US4124675A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process of insert molding of teflon tube and plastic body
Assignee: Taut Inc
•
Filing: 1978-02-10
•
Granted: 1978-11-07
•
Expires: 1998-02-10
Abstract
Abstract A process of molding a teflon tube to a plastic body which includes the steps of jacketing an end zone of a tube of teflon with a sleeve of plastic and with a portion of the teflon extending from the sleeve and heating the extending zone of the teflon so that in response to the heat the teflon curls about the plastic forming a mechanical lock and molding plastic about the plastic sleeve at the end to form a bond and mechanical lock.
Inventors
- 👤 Richard H. McFarlane
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-06 13:57
CPC Classifications
B; B29; B29C; B29C66/00; B29C66/80; B29C66/83; B29C66/832; B29C66/8322; B29C57/00; B29C65/00; B29C65/56; B29C65/567; B29C65/568; B29C66/01; B29C66/05; B29C66/10; B29C66/13; B29C66/131; B29C66/135; B29C66/50; B29C66/51; B29C66/53; B29C66/534; B29C66/5344; B29C66/70; B29C66/71; B29C66/81; B29C66/814; B29C66/8141; B29C66/81427; B29C66/81429; B29C66/81431; B29C66/532; B29C66/5324; B29C66/53241; B29C66/81411; B29C66/81421; B29C66/81422; B29C66/81423; B29K; B29K2027/00; B29K2027/12; B29K2027/18; B29L; B29L2031/00; B29L2031/753; B29L2031/7542; B29L2031/7544
Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
202 words
The process of insert molding a Teflon tube in a plastic body, comprising the steps of: first, holding a Teflon tube in a fixed axial position at a zone spaced from one end of the tube, the space between said zone and said one end of the tube being of a predetermined axial length having a terminal mouth, second, positioning a plastic sleeve of predetermined wall thickness closely about said predetermined axial length of said tube, said sleeve being of an axial length less than said predetermined length defining and extending terminal end zone of the Teflon tube. annular recess symmetrically about said nose with the surface of said nose defining the interior wall of said recess, said annular recess terminating at an edge spaced radially outwardly from said nose a distance greater than the sum of twice the thickness of said tube plus the thickness of said sleeve, said recess being generally semi-circular as seen in an elevation cross sectional view, fourth, advancing the nose of said heated tool into the mouth of the tube to initiate bending of the mouth and extending terminal end zone of the tube back upon itself with the mouth spaced radially outwardly of the tube,
Claim 2
Dependent Claim
202 words
The process of insert molding a Teflon tube in a plastic body, comprising the steps of: first, holding a Teflon tube in a fixed axial position at a zone spaced from one end of the tube, the space between said zone and said one end of the tube being of a predetermined axial length having a terminal mouth, second, positioning a plastic sleeve of predetermined wall thickness closely about said predetermined axial length of said tube, said sleeve being of an axial length less than said predetermined length defining and extending terminal end zone of the Teflon tube. annular recess symmetrically about said nose with the surface of said nose defining the interior wall of said recess, said annular recess terminating at an edge spaced radially outwardly from said nose a distance greater than the sum of twice the thickness of said tube plus the thickness of said sleeve, said recess being generally semi-circular as seen in an elevation cross sectional view, fourth, advancing the nose of said heated tool into the mouth of the tube to initiate bending of the mouth and extending terminal end zone of the tube back upon itself with the mouth spaced radially outwardly of the tube,
Claim 3
Dependent Claim
136 words
fifth, continuing to advance the tool and melting the plastic of the sleeve between the turned back portion of the tube and the wall of the tube forming a relatively thick annular ring of plastic between the Teflon of the turned back portion and the tube, sixth, holding said heated tool in the mouth until the brink end of the mouth portion of the Teflon tube is turned back toward the tube and over the plastic ring at the zone of juncture of the plastic ring and the sleeve to captivate the melted plastic ring of the end of the plastic sleeve between the Teflon, seventh, removing the nose of the heated tool from the tube, eighth, releasing the jaws, and ninth, insert molding and plastic piece about said ring and a portion of said sleeve.
Claim 4
Dependent Claim
136 words
fifth, continuing to advance the tool and melting the plastic of the sleeve between the turned back portion of the tube and the wall of the tube forming a relatively thick annular ring of plastic between the Teflon of the turned back portion and the tube, sixth, holding said heated tool in the mouth until the brink end of the mouth portion of the Teflon tube is turned back toward the tube and over the plastic ring at the zone of juncture of the plastic ring and the sleeve to captivate the melted plastic ring of the end of the plastic sleeve between the Teflon, seventh, removing the nose of the heated tool from the tube, eighth, releasing the jaws, and ninth, insert molding and plastic piece about said ring and a portion of said sleeve.
Claim 5
Dependent Claim
15 words
The process as set forth in claim 1 wherein the plastic sleeve is of polypropylene.
Claim 6
Dependent Claim
16 words
The process as set forth in claim 1 wherein said plastic piece is made of elastomer.
Claim 7
Dependent Claim
12 words
The process of claim 3 wherein said elastomer is a styrene-butadiene composition.
Claim 8
Dependent Claim
28 words
The process of claim 1 including the steps of releasing jaws holding said tube and molding a plastic piece about said ring and a portion of said sleeve.
Claim 9
Dependent Claim
68 words
The process as set forth in claim 5 wherein said insert molding includes the step of forming a passageway in the piece axially aligned with said tube and wherein the outside diameter of the passageway is greater than the inside diameter of the tube and less than the outside diameter of the plastic ring, to captivate the tube against axial displacement relative to the plastic of the piece.
Claim 10
Dependent Claim
14 words
The process as set forth in claim 2 wherein the sleeve is of polypropylene.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-11-06 | 1982-05-08 | 1982-11-07 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-11-06 | 1986-05-08 | 1986-11-07 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-11-06 | 1990-05-08 | 1990-11-07 | $7700.00 | Window Closed / Lapsed |