Abstract

Abstract A method of forming a ball core is disclosed. A flowable homogeneous mass of a thermoplastic resin and a blowing agent is injected into the spherical cavity of a mold under temperature and pressure conditions sufficient to activate the blowing agent. The mold is cooled to 32° to 65° F. so as to form a skin on the surface of the mass. The mass is held within the mold cavity for a sufficient time so that the skin has adequate strength to prevent its rupture by blowing agent contained within the mass, upon removal of the mass from the mold cavity. The mass is cooled at an exterior temperature of 32° to 65° F. A ball core for baseballs and softballs is also disclosed.

Inventors

  • 👤 Julius Tomar

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 22:50
CPC Classifications
A; A63; A63B; A63B37/00; A63B37/02; A63B37/06; A63B45/00; B; B29; B29C; B29C44/00; B29C44/02; B29C44/04; B29C44/0407; Y; Y10; Y10S; Y10S264/00; Y10S264/05; Y10S264/14; Y10S264/83

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 157 words
A method of forming a game ball core comprising: forming a flowable homogeneous mass from a thermoplastic resin and a blowing agent by the application of heat and pressure thereto in an injection molding machine; injecting said mass into the spherical cavity of a mold cooled to 32° to 65° F. to foam said mass and fill the mold cavity; holding said mass in the mold cavity for a sufficient time to form a non-porous skin on the outer surface of said mass, said skin being of adequate strength to prevent rupture of the skin by blowing agent contained within the mass upon removal of said mass from the mold cavity, said time being less than required to dimensionally stabilize said mass; removing said mass from the mold; and cooling said mass at an exterior temperature of 32° to 65° F. to produce a game ball core having a dimension substantially the same as the mold cavity.
Claim 2
Independent Claim 157 words
A method of forming a game ball core comprising: forming a flowable homogeneous mass from a thermoplastic resin and a blowing agent by the application of heat and pressure thereto in an injection molding machine; injecting said mass into the spherical cavity of a mold cooled to 32° to 65° F. to foam said mass and fill the mold cavity; holding said mass in the mold cavity for a sufficient time to form a non-porous skin on the outer surface of said mass, said skin being of adequate strength to prevent rupture of the skin by blowing agent contained within the mass upon removal of said mass from the mold cavity, said time being less than required to dimensionally stabilize said mass; removing said mass from the mold; and cooling said mass at an exterior temperature of 32° to 65° F. to produce a game ball core having a dimension substantially the same as the mold cavity.
Claim 3
Dependent Claim 25 words
The method of claim 1 wherein said thermoplastic resin is an ethylene vinyl acetate copolymer having 12% to 30% by weight polymerized vinyl acetate units.
Claim 4
Dependent Claim 21 words
The method of claim 2 wherein said ethylene vinyl acetate copolymer has 18% to 25% by weight polymerized vinyl acetate units.
Claim 5
Dependent Claim 18 words
The method of claim 1 wherein said mold is cooled to a temperature of 35° to 45° F.
Claim 6
Dependent Claim 18 words
The method of claim 1 wherein said mass is held in said mold for greater than four minutes.
Claim 7
Dependent Claim 26 words
The method of claim 1 wherein said cooling is provided by immersing said mass in a cooling bath having a temperature of 32° to 65° F.
Claim 8
Dependent Claim 17 words
The method of claim 6 wherein said cooling bath has a temperature of 35° to 45° F.
Claim 9
Dependent Claim 15 words
The method of claim 6 wherein said mass is immersed for at least 15 minutes.
Claim 10
Dependent Claim 19 words
The method of claim 1 wherein said mass is cooled at an exterior temperature of 35° to 45° F.

References Cited (Backward Citations)

US2753599A Cited
US1345904A Cited
US1538789A Cited
US1803121A Cited
US3069170A Cited
US3268636A Cited
US3313545A Cited
US3468990A Cited
US3905150A Cited
US3776989A Cited
US3976295A Cited
US3976295B1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-03-12 1982-09-11 1983-03-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-03-12 1986-09-11 1987-03-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-03-12 1990-09-11 1991-03-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag