Abstract

Abstract A method for the production of a fine-grained mixture of mineral solids such as pulverized raw material for the calcining of cement clinkers composed of several materials, one of the starting materials constituting a substantial proportion of the total mixture and having a grain size suitable for further processing, but having a relatively high moisture content, and another starting material also constituting a substantial proportion of the total mixture and consisting of coarse grained fragments. In accordance with the present invention, these two starting materials, together with other additives which might be present, are mixed and suspended in a column of heated air to dry the mixture to a moisture level suitable for further processing.

Inventors

  • 👤 Kunibert Brachthauser

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 18:58
CPC Classifications
C; C04; C04B; C04B7/00; C04B7/36; C04B7/38; C04B7/40

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 132 words
A method for the production of a mixture of fine-grained mineral solids from at least two components, each forming an essential part of the mixture, the first of said components being in the form of a slurry and the second of said components being a relatively coarse, moist mineral material, which comprises: partially dehydrating said slurry, mixing a portion of the partially dehydrated slurry with said second component in a mill while introducing hot drying gases into said mill, passing the output of said mill into a sifter, further dehydrating the remainder of said partially dehydrated slurry, mixing the futher dehydrated remainder with particulate matter recovered from said sifter to produce a relatively moist mixture, and combining said relatively moist mixture with the output of said mill en route to said sifter.
Claim 2
Independent Claim 132 words
A method for the production of a mixture of fine-grained mineral solids from at least two components, each forming an essential part of the mixture, the first of said components being in the form of a slurry and the second of said components being a relatively coarse, moist mineral material, which comprises: partially dehydrating said slurry, mixing a portion of the partially dehydrated slurry with said second component in a mill while introducing hot drying gases into said mill, passing the output of said mill into a sifter, further dehydrating the remainder of said partially dehydrated slurry, mixing the futher dehydrated remainder with particulate matter recovered from said sifter to produce a relatively moist mixture, and combining said relatively moist mixture with the output of said mill en route to said sifter.
Claim 3
Dependent Claim 22 words
A method according to claim 1 in which the partial dehydration is carried out to a water content of 30 to 50%.
Claim 4
Dependent Claim 22 words
A method according to claim 1 in which the further dehydration is carried out to a water content of 15 to 30%.

References Cited (Backward Citations)

US2964299A Cited
US3408745A Cited
US3645513A Cited
US3721014A Cited
US3974572A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-12-25 1982-06-26 1982-12-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-12-25 1986-06-26 1986-12-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-12-25 1990-06-26 1990-12-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag