US4134945A Expired / Lapsed US ⏱️ 0.0 years remaining

Method and apparatus for making foam

Assignee: ER Carpenter Co
•
Filing: 1976-11-02
•
Granted: 1979-01-16
•
Expires: 1996-11-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An improvement in the manufacture of flexible densified polyurethane foam wherein the partially cured freely risen foam is fed through a crush conveyor to minimize the density gradient throughout the vertical cross section. The crush conveyor includes an upper crushing section which is arcuate and has a radius of a dimension such that the ratio of the radius of the arc to height of the partially cured freely risen foam is 1.1 to 1 or greater. The crush conveyor has a bottom crushing section which may be arcurate with a radius of a dimension such that the ratio of its radius to the height of the partially cured freely risen foam is also 1.1 to 1 or greater. The radius of the bottom arcuate crushing section may be the same or larger than the radius of the top arc. As an alternative, the bottom crushing section may be planar and may be horizontal, or inclined with respect to the horizontal.

Inventors

  • 👤 Alan H. Milford
  • 👤 Oliver J. Proulx

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 21:25
CPC Classifications
B; B29; B29C; B29C44/00; B29C44/34; B29C44/56; B29C44/5627

Claims Analysis

Total Claims: 20
Claim 1
Independent Claim 119 words
In an apparatus for making flexible densified polyurethane foam wherein a cellular polyurethane foam-forming reaction mixture is allowed to rise and is crushed before being completely cured, the improvement comprising crush conveyor means for crushing said partially cured freely risen cellular foam as said foam is being conveyed, said conveyor means including an upper crushing portion of arcuate configuration having a radius of a dimension such that the ratio of the arc radius to height of the freely risen foam is greater than 2.67 to 1, and a bottom crushing portion oppositely disposed from the upper crushing portion, said bottom crushing portion comprising a planar section and the final foam density is under about four pounds per cubic foot.
Claim 2
Dependent Claim 119 words
In an apparatus for making flexible densified polyurethane foam wherein a cellular polyurethane foam-forming reaction mixture is allowed to rise and is crushed before being completely cured, the improvement comprising crush conveyor means for crushing said partially cured freely risen cellular foam as said foam is being conveyed, said conveyor means including an upper crushing portion of arcuate configuration having a radius of a dimension such that the ratio of the arc radius to height of the freely risen foam is greater than 2.67 to 1, and a bottom crushing portion oppositely disposed from the upper crushing portion, said bottom crushing portion comprising a planar section and the final foam density is under about four pounds per cubic foot.
Claim 3
Dependent Claim 21 words
The apparatus of claim 1 wherein said bottom crushing section is inclined upwardly toward the downstream end of the conveyor means.
Claim 4
Dependent Claim 15 words
The apparatus of claim 2 wherein said bottom crushing section is inclined less than 10°.
Claim 5
Dependent Claim 15 words
The apparatus of claim 1 wherein said ratio is between under about 10.5 to 1.
Claim 6
Dependent Claim 134 words
In an apparatus for making flexible densified polyurethane foam wherein a cellular foam-forming mixture is allowed to rise and is crushed before being completely cured, the improvement comprising crush conveyor means for crushing said partially cured cellular freely risen foam as said foam is being conveyed, said conveyor means including an upper crushing portion of arcuate configuration having a radius of a dimension such that the ratio of the arc radius to the height of the freely risen foam is greater than 2.67 to 1, and a bottom crushing portion being of an arcuate configuration having a radius of a dimension such that the ratio of arc radius to the height of the freely risen foam is greater than 1.1 to 1 and the final foam density is under four pounds per cubic foot.
Claim 7
Dependent Claim 134 words
In an apparatus for making flexible densified polyurethane foam wherein a cellular foam-forming mixture is allowed to rise and is crushed before being completely cured, the improvement comprising crush conveyor means for crushing said partially cured cellular freely risen foam as said foam is being conveyed, said conveyor means including an upper crushing portion of arcuate configuration having a radius of a dimension such that the ratio of the arc radius to the height of the freely risen foam is greater than 2.67 to 1, and a bottom crushing portion being of an arcuate configuration having a radius of a dimension such that the ratio of arc radius to the height of the freely risen foam is greater than 1.1 to 1 and the final foam density is under four pounds per cubic foot.
Claim 8
Dependent Claim 23 words
The apparatus of claim 5 wherein said ratio of said bottom crushing portion is greater than said ratio of said upper conveyor portion.
