Abstract

Abstract An improved process for making a gas diffusion electrode which comprises heating of the mixed electrode material prior to forming the electrode. Because of the stickiness or self adhesion characteristics of the electrode mixture, the invention includes special transport apparatus having a fluidized bed that uniformly disperses the sticky electrode material onto a conveyor belt for forming the electrode without subsequent heating.

Inventors

  • 👤 Royce E. Biddick

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 05:56
CPC Classifications
H; H01; H01M; H01M4/00; H01M4/86; H01M4/88; H01M4/8875; H01M4/8663; H01M4/8668; H01M12/00; H01M12/04; H01M12/06; Y; Y10; Y10S; Y10S264/00; Y10S264/51; Y10S425/00; Y10S425/02

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 93 words
The process for manufacture of a continuous electrode comprising: preparing a bulk electrode material including a hydrophobic binder comprised of sticky electrode material particles; fluidizing the sticky electrode material particles in a fluid stream by observing sticky electrode particle behavior in a fluid stream and controlling the fluid stream such that particles are maintained in a uniform suspension allowing a uniform flow of sticky electrode particles over a weir onto a moving member to thereby produce a continuous strip of electrode particles; and then compressing the electrode particles to produce a continuous electrode.
Claim 2
Dependent Claim 93 words
The process for manufacture of a continuous electrode comprising: preparing a bulk electrode material including a hydrophobic binder comprised of sticky electrode material particles; fluidizing the sticky electrode material particles in a fluid stream by observing sticky electrode particle behavior in a fluid stream and controlling the fluid stream such that particles are maintained in a uniform suspension allowing a uniform flow of sticky electrode particles over a weir onto a moving member to thereby produce a continuous strip of electrode particles; and then compressing the electrode particles to produce a continuous electrode.
Claim 3
Dependent Claim 37 words
The process for manufacture of a continuous electrode as described in claim 1 wherein said bulk electrode material is heated to drive off unwanted suspension materials in the bulk electrode material to thereby produce an electrode material.
Claim 4
Dependent Claim 22 words
The process for manufacture of a continuous electrode as described in claim 1 wherein said bulk electrode material is characterized by self-adhesion.
Claim 5
Dependent Claim 148 words
The process for manufacture of a continuous electrode comprising: preparing a bulk electrode mixture including a hydrophobic binder having a predetermined melting temperature, said bulk electrode material characterized by self-adhesion; first heating the bulk electrode mixture to a temperature below the melting temperature of the hydrophobic binder to drive off unwanted suspension materials in the bulk electrode mixture to thereby produce large lumps of electrode mixture; breaking up the lumps of electrode mixture to produce self-adhering electrode particles; fluidizing the self-adhering electrode particles in a fluid stream by observing sticky electrode particle behavior in a fluid stream and controlling the fluid stream such that particles are maintained in a uniform suspension allowing a uniform flow of sticky electrode particles over a weir onto a moving member to thereby produce a continuous strip of self-adhering electrode particles; and then compressing the electrode particles to produce a continuous self-adhering electrode.
Claim 6
Dependent Claim 148 words
The process for manufacture of a continuous electrode comprising: preparing a bulk electrode mixture including a hydrophobic binder having a predetermined melting temperature, said bulk electrode material characterized by self-adhesion; first heating the bulk electrode mixture to a temperature below the melting temperature of the hydrophobic binder to drive off unwanted suspension materials in the bulk electrode mixture to thereby produce large lumps of electrode mixture; breaking up the lumps of electrode mixture to produce self-adhering electrode particles; fluidizing the self-adhering electrode particles in a fluid stream by observing sticky electrode particle behavior in a fluid stream and controlling the fluid stream such that particles are maintained in a uniform suspension allowing a uniform flow of sticky electrode particles over a weir onto a moving member to thereby produce a continuous strip of self-adhering electrode particles; and then compressing the electrode particles to produce a continuous self-adhering electrode.
Claim 7
Dependent Claim 19 words
The process of claim 4 wherein the time of heating the electrode mixture is a minimum of 5 minutes.
Claim 8
Dependent Claim 11 words
The process of claim 4 wherein the hydrophobic binder comprises polytetrafluoroethylene.
Claim 9
Dependent Claim 11 words
The process of claim 4 wherein the hydrophobic binder comprises polypropylene.
Claim 10
Dependent Claim 21 words
The process of claim 4 including the step of shaking the bulk electrode mixture to break up any lumps formed therein.
Claim 11
Dependent Claim 24 words
The process of claim 8 including the step of directing the fluidized self-adhering particles over a weir and onto a conveyor belt for compressing.
Claim 12
Dependent Claim 17 words
The process of claim 9 including the step of pressing a collector screen into said electrode mixture.
Claim 13
Dependent Claim 15 words
The process of claim 10 including compressing the electrode mixture between a pair of rollers.

References Cited (Backward Citations)

US3027601A Cited
GB931732A Cited
US3195958A Cited
US3674389A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-12-11 1982-06-12 1982-12-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-12-11 1986-06-12 1986-12-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-12-11 1990-06-12 1990-12-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag