Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
198 words
Method for making a slub yarn, the method comprising: (a) feeding a yarn bundle of individual continuous filaments from a source of supply to and through a first fluid jet device having cocurrent and countercurrent fluid flows therethrough and thereby randomly breaking some of the individual filaments at random intervals along the length of the yarn bundle, (b) maintaining at the same time a drafting force on the yarn bundle sufficient to prevent the broken filaments from entangling with the yarn bundle and to enhance filament breaking, the drafting force being exerted under ambient temperature conditions between two moving surfaces, the linear speeds of which are adjusted such that the drafting force is no more than 1.2 grams per denier; (c) passing the yarn bundle with the nonentangled broken filaments to and through a second fluid jet device having cocurrent and countercurrent fluid flows therethrough and by such fluid flows sliding the broken filaments along the yarn bundle and entangling them with the yarn bundle and thereby forming the broken filaments into slubs; and (d) taking up the yarn bundle at a slower speed than the speed at which the yarn bundle enters the second fluid jet device.
Claim 2
Dependent Claim
198 words
Method for making a slub yarn, the method comprising: (a) feeding a yarn bundle of individual continuous filaments from a source of supply to and through a first fluid jet device having cocurrent and countercurrent fluid flows therethrough and thereby randomly breaking some of the individual filaments at random intervals along the length of the yarn bundle, (b) maintaining at the same time a drafting force on the yarn bundle sufficient to prevent the broken filaments from entangling with the yarn bundle and to enhance filament breaking, the drafting force being exerted under ambient temperature conditions between two moving surfaces, the linear speeds of which are adjusted such that the drafting force is no more than 1.2 grams per denier; (c) passing the yarn bundle with the nonentangled broken filaments to and through a second fluid jet device having cocurrent and countercurrent fluid flows therethrough and by such fluid flows sliding the broken filaments along the yarn bundle and entangling them with the yarn bundle and thereby forming the broken filaments into slubs; and (d) taking up the yarn bundle at a slower speed than the speed at which the yarn bundle enters the second fluid jet device.
Claim 3
Dependent Claim
13 words
Method as defined in claim 1, wherein the fluid flows are compressed gasses.
Claim 4
Dependent Claim
71 words
Method as defined in claim 1, wherein said first fluid jet device has about 25% of the volume of fluid flow flowing countercurrent to the direction of movement of the yarn bundle and about 75% of the volume of fluid flow flowing cocurrent, and said second fluid jet device has about 50% of the volume of fluid flow flowing countercurrent and about 50% of the volume of fluid flow flowing cocurrent.
Claim 5
Dependent Claim
39 words
Method as defined in claim 3, wherein the fluid flow for said first fluid jet device is about 5-20 S.C.F.M. at about 20-100 p.s.i.g. and for said second fluid jet device is about 8-30 S.C.F.M. at about 50-200 p.s.i.g.
Claim 6
Dependent Claim
78 words
Method as defined in claim 1, wherein a second yarn bundle of individual continuous filaments is fed from a separate source of supply to join the first-mentioned yarn bundle prior to the latter passing through the second fluid jet device, and wherein the broken filaments of the first-mentioned yarn bundle are entangled to make aesthetically desirable slubs with both the first-mentioned and second yarn bundles as the two yarn bundles pass together through the second fluid jet device.