Claim 9
Dependent Claim 19 words
The apparatus of claim 5 wherein said ratio of said upper crushing portion is under about 10.5 to 1.
Claim 10
Dependent Claim 24 words
The apparatus of claim 5 wherein said ratio of said lower crushing portion is between about 2 to 1 and about 10.5 to 1.
Claim 11
Dependent Claim 133 words
In a process for making flexible densified polyurethane foam wherein a cellular polyurethane foam-forming reaction mixture is allowed to rise and is crushed before being cured, the improvement comprising conveying said cellular partially cured freely risen foam to a crush conveyor and crushing said foam as said foam is being conveyed between upper and lower crushing portions of said crush conveyor, said upper crushing portions of said crush conveyor, said upper crushing portion being of arcuate configuration having a radius of a dimension such that the ratio of the arc radicus to the height of the freely risen foam is greater than 2.67 to 1, the lower crushing portion being oppositely disposed from said upper portion and comprising a planar section and the final foam density is under 4 pounds per cubic foot.
Claim 12
Dependent Claim 133 words
In a process for making flexible densified polyurethane foam wherein a cellular polyurethane foam-forming reaction mixture is allowed to rise and is crushed before being cured, the improvement comprising conveying said cellular partially cured freely risen foam to a crush conveyor and crushing said foam as said foam is being conveyed between upper and lower crushing portions of said crush conveyor, said upper crushing portions of said crush conveyor, said upper crushing portion being of arcuate configuration having a radius of a dimension such that the ratio of the arc radicus to the height of the freely risen foam is greater than 2.67 to 1, the lower crushing portion being oppositely disposed from said upper portion and comprising a planar section and the final foam density is under 4 pounds per cubic foot.
Claim 13
Dependent Claim 17 words
In the method of claim 9, said bottom crushing section being inclined with respect to the horizontal.
Claim 14
Dependent Claim 15 words
In the method of claim 9 said bottom crushing section being inclined less than 10°.
Claim 15
Dependent Claim 14 words
In the method of claim 9, said ratio being under about 10.5 to 1.
Claim 16
Dependent Claim 152 words
In a process for making flexible densified foam wherein a cellular polyurethane foam-forming reaction mixture is allowed to rise and is crushed before being cured, the improvement comprising conveying said partially cured freely risen foam to a crush conveyor and crushing said foam as said foam is being conveyed between upper and lower crushing portions of said crush conveyor, said upper crushing portion being of arcuate configuration having a radius of a dimension such that the ratio of the arc radius to the height of the freely risen foam is greater than 2.67 to 1, and said bottom crushing poriton being oppositely disposed from said upper portion and being of an arcuate configuration having a radius of a dimension such that the ratio of arc radius to the height of the freely risen foam is greater than 1.1 to 1, the foam product density is under about 4 pounds per cubic foot.
Claim 17
Dependent Claim 152 words
In a process for making flexible densified foam wherein a cellular polyurethane foam-forming reaction mixture is allowed to rise and is crushed before being cured, the improvement comprising conveying said partially cured freely risen foam to a crush conveyor and crushing said foam as said foam is being conveyed between upper and lower crushing portions of said crush conveyor, said upper crushing portion being of arcuate configuration having a radius of a dimension such that the ratio of the arc radius to the height of the freely risen foam is greater than 2.67 to 1, and said bottom crushing poriton being oppositely disposed from said upper portion and being of an arcuate configuration having a radius of a dimension such that the ratio of arc radius to the height of the freely risen foam is greater than 1.1 to 1, the foam product density is under about 4 pounds per cubic foot.
Claim 18
Dependent Claim 23 words
In the process of claim 13, said ratio of said lower crushing portion being greater than said ratio of said upper crushing portion.
Claim 19
Dependent Claim 19 words
In the process of claim 13, said ratio of said upper crushing portion being under about 10.5 to 1.
Claim 20
Dependent Claim 24 words
In the process of claim 13, said ratio of said lower crushing portion being between about 2 to 1 and about 10.5 to 1.

References Cited (Backward Citations)

US2326889A Cited
US3147164A Cited
US3112524A Cited
US3298884A Cited
US3562767A Cited
US3506600A Cited
US3993426A Cited
US3836298A Cited
US3860368A Cited
US3945789A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-01-15 1982-07-17 1983-01-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-01-15 1986-07-17 1987-01-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-01-15 1990-07-17 1991-01-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag