926258A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-04-09 1982-10-09 1983-04-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-04-09 1986-10-09 1987-04-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-04-09 1990-10-09 1991-04-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag