Abstract

Abstract The present invention provides a process and apparatus for texturizing protein products wherein a protein dough containing a heat coagulable protein is passed through a screw conveyor that has an internal conveying section which changes in configuration such that the dough is stretched during passage through the conveyor, while at the same time is heated to a temperature above the heat coagulation temperature of the protein to ultimately provide a meat-like fiber structure wherein the fibers are aligned.

Inventors

  • 👤 Peter W. A. de Ruyter

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 21:18
CPC Classifications
A; A23; A23J; A23J3/00; A23J3/22; A23J3/26; B; B29; B29C; B29C48/00; B29C48/03; B29C48/25; B29C48/36; B29C48/50; B29C48/505; B29C48/52; B29C48/525; B29C48/53; B30; B30B; B30B11/00; B30B11/22; B30B11/24; Y; Y10; Y10S; Y10S426/00; Y10S426/802

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 121 words
A method for texturizing protein products comprising the steps of forming a wet protein dough containing a heat-coagulable protein, passing said dough through a conveyor comprised of a barrel having a constant internal diameter and a rotatable screw therein, said screw having a root of increasing diameter and helical flights thereon of an increasing helix angle, said root of increasing diameter and said increasing helix angle being such that the volume of dough in any 360° turn of the screw is substantially constant, and heating said dough while passing through said conveyor to a temperature above the heat-coagulation temperature of the heat-coagulable protein in said dough to provide a meat-like fiber structure wherein the fibers are aligned in a curvi-linear manner.
Claim 2
Independent Claim 121 words
A method for texturizing protein products comprising the steps of forming a wet protein dough containing a heat-coagulable protein, passing said dough through a conveyor comprised of a barrel having a constant internal diameter and a rotatable screw therein, said screw having a root of increasing diameter and helical flights thereon of an increasing helix angle, said root of increasing diameter and said increasing helix angle being such that the volume of dough in any 360° turn of the screw is substantially constant, and heating said dough while passing through said conveyor to a temperature above the heat-coagulation temperature of the heat-coagulable protein in said dough to provide a meat-like fiber structure wherein the fibers are aligned in a curvi-linear manner.
Claim 3
Dependent Claim 80 words
A method according to claim 1 wherein the step of forming a wet protein dough comprises the steps of forming a protein mix containing from 30% to 100% by weight of a heat coagulable protein, adjusting the moisture content of the protein mix to form a wet protein dough having a moisture content of from 20% to 80% by weight of the dough, and mixing the dough at a temperature less than the heat coagulation temperature of the protein therein.
Claim 4
Dependent Claim 25 words
A method as defined in claim 2, wherein said dough is heated to a temperature in said conveyor of between 170° F. to 300° F.
Claim 5
Independent Claim 161 words
A method for texturizing protein products comprising the steps of forming a wet protein dough containing heat coagulable protein, passing said dough through a conveyor comprised of a barrel of an increasing internal diameter, said barrel having a rotatable screw therein, said screw having a root of increasing diameter, said root diameter increasing at a rate greater than the increase in the internal diameter of the barrel, and helical flights on said screw root, said helical flights being of a decreasing helix angle, the rate of increase of the internal diameter of the barrel, the rate of increase of the diameter of the screw root, and the decreasing helix angle, being such that the dough volume in each 360° turn of the screw is substantially constant, and heating said protein dough while passing through said conveyor to a temperature about the heat-coagulation temperature of the heat-coagulable protein in said dough to provide a meat-like fiber structure wherein the fibers are oriented.
Claim 6
Independent Claim 161 words
A method for texturizing protein products comprising the steps of forming a wet protein dough containing heat coagulable protein, passing said dough through a conveyor comprised of a barrel of an increasing internal diameter, said barrel having a rotatable screw therein, said screw having a root of increasing diameter, said root diameter increasing at a rate greater than the increase in the internal diameter of the barrel, and helical flights on said screw root, said helical flights being of a decreasing helix angle, the rate of increase of the internal diameter of the barrel, the rate of increase of the diameter of the screw root, and the decreasing helix angle, being such that the dough volume in each 360° turn of the screw is substantially constant, and heating said protein dough while passing through said conveyor to a temperature about the heat-coagulation temperature of the heat-coagulable protein in said dough to provide a meat-like fiber structure wherein the fibers are oriented.
Claim 7
Dependent Claim 78 words
A method according to claim 4 wherein the step of forming a wet protein dough comprises the steps of forming a protein mix containing from 30% to 100% by weight of a heat-coagulable protein, adjusting the moisture content of the protein mix to form a wet protein dough having a moisture content of from 20% to 80% by weight of the dough, and mixing the dough at a temperature less than the heat-coagulation temperature of the protein therein.
Claim 8
Dependent Claim 25 words
A method as defined in claim 4, wherein said dough is heated to a temperature in said conveyor of between 170° F. to 300° F.
Claim 9
Dependent Claim 56 words
A method according to claim 1 wherein said conveyor additionally includes a compaction section wherein said barrel has a constant internal diameter and said screw root is of an increasing diameter while said helix angle remains constant such that the volume of dough in any 360° turn of the screw diminishes in the direction of conveying.
Claim 10
Dependent Claim 19 words
A method as defined in claim 1 wherein said conveyor additionally comprises a mixing section and a compaction section.
Claim 11
Dependent Claim 20 words
A method according to claim 1 including the step of discharging the meat-like fiber structure from said conveyor into air.

References Cited (Backward Citations)

US2384521A Cited
US3230902A Cited
US3498793A Cited
US3336137A Cited
US3664795A Cited
US3728053A Cited
US3693533A Cited
US3822361A Cited
US3904769A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-11-13 1982-05-15 1982-11-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-11-13 1986-05-15 1986-11-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-11-13 1990-05-15 1990-11-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag