← Back to Patent Explorer
US4129630A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for producing thermoplastic resin films having reduced thickness unevenness

Assignee: Teijin Ltd
•
Filing: 1976-03-29
•
Granted: 1978-12-12
•
Expires: 1996-03-29
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for producing a film of reduced thickness unevenness which comprises extruding a thermoplastic resin from an extrusion die into a film form, exposing the extrudate to an electric field induced by an electrostaticity applying electrode, and then pinning it to the surface of a cooling drum, wherein a shielding object is disposed between the extrusion surface of the die and the electrostaticity applying electrode thereby to maintain the applied voltage constant in the widthwise direction of the extrudate and to enable the extrudate to adhere intimately to the surface of the cooling drum, and an apparatus for producing a film of reduced thickness unevenness comprising an extrusion die equipped with means for adjusting the thickness unevenness of the film by temperature control, an electrode for applying electrostaticity, a cooling drum and a shielding object, said shielding object being a conductive object, a non-conductive object or a combination of these, and being disposed between the extrusion surface of the die and the electrostaticity applying electrode.

Inventors

  • 👤 Masami Etchu
  • 👤 Takao Yamaguchi
  • 👤 Norio Takagi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 06:57
CPC Classifications
B; B29; B29C; B29C48/00; B29C48/25; B29C48/88; B29C48/911; B29C48/9135; B29C48/915; B29C48/9165; B29C48/03; B29C48/07; B29C48/08; B29C48/78; B29C48/86; B29C48/865; B29C48/914; B29C48/92; B29C2948/00; B29C2948/92; B29C2948/92504; B29C2948/92609; B29C2948/92647; B29C2948/92704; B29C2948/92819; B29C2948/92857; B29C2948/92904

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 98 words
In a process for producing a film of reduced thickness unevenness by extruding a thermoplastic resin from an extrusion die into a film form, exposing the extrudate to an electric field induced by a single electrostaticity applying electrode, and then pinning it to the surface of a cooling drum, the improvement comprising disposing a non-grounded shielding object between the extrusion surface of the die and the electrostaticity applying electrode thereby to maintain the applied voltage constant in the widthwise direction of the extrudate and to enable the extrudate to adhere intimately to the surface of the cooling drum.
Claim 2
Dependent Claim 98 words
In a process for producing a film of reduced thickness unevenness by extruding a thermoplastic resin from an extrusion die into a film form, exposing the extrudate to an electric field induced by a single electrostaticity applying electrode, and then pinning it to the surface of a cooling drum, the improvement comprising disposing a non-grounded shielding object between the extrusion surface of the die and the electrostaticity applying electrode thereby to maintain the applied voltage constant in the widthwise direction of the extrudate and to enable the extrudate to adhere intimately to the surface of the cooling drum.
Claim 3
Dependent Claim 13 words
The process of claim 1 wherein said shielding object is a non-conductive object.
Claim 4
Dependent Claim 20 words
The process of claim 1 wherein said shielding object is a combination of a conductive object and a non-conductive object.
Claim 5
Dependent Claim 31 words
The process of claim 1 wherein said electrode is shielded from said die extrusion surface by securing said shielding object to a part or the whole of the die extrusion surface.
Claim 6
Dependent Claim 26 words
The process of claim 1 wherein said electrode is shielded from said die extrusion surface by disposing said shielding object in the vicinity of said electrode.
Claim 7
Dependent Claim 47 words
The process according to claim 1 which further comprises controlling the thickness uniformity of the extruded film by locally heating the thermoplastic resin to thereby change the flow rate of the molten resin in said locally heated area to thereby provide films having a more uniform thickness.

References Cited (Backward Citations)

US3655307A Cited
US3660549A Cited
US3686374A Cited
US3758251A Cited
US3779682A Cited
US3795474A Cited
US3904725A Cited
US3883279A Cited
US3820929A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-12-11 1982-06-12 1982-12-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-12-11 1986-06-12 1986-12-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-12-11 1990-06-12 1990-12-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag