Abstract

Abstract A highly active catalyst for oxidative dehydrogenation reactions made up of Pd-Au alloy particles containing about 40 to 80 aromatic percent Au and ranging from 15 to 40 A in size, said particles being supported in an amount of from about 1.5 to 10 weight percent on a silica or other suitable carrier. The alloy particles, which have a surface composition similar to the overall composition, are prepared by an ion-exchange method in which a stable AU III compound such as bisethylenediamine Au III chloride and a palladium salt are added to an aqueous ammoniacal dispersion of the carrier material (i.e. silica gel) to form a precursor which is subsequently reduced in dihydrogen.

Inventors

  • 👤 Michel Boudart
  • 👤 Yiu-Lau Lam

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 04:32
CPC Classifications
B; B01; B01J; B01J23/00; B01J23/38; B01J23/48; B01J23/52; Y; Y10; Y10S; Y10S502/00; Y10S502/506; Y10S502/509; Y10S502/511

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 55 words
A catalyst useful in hydrogenation and oxidative dehydrogenation reactions comprising Pd-Au alloy particles containing from about 30 to 80 atomic percent Au and ranging in size from about 15 to 40A, said alloy particles being supported in an amount of from about 1.5 to 10 weight percent on an inert, porous adsorptive, refractory oxide support.
Claim 2
Dependent Claim 55 words
A catalyst useful in hydrogenation and oxidative dehydrogenation reactions comprising Pd-Au alloy particles containing from about 30 to 80 atomic percent Au and ranging in size from about 15 to 40A, said alloy particles being supported in an amount of from about 1.5 to 10 weight percent on an inert, porous adsorptive, refractory oxide support.
Claim 3
Dependent Claim 14 words
The catalyst of claim 1 wherein the supporting material is silica or silica gel.
Claim 4
Dependent Claim 18 words
The catalyst of claim 2 wherein the alloy particles contain from about 40 to 80 weight percent Au.
Claim 5
Independent Claim 153 words
A method for preparing a catalyst made up of fine Pd-Au alloy particles of uniform composition held on an inert, porous, adsorptive, refractory oxide support, said method comprising adding a dilute aqueous solution of stable Pd- and Au III-containing compounds, present in proportions calculated to give the desired Pd-Au alloy composition, to a warm dispersion of said support in an aqueous ammoniacal medium whereby Au III- and Pd-containing ions are exchanged for NH 4 + ions present in the support; washing the resulting support to free the same of other than Au III- and Pd-containing ions; and heating the washed support in dihydrogen at temperatures effective to reduce the metals and form fine Pd-Au alloy particles on the support surfaces; said stable Pd- and Au III-containing compounds each being characterized by the ability to withstand temperatures of 60°-80° C. when in continuous contact with ammoniacal solutions having a pH of at least 11.
Claim 6
Independent Claim 153 words
A method for preparing a catalyst made up of fine Pd-Au alloy particles of uniform composition held on an inert, porous, adsorptive, refractory oxide support, said method comprising adding a dilute aqueous solution of stable Pd- and Au III-containing compounds, present in proportions calculated to give the desired Pd-Au alloy composition, to a warm dispersion of said support in an aqueous ammoniacal medium whereby Au III- and Pd-containing ions are exchanged for NH 4 + ions present in the support; washing the resulting support to free the same of other than Au III- and Pd-containing ions; and heating the washed support in dihydrogen at temperatures effective to reduce the metals and form fine Pd-Au alloy particles on the support surfaces; said stable Pd- and Au III-containing compounds each being characterized by the ability to withstand temperatures of 60°-80° C. when in continuous contact with ammoniacal solutions having a pH of at least 11.
Claim 7
Dependent Claim 31 words
The method of claim 4 wherein the Au-containing compound employed to form the dilute aqueous solution is one wherein Au III is complexed with one of 1,2-ethanediamine, 1,2-propanediamine, 2,2'-bipyridine and 1,10-phenanthroline.
Claim 8
Dependent Claim 15 words
The method of claim 5 wherein the Au-containing complex employed is bis-ethylenediamine Au III chloride.

References Cited (Backward Citations)

US3156735A Cited
US3441601A Cited
US3775342A Cited
US3957688A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-01-22 1982-07-24 1983-01-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-01-22 1986-07-24 1987-01-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-01-22 1990-07-24 1991-01-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag