Polyurethane tire sidewalls

Assignee: Bridgestone Firestone Inc
•
Filing: 1976-12-21
•
Granted: 1978-12-26
•
Expires: 1996-12-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Polyurethane pneumatic tires with colored sidewalls are produced by applying one or more elastomeric coatings thereto. A colored polyurethane elastomeric coating may be applied directly to the sidewall, but it may be applied to a primer elastomeric coating which is first applied and the colored coating is applied to it either before or after it is cured. The color of the colored coating may be produced by dyeing or pigmenting.

Inventors

  • 👤 Durward T. Roberts, Jr.

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 23:36
CPC Classifications
B; B29; B29D; B29D30/00; B29D30/06; B29D30/72; B60; B60C; B60C13/00; B60C13/04; B29D2030/728; B60C2013/045; Y; Y10; Y10S; Y10S152/00; Y10S152/12

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 151 words
A pneumatic tire with polyurethane in the surface exposed at the sidewall, with a cured, colored polyurethane coating over said surface which coating is adhered to said surface by a reaction product of (1) free --NCO from a prepolymer from which the coating is derived, wherein said prepolymer is formed from a substantially saturated hydroxy-terminated diol having a molecular weight of 500 to 10,000 or higher and a substantially saturated aliphatic diisocyanate; with (2) free --OH and --NH in said surface, so that the coating adheres so firmly to the surface that when the tire mounted on a rim and inflated to 24 psi, is tested against a flat large wheel surface at 50 mph., and the pressure of the tire against the wheel is increased to 200 percent of the rated load, as the test is run until the tire fails the coating remains in place and does not crack.
Claim 2
Dependent Claim 151 words
A pneumatic tire with polyurethane in the surface exposed at the sidewall, with a cured, colored polyurethane coating over said surface which coating is adhered to said surface by a reaction product of (1) free --NCO from a prepolymer from which the coating is derived, wherein said prepolymer is formed from a substantially saturated hydroxy-terminated diol having a molecular weight of 500 to 10,000 or higher and a substantially saturated aliphatic diisocyanate; with (2) free --OH and --NH in said surface, so that the coating adheres so firmly to the surface that when the tire mounted on a rim and inflated to 24 psi, is tested against a flat large wheel surface at 50 mph., and the pressure of the tire against the wheel is increased to 200 percent of the rated load, as the test is run until the tire fails the coating remains in place and does not crack.
Claim 3
Dependent Claim 15 words
A tire of claim 1 in which the coating is adhered directly to the sidewall.
Claim 4
Dependent Claim 29 words
A tire of claim 1 in which the coating is adhered to a primer on the sidewall, wherein said primer comprises a polyurethane prepolymer and a curing agent therefore.
Claim 5
Independent Claim 63 words
The method of coating a pneumatic tire having polyurethane in the surface exposed at a sidewall which method comprises (1) applying to said surface a colored coating composition comprising an elastomeric NCO-terminated polyurethane prepolymer and a curing agent therefor wherein said NCO-terminated polyurethane prepolymer reacts with free --OH and --NH in the surface of said tire, and (2) heating to effect said reaction.
Claim 6
Independent Claim 63 words
The method of coating a pneumatic tire having polyurethane in the surface exposed at a sidewall which method comprises (1) applying to said surface a colored coating composition comprising an elastomeric NCO-terminated polyurethane prepolymer and a curing agent therefor wherein said NCO-terminated polyurethane prepolymer reacts with free --OH and --NH in the surface of said tire, and (2) heating to effect said reaction.
Claim 7
Dependent Claim 16 words
The method of claim 4 in which the coating is applied directly to the polyurethane sidewall.
Claim 8
Dependent Claim 27 words
The method of claim 4 in which a primer of a polyurethane prepolymer and a curing agent is applied to the polyurethane sidewall before applying the coating.
Claim 9
Dependent Claim 26 words
The method of claim 4 in which the coating composition includes an aliphatic diamine which is blocked with a ketone or aldehyde and aliphatic diisocyanate-polyurethane prepolymer.

References Cited (Backward Citations)

US2566328A Cited
US2574233A Cited
US2742942A Cited
US2749960A Cited
US2905582A Cited
US3648748A Cited
USRE28424E Cited
US3806486A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-12-25 1982-06-26 1982-12-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-12-25 1986-06-26 1986-12-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-12-25 1990-06-26 1990-12-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag