Method of arc welding under water

Assignee: Individual
•
Filing: 1977-01-12
•
Granted: 1979-02-13
•
Expires: 1997-01-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In a method of arc welding under water or at superatmospheric pressure (or both) the weld is made in a chamber containing a gaseous atmosphere. The weld metal is deposited from flux-cored welding wire whose core contains strong deoxidant(s) such as aluminium, magnesium, titanium, zirconium, lithium and calcium. A shielding gas containing a selected proportion of oxygen or oxygen-containing gas but consisting mainly of an inert gas such as argon or helium is employed to surround the arc. The shielding gas is constituted by the atmosphere in the chamber.

Inventors

  • 👤 Brian E. Pinfold

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 12:43
CPC Classifications
B; B23; B23K; B23K9/00; B23K9/32; B23K9/325; B23K35/00; B23K35/02; B23K35/0255; B23K35/0261; B23K35/0266; B23K9/0061; B23K9/12; B23K9/133; B23K9/1336

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 145 words
A method of arc welding in an underwater chamber containing a gaseous environment, including the steps of forming the gaseous environment at superatmospheric pressure in the chamber by passing into the chamber at least one inert gas selected from the group consisting of argon, krypton, xenon and helium and at least one oxygen-containing gas selected from the group consisting of oxygen and carbon dioxide, depositing weld metal from a consumable, flux-cored arc welding wire containing at least one strong deoxidiser selected from the group consisting of magnesium, aluminum, zirconium, titanium, barium, lithium and calcium, the proportion of oxygen in said oxygen-containing gas in the gaseous environment having a partial pressure less than the partial pressure of oxygen in air at atmospheric pressure and constituting less than 14% by volume of the gaseous environment and extracting the fume emitted by the welding from said gaseous environment.
Claim 2
Independent Claim 145 words
A method of arc welding in an underwater chamber containing a gaseous environment, including the steps of forming the gaseous environment at superatmospheric pressure in the chamber by passing into the chamber at least one inert gas selected from the group consisting of argon, krypton, xenon and helium and at least one oxygen-containing gas selected from the group consisting of oxygen and carbon dioxide, depositing weld metal from a consumable, flux-cored arc welding wire containing at least one strong deoxidiser selected from the group consisting of magnesium, aluminum, zirconium, titanium, barium, lithium and calcium, the proportion of oxygen in said oxygen-containing gas in the gaseous environment having a partial pressure less than the partial pressure of oxygen in air at atmospheric pressure and constituting less than 14% by volume of the gaseous environment and extracting the fume emitted by the welding from said gaseous environment.

References Cited (Backward Citations)

US2281070A Cited
US3527916A Cited
US3566073A Cited
US3837171A Cited
US3670135A Cited
US3876852A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-02-12 1982-08-14 1983-02-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-02-12 1986-08-14 1987-02-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-02-12 1990-08-14 1991-02-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag