Abstract

Abstract A room temperature electrolyte comprising a fused salt mixture of aluminum trichloride and an alkyl pyridinium chloride wherein the alkyl radical is selected from the group consisting of ethyl, methyl, 1-propyl and 1-butyl radicals.

Inventors

  • 👤 John C. Nardi
  • 👤 Charles L. Hussey
  • 👤 Lowell A. King

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 17:23
CPC Classifications
H; H01; H01M; H01M10/00; H01M10/36; H01M6/00; H01M6/14; Y; Y02; Y02E; Y02E60/00; Y02E60/10

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 37 words
A room temperature molten, fused salt electrolytic composition comprising a mixture of; (1) aluminum trichloride and (2) a 1-alkyl pyridinium chloride wherein said alkyl radical is selected from the group consisting of methyl, ethyl, 1-propyl and 1-butyl.
Claim 2
Dependent Claim 37 words
A room temperature molten, fused salt electrolytic composition comprising a mixture of; (1) aluminum trichloride and (2) a 1-alkyl pyridinium chloride wherein said alkyl radical is selected from the group consisting of methyl, ethyl, 1-propyl and 1-butyl.
Claim 3
Dependent Claim 21 words
A room temperature molten, fused salt electrolytic composition comprising a 2:1 molar ratio mixture of aluminum trichloride and methyl pyridinium chloride.
Claim 4
Dependent Claim 21 words
A room temperature molten, fused salt electrolytic composition comprising a 2:1 molar ratio mixture of aluminum trichloride and methyl pyridinium chloride.
Claim 5
Dependent Claim 21 words
A room temperature molten, fused salt, electrolytic composition comprising a 2:1 molar ratio mixture of aluminum trichloride and ethyl pyridinium chloride.
Claim 6
Dependent Claim 21 words
A room temperature molten, fused salt, electrolytic composition comprising a 2:1 molar ratio mixture of aluminum trichloride and ethyl pyridinium chloride.
Claim 7
Dependent Claim 21 words
A room temperature molten, fused salt, electrolytic composition comprising a 2:1 molar ratio mixture of aluminum trichloride and 1-propyl pyridinium chloride.
Claim 8
Dependent Claim 21 words
A room temperature molten, fused salt, electrolytic composition comprising a 2:1 molar ratio mixture of aluminum trichloride and 1-propyl pyridinium chloride.
Claim 9
Dependent Claim 21 words
A room temperature molten fused salt, electrolytic composition comprising a 2:1 molar ratio mixture of aluminum trichloride and 1-butyl pyridinium chloride.
Claim 10
Dependent Claim 21 words
A room temperature molten fused salt, electrolytic composition comprising a 2:1 molar ratio mixture of aluminum trichloride and 1-butyl pyridinium chloride.

References Cited (Backward Citations)

US3073884A Cited
US3423242A Cited
US3819415A Cited
US3542602A Cited
US3562017A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-10-23 1982-04-24 1982-10-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-10-23 1986-04-24 1986-10-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-10-23 1990-04-24 1990-10-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag