Abstract

Abstract Catalyst for dehydrogenating hydrocarbons, as manufactured by the process comprising:

Inventors

  • 👤 Philippe Courty

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 11:13
CPC Classifications
B; B01; B01J; B01J23/00; B01J23/70; B01J23/76; B01J23/84; B01J23/85; B01J23/86; B01J23/862; B01J37/00; B01J37/0009; C; C07; C07C; C07C5/00; C07C5/32; C07C5/321; C07C5/322

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 207 words
A catalyst comprising iron oxide, chromium oxide, 5-40% by weight of kaliophyllite and excess potassium oxide with respect to said kaliophyllite, especially for dehydrogenating hydrocarbons, as obtained by the process comprising the steps of: admixing at least one iron compound, at least one chromium compound and at least one potassium compound; moistening and malaxing the resulting mixture and adding thereto at least one clayish material selected from the group consisting of kaolinite, halloisite, bentonite, montmorillonite, attapulgite and mixtures thereof, and homogenizing the mixture to form a paste; shaping said paste, drying and roasting it at a temperature of bout 870 - 1050° C, said clayish material being used in such a proportion as to obtain after said roasting a final catalyst containing 5 to 40% by weight of kaliophillite of the formula Al 2 O 3 , 2 SiO 2 , K 2 O as formed by the reaction between said clayish material and a portion of said potassium compound; the iron, chromium and potassium compounds being used in proportions corresponding as oxides, to ratios by weight: ##EQU16## and said potassium compound being used in excess with respect to the amount liable to combine with said clayish material to form said kaliophyllite, and thereby forming said catalyst.
Claim 2
Dependent Claim 207 words
A catalyst comprising iron oxide, chromium oxide, 5-40% by weight of kaliophyllite and excess potassium oxide with respect to said kaliophyllite, especially for dehydrogenating hydrocarbons, as obtained by the process comprising the steps of: admixing at least one iron compound, at least one chromium compound and at least one potassium compound; moistening and malaxing the resulting mixture and adding thereto at least one clayish material selected from the group consisting of kaolinite, halloisite, bentonite, montmorillonite, attapulgite and mixtures thereof, and homogenizing the mixture to form a paste; shaping said paste, drying and roasting it at a temperature of bout 870 - 1050° C, said clayish material being used in such a proportion as to obtain after said roasting a final catalyst containing 5 to 40% by weight of kaliophillite of the formula Al 2 O 3 , 2 SiO 2 , K 2 O as formed by the reaction between said clayish material and a portion of said potassium compound; the iron, chromium and potassium compounds being used in proportions corresponding as oxides, to ratios by weight: ##EQU16## and said potassium compound being used in excess with respect to the amount liable to combine with said clayish material to form said kaliophyllite, and thereby forming said catalyst.
Claim 3
Dependent Claim 30 words
A catalyst according to claim 1, in which said excess of potassium compound is in the following relations to the iron compound and the chromium compound calculated as oxides: ##EQU17##
Claim 4
Dependent Claim 26 words
A catalyst according to claim 1, in which the iron, chromium or potassium compounds are used in proportions corresponding, as oxides, to ratios by weight: ##EQU18##
Claim 5
Dependent Claim 37 words
A catalyst according to claim 1 in which up to 50% by moles of the potassium compound is replaced with an equivalent amount of at least one other alkali-metal compound and/or at least one alkaline-earth metal compound.
Claim 6
Dependent Claim 28 words
A catalyst according to claim 4, in which the potassium compound is partially replaced by at least one compound of a metal selected from sodium, calcium and barium.
Claim 7
Dependent Claim 12 words
A catalyst according to claim 1, wherein the clayish material is kaolinite.
Claim 8
Dependent Claim 12 words
A catalyst according to claim 1, wherein the clayish material is clay.
Claim 9
Dependent Claim 46 words
A catalyst according to claim 4, in which up to 50% by moles of the potassium compound is replaced with a sodium compound and the resulting catalyst also comprises nepheline of the molar composition Al 2 O 3 , 2 SiO 2 , Na 2 O.
Claim 10
Dependent Claim 33 words
A catalyst according to claim 1, further comprising from 0.1 to 5% by weight of at least one oxide of at least one metal selected from copper, vanadium, zinc, magnesium, manganese and bismuth.
Claim 11
Dependent Claim 12 words
A catalyst according to claim 9, wherein said oxide is vanadium oxide.
Claim 12
Dependent Claim 46 words
A catalyst according to claim 1, in which the roasting step comprises a period of temperature increase of 3 to 10 hours, a stage of 1 to 5 hours at a temperature from 870 to 1050° C, and a cooling period of 10 to 30 hours.
Claim 13
Dependent Claim 14 words
A catalyst according to claim 1, having a halogen content lower then 1000 ppm.
Claim 14
Dependent Claim 66 words
A catalyst according to claim 1, shaped as extrudates of a 3 to 6 mm diameter, having a filling density in an industrial reactor from 0.80 to 1.15 T/m 3 , a crushing strength, measured on a Erweka machine, from 1.6 to 3 kg/mm, a porosity, measured by mercury porosimetry, from 18 to 60 ml/100 g and an average pore diameter from 3000 to 11000 A.
Claim 15
Dependent Claim 15 words
A catalyst according to claim 1, wherein the iron compound consists essentially of ferric oxide.
Claim 16
Dependent Claim 36 words
A catalyst according to claim 1, wherein the iron compound consists essentially of a mixture of 80 - 95% b.w. of ferric oxide and 5 - 20% b.w. of iron hydroxide, calculated as the corresponding oxide.

References Cited (Backward Citations)

US3100234A Cited
US3752773A Cited
US3703593A Cited
US3867305A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-01-15 1982-07-17 1983-01-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-01-15 1986-07-17 1987-01-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-01-15 1990-07-17 1991-01-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag