← Back to Patent Explorer
US4143119A Expired / Lapsed US ⏱️ 0.0 years remaining

Method and composition for inhibiting the corrosion of ferrous metals

Assignee: Dow Chemical Co
•
Filing: 1977-06-16
•
Granted: 1979-03-06
•
Expires: 1997-06-16
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A copper based corrosion inhibitor composition and a method for employing the same to prevent corrosion of metal in contact with acid-gases, i.e., hydrogen sulfide, carbonyl sulfide and carbon dioxide. Copper, or a copper compound and sulfur or a sulfur compound, is maintained in solution in contact with the metal under conditions of operation, particularly the thermal regeneration, which provide copper ions and sulfur atoms, particularly polysulfide moieties at the surface of the metal, e.g. copper sulfide is dissolved in an aqueous alkanolamine, monoethanolamine, solution used as an absorbent for acid-gas removal from sour-gas. The copper and sulfur moieties may be formed in situ or prepared and added in solution. The inhibitor has particular utility in protecting metal surfaces which are subject to corrosion as an incidence of the acid-gas content of either natural or synthetic gases.

Inventors

  • 👤 Robert G. Asperger
  • 👤 Leroy S. Krawczyk
  • 👤 Billy D. Oakes

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 22:42
CPC Classifications
C; C23; C23F; C23F11/00; C23F11/06; B; B01; B01D; B01D3/00; B01D3/14; B01D3/32; B01D3/322; B01D53/00; B01D53/14; B01D53/1493; B01D53/34; B01D53/46; B01D53/48; B01D53/52; B01D53/526; Y; Y02; Y02C; Y02C20/00; Y02C20/40

