Abstract

Abstract In the process for effecting a continuous dehydrogenation of hydrocarbons to more unsaturated hydocarbons, particularly alkyl aromatic hydrocarbon to more unsaturated alkyl aromatic hydrocarbons, the improvement which comprises effecting the dehydrogenation with a catalyst comprising a mixture of iron oxide, potassium oxide, carbonate or mixtures thereof, vanadium oxide, optionally chromium oxide and an oxide selected from the group consisting of an oxide of aluminum, cadmium, magnesium, manganese, nickel, a member of the rare earth series, uranium and mixtures thereof.

Inventors

  • 👤 Gregor H. Riesser

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 23:56
CPC Classifications
B; B01; B01J; B01J23/00; B01J23/70; B01J23/76; B01J23/84; B01J23/889; B01J23/8892; B01J23/85; B01J23/86; B01J23/862; B01J23/866; B01J23/888; C; C07; C07C; C07C5/00; C07C5/32; C07C5/321; C07C5/322; C07C5/327; C07C5/333; C07C5/3332

Claims Analysis

Total Claims: 22
Claim 1
Independent Claim 181 words
In a process for effecting a continuous dehydrogenation of hydrocarbons to more unsaturated hydrocarbons at a temperature between about 500° C. and about 700° C., the improvement which comprises effecting the dehydrogenation with a catalyst comprising a mixture having: (a) from about 50 to about 95 percent by weight of an iron oxide, measured as ferric oxide; (b) from about 5 to about 30 percent by weight of a potassium compound selected from the group consisting essentially of potassium oxide, potassium carbonate, and mixtures thereof, measured as potassium oxide; (c) from about 0.01 to about 9 percent by weight of a vanadium oxide, measured as vanadium pentoxide, (d) from about 0.01 to about 10 percent by weight of an additive oxide selected from the group consisting of an oxide of cadmium, magnesium, manganese, nickel, a member of a rare earth series, uranium, and mixtures thereof measured as the individual oxide having the most stable form in air at one atmosphere and 25° C., and (e) from 0 to about 30 percent by weight of a chromium oxide measured as chromic oxide.
Claim 2
Dependent Claim 181 words
In a process for effecting a continuous dehydrogenation of hydrocarbons to more unsaturated hydrocarbons at a temperature between about 500° C. and about 700° C., the improvement which comprises effecting the dehydrogenation with a catalyst comprising a mixture having: (a) from about 50 to about 95 percent by weight of an iron oxide, measured as ferric oxide; (b) from about 5 to about 30 percent by weight of a potassium compound selected from the group consisting essentially of potassium oxide, potassium carbonate, and mixtures thereof, measured as potassium oxide; (c) from about 0.01 to about 9 percent by weight of a vanadium oxide, measured as vanadium pentoxide, (d) from about 0.01 to about 10 percent by weight of an additive oxide selected from the group consisting of an oxide of cadmium, magnesium, manganese, nickel, a member of a rare earth series, uranium, and mixtures thereof measured as the individual oxide having the most stable form in air at one atmosphere and 25° C., and (e) from 0 to about 30 percent by weight of a chromium oxide measured as chromic oxide.
Claim 3
Dependent Claim 24 words
The process of claim 1 wherein the additive oxide is selected from the group consisting of cadmium, magnesium, manganese, nickel, uranium and mixtures thereof.
Claim 4
Dependent Claim 22 words
The process of claim 2 wherein the additive oxide is selected from the group consisting of cadmium, manganese, nickel, and mixtures thereof.
Claim 5
Dependent Claim 21 words
The process of claim 2 wherein the additive oxide is selected from the group consisting of magnesium, uranium and mixtures thereof.
Claim 6
Dependent Claim 23 words
The process of claim 1 wherein the additive oxide is selected from the group consisting of the rare earth series and mixtures thereof.
Claim 7
Dependent Claim 18 words
The process of claim 1 wherein the chromium oxide ranges from 0 to about 20 percent by weight.
Claim 8
Dependent Claim 24 words
The process of claim 6 wherein the additive oxide is selected from the group consisting of cadmium, magnesium, manganese, nickel, uranium, and mixtures thereof.
Claim 9
Dependent Claim 22 words
The process of claim 7 wherein the additive oxide is selected from the group consisting of cadmium, manganese, nickel, and mixtures thereof.
Claim 10
Dependent Claim 21 words
The process of claim 7 wherein the additive oxide is selected from the group consisting of magnesium, uranium and mixtures thereof.
Claim 11
Dependent Claim 23 words
The process of claim 6 wherein the additive oxide is selected from the group consisting of the rare earth series and mixtures thereof.
Claim 12
Dependent Claim 50 words
The process of claim 1 wherein the hydrocarbon is an alkyl aromatic hydrocarbon, and the more unsaturated hydrocarbon is an alkenyl aromatic hydrocarbon, the iron oxide ranges from about 75 to about 95 percent by weight, and the potassium compound ranges from about 6 to about 25 percent by weight.
Claim 13
Dependent Claim 19 words
The process of claim 11 wherein the alkyl aromatic hydrocarbon is ethylbenzene and the alkenyl aromatic hydrocarbon is styrene.
Claim 14
Dependent Claim 24 words
The process of claim 12 wherein the additive oxide is selected from the group consisting of cadmium, magnesium, manganese, nickel, uranium, and mixtures thereof.
Claim 15
Dependent Claim 22 words
The process of claim 13 wherein the additive oxide is selected from the group consisting of cadmium, manganese, nickel, and mixtures thereof.
Claim 16
Dependent Claim 21 words
The process of claim 13 wherein the additive oxide is selected from the group consisting of magnesium, uranium and mixtures thereof.
Claim 17
Dependent Claim 23 words
The process of claim 12 wherein the additive oxide is selected from the group consisting of the rare earth series and mixtures thereof.
Claim 18
Dependent Claim 18 words
The catalyst of claim 12 wherein the chromium oxide ranges from 0 to about 20 percent by weight.
Claim 19
Dependent Claim 58 words
The process of claim 1 wherein the catalyst is prepared by combining iron, potassium, optionally chromium, vanadium and additive oxides and/or compounds thermally decomposable to oxides upon calcination with water to form a paste, forming the paste into pellets, drying the pellets and then calcining the pellets at a temperature from about 600° C. to about 1000° C.
Claim 20
Dependent Claim 16 words
The process of claim 18 wherein the drying and calcining are performed sequentially in one step.
Claim 21
Dependent Claim 59 words
The process of claim 12 wherein the catalyst is prepared by combining iron, potassium, optionally chromium, vanadium and additive oxides and/or compounds thermally decomposable to oxides upon calcination with water to form a paste, forming the paste into pellets, drying the pellets and then calcining the pellets at a temperature ranging from about 600° C. to about 1000° C.
Claim 22
Dependent Claim 16 words
The process of claim 20 wherein the drying and calcining are performed sequentially in one step.

References Cited (Backward Citations)

USRE22800E Cited
US2395876A Cited
US2370798A Cited
US2397218A Cited
US2414585A Cited
US3084125A Cited
US3849339A Cited
US4039601A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-03-05 1982-09-04 1983-03-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-03-05 1986-09-04 1987-03-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-03-05 1990-09-04 1991-03-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag