Abstract
Abstract A paint composition comprises (A) 30 to 70 percent by weight of an oil-modified alkyd resin of an oil length of 30 to 70 percent which has been modified with sorbic acid, crotonic acid, or 2-( beta -furyl) acrylic acid, the content of which is 0.5 to 30 percent by weight and (B) 70 to 30 percent by weight of a polymerizable monomer in which the oil-modified alkyd resin is dissolved.
Inventors
- 👤 Mitsutoshi Aritomi
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 14:44
CPC Classifications
C; C08; C08K; C08K5/00; C08K5/04; C08K5/10; C08K5/101; C08G; C08G63/00; C08G63/02; C08G63/12; C08G63/16; C08G63/20; C09; C09D; C09D167/00; C09D167/08
Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
125 words
An oil-modified alkyd resin composition comprising: from 30 to 70 percent by weight of an ingredient (A) comprising an oil-modified alkyd resin of an oil length of from 30 to 70 percent which is a poly condensation reaction product of: (a) a polybasic acid, (b) a polyhydric alcohol, (c) a saturated or unsaturated fatty acid or oil, and (d) an α,β-unsaturated monocarboxylic acid selected from the group consisting of sorbic acid, crotonic acid, and 2-(beta-furyl)acrylic acid, the content of the α,β-unsaturated monocarboxylic acid in the alkyd resin being 0.5 to 30 percent by weight; and from 70 to 30 percent by weight of an ingredient (B) comprising a polymerizable monomer having a boiling point higher than 200° C. in which the ingredient (A) is dissolved.
Claim 2
Dependent Claim
125 words
An oil-modified alkyd resin composition comprising: from 30 to 70 percent by weight of an ingredient (A) comprising an oil-modified alkyd resin of an oil length of from 30 to 70 percent which is a poly condensation reaction product of: (a) a polybasic acid, (b) a polyhydric alcohol, (c) a saturated or unsaturated fatty acid or oil, and (d) an α,β-unsaturated monocarboxylic acid selected from the group consisting of sorbic acid, crotonic acid, and 2-(beta-furyl)acrylic acid, the content of the α,β-unsaturated monocarboxylic acid in the alkyd resin being 0.5 to 30 percent by weight; and from 70 to 30 percent by weight of an ingredient (B) comprising a polymerizable monomer having a boiling point higher than 200° C. in which the ingredient (A) is dissolved.
Claim 3
Dependent Claim
52 words
An oil-modified alkyd resin composition as claimed in claim 1 in which the composition further comprises from 0.5 to 5 parts by weight of an organic peroxide and from 0.01 to 5 parts by weight of a reducing agent with respect to 100 parts by weight of the ingredients (A) and (B).
Claim 4
Dependent Claim
31 words
An oil-modified alkyd resin composition as claimed in claim 1 in which from 2 to 100 mole percent of a polybasic acid constituent of the oil-modified alkyd resin is 3-(β-methyl-2-butenyl)-5-methyl-1,2,3,6-tetrahydrophthalic anhydride.
Claim 5
Dependent Claim
24 words
An oil-modified alkyd resin composition as claimed in claim 1 in which the ingredient (B) is a mixture of 2-hydroxypropyl acrylate and 1,4-butanediol diacrylate.
Claim 6
Dependent Claim
43 words
An oil-modified alkyd resin composition as claimed in claim 1 in which an oil or fatty acid which is a constituent of the oil-modified alkyd resin contains more than 60 percent by weight of linoleic acid or linolenic acid or a mixture thereof.
Claim 7
Dependent Claim
30 words
An oil-modified alkyd resin composition as claimed in claim 1 in which the concentration of sorbic acid in the oil-modified alkyd resin is from 0.5 to 30 parts by weight.
Claim 8
Dependent Claim
27 words
An oil-modified alkyd resin composition as claimed in claim 1 in which said ingredient B is an acrylate or methacrylate having a boiling point above 200° C.
Claim 9
Dependent Claim
80 words
An oil-modified alkyd resin composition as claimed in claim 1 in which said ingredient B is a monoacrylate or monomethacrylate ester wherein the ester group thereof is selected from group consisting of 2-hydroxyethyl, 2-hydroxylpropyl, 2-hydroxyethoxyethyl, 4-hydroxybutyl, 5-hydroxypentyl, 6-hydroxyhexyl, neopentylglycol, 3-butoxy-2-hydroxypropyl, 2-hydroxyl-1-, -2-phenylethyl, polypropylene glycol, glycerine, diethyleneglycol, cyclohexyl, benzyl, 2-ethoxyethyl, 2-butoxyethyl, and tetrahydrofuryl, or a di-, tri-, or tetraacrylate ester of a polyol selected from the group consisting of 1,4-butanediol, 1,6-hexanediol, neopentylglycol, trimethylol-propane, pentaerythritol, pentaerythritol, and glycerine and a combination thereof.
Claim 10
Dependent Claim
38 words
An oil-modified alkyd resin composition as claimed in claim 1 in which said ingredient B is selected from the group consisting of tetrahydrofurfuryl acrylate, 2-hydroxylethyl methacrylate, 2-hydroxypropyl acrylate, 3-butoxy-2-hydroxypropyl acrylate, 1,4-butanediol diacrylate, 1,6-hexanediol diacrylate, trimethylolpropane triacrylate and trimethyacrylate.
References Cited (Backward Citations)
US1950468A
Cited
US2381884A
Cited
US2628209A
Cited
US3380942A
Cited
US3390205A
Cited
US3894978A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1982-04-02 | 1982-10-02 | 1983-04-03 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1986-04-02 | 1986-10-02 | 1987-04-03 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1990-04-02 | 1990-10-02 | 1991-04-03 | $7700.00 | Window Closed / Lapsed |