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 192 words
A corrosion inhibiting composition for ferrous metal and its alloys, in contact with acid-gas stripping absorbent solutions selected from the group consisting of alkanolamines having the formula: ##STR3## wherein each R 1 and R 2 represents independently hydrogen, or --C(R 3 ) 2 C(R 3 ) 2 --OH and R 3 represents an independently selected radical of hydrogen or C 1-3 alkyl radical, sulfolane, (tetrahydrothiophene-1,1-dioxide), potassium carbonate or diglycolamines, each alone or in combination with one or more of each other as aqueous solutions or glycol solutions, said compositions consisting essentially of: (a) a source of copper ion selected from the group consisting of copper metal, copper sulfide and copper salts, (b) a source of sulfur atoms selected from the group consisting of 1) sulfur, or 2) hydrogen sulfide and/or COS in combination with an oxidizing agent which will produce in solution the sulfur atom, at least some of which is the polysulfide, under the conditions of operation in an acid-gas stripping plant which employs thermal regeneration techniques for separating the combined chemisorbed acid-gas from the stripping absorbent, and (c) a solvent for (a) and (b) selected from the afore-enumerated absorbent solutions.
Claim 2
Dependent Claim 192 words
A corrosion inhibiting composition for ferrous metal and its alloys, in contact with acid-gas stripping absorbent solutions selected from the group consisting of alkanolamines having the formula: ##STR3## wherein each R 1 and R 2 represents independently hydrogen, or --C(R 3 ) 2 C(R 3 ) 2 --OH and R 3 represents an independently selected radical of hydrogen or C 1-3 alkyl radical, sulfolane, (tetrahydrothiophene-1,1-dioxide), potassium carbonate or diglycolamines, each alone or in combination with one or more of each other as aqueous solutions or glycol solutions, said compositions consisting essentially of: (a) a source of copper ion selected from the group consisting of copper metal, copper sulfide and copper salts, (b) a source of sulfur atoms selected from the group consisting of 1) sulfur, or 2) hydrogen sulfide and/or COS in combination with an oxidizing agent which will produce in solution the sulfur atom, at least some of which is the polysulfide, under the conditions of operation in an acid-gas stripping plant which employs thermal regeneration techniques for separating the combined chemisorbed acid-gas from the stripping absorbent, and (c) a solvent for (a) and (b) selected from the afore-enumerated absorbent solutions.
Claim 3
Dependent Claim 94 words
A ferrous metal corrosion inhibiting composition consisting of: (a) copper as the copper metal, copper sulfide or copper salt; (b) an oxidizing agent which, in the presence of sulfur or a sulfur containing compound, will convert the sulfur to the sulfur atom and/or oxidize copper to the copper ion, and (c) an alkanolamine of the formula: ##STR4## wherein each R 1 and R 2 represents independently hydrogen, or --C(R 3 ) 2 C(R 3 ) 2 --OH and where R 3 represents an independently selected radical of hydrogen or a C 1-3 alkyl radical.
Claim 4
Dependent Claim 94 words
A ferrous metal corrosion inhibiting composition consisting of: (a) copper as the copper metal, copper sulfide or copper salt; (b) an oxidizing agent which, in the presence of sulfur or a sulfur containing compound, will convert the sulfur to the sulfur atom and/or oxidize copper to the copper ion, and (c) an alkanolamine of the formula: ##STR4## wherein each R 1 and R 2 represents independently hydrogen, or --C(R 3 ) 2 C(R 3 ) 2 --OH and where R 3 represents an independently selected radical of hydrogen or a C 1-3 alkyl radical.
Claim 5
Dependent Claim 42 words
The ferrous metal inhibiting composition of claim 1 consisting of copper metal and a compound yielding sulfur atoms by reaction with an oxidizing agent in solution of an acid-gas stripping absorbent under the conditions of acid-gas stripping and regeneration of stripping absorbent.
Claim 6
Dependent Claim 16 words
The ferrous metal corrosion inhibiting composition of claim 1 wherein copper sulfide is the copper source.
Claim 7
Dependent Claim 20 words
The ferrous metal corrosion inhibiting composition of claim 1 wherein copper sulfide is the copper source and an oxidizing agent.
Claim 8
Dependent Claim 12 words
The inhibitor composition of claim 5 wherein the oxidizing agent is sulfur.
Claim 9
Dependent Claim 105 words
A corrosion inhibited acid-gas absorbing composition consisting of an aqueous acid-gas stripping absorbent solution selected from the group consisting of alkanolamines having the formula: ##STR5## wherein each R 1 and R 2 represents independently hydrogen, or --C(R 3 ) 2 C(R 3 ) 2 --OH and wherein R 3 represents an independently selected radical of hydrogen or C 1-3 alkyl radical, sulfolane, (tetrahydrothiophene-1,1-dioxide), potassium carbonate, or diglycolamines, each alone or in combination with one or more of each other as aqueous solution containing from 1 to 5000 ppm copper and 1 to 5000 ppm sulfur, at least some of which is present as the polysulfide.
Claim 10
Dependent Claim 105 words
A corrosion inhibited acid-gas absorbing composition consisting of an aqueous acid-gas stripping absorbent solution selected from the group consisting of alkanolamines having the formula: ##STR5## wherein each R 1 and R 2 represents independently hydrogen, or --C(R 3 ) 2 C(R 3 ) 2 --OH and wherein R 3 represents an independently selected radical of hydrogen or C 1-3 alkyl radical, sulfolane, (tetrahydrothiophene-1,1-dioxide), potassium carbonate, or diglycolamines, each alone or in combination with one or more of each other as aqueous solution containing from 1 to 5000 ppm copper and 1 to 5000 ppm sulfur, at least some of which is present as the polysulfide.
Claim 11
Dependent Claim 16 words
A corrosion inhibitor composition comprising the composition of claim 6 wherein said medium is an alkanolamine.
Claim 12
Dependent Claim 67 words
A corrosion inhibitor composition comprising the composition of claim 1 dissolved in an aqueous gas-absorbing solution selected from the group consisting of potassium carbonate and alkanolamines, having the formula: ##STR6## wherein each R 1 and R 2 represents independently hydrogen, or --C(R 3 ) 2 C(R 3 ) 2 --OH and where R 3 represents an independently selected radical of hydrogen or a C 1-3 alkyl radical.
Claim 13
Dependent Claim 152 words
In the method for removing acid-gases from natural and synthetic gases containing the same by contacting the acid-gas containing gases with a solution of a gas absorbing solution selected from the group consisting of alkanolamines having the formula: ##STR7## wherein each R 1 and R 2 represents independently hydrogen, or --C(R 3 ) 2 C(R 3 ) 2 --OH and R 3 represents an independently selected radical of hydrogen or C 1-3 alkyl radical, sulfolane, (tetrahydrothiophene-1,1-dioxide), potassium carbonate or diglycolamines, each alone or in combination with one or more of each other as aqueous solutions or glycol solutions, and freeing the medium of the acid-gases by heating, the improvement of which consists of maintaining in solution in said medium the composition of claim 1 thereby to reduce the corrosive attack of the acid-gases on the metallic components of the equipment in which the acid-gas removal and regeneration of medium is carried out.

References Cited (Backward Citations)

US1989004A Cited
US2405672A Cited
US2559580A Cited
US3372981A Cited
US3932583A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-03-05 1982-09-04 1983-03-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-03-05 1986-09-04 1987-03-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-03-05 1990-09-04 1991-03-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag