Formation of colloidal dispersions of selenium by the locus control method
Assignee: Xerox Corp
•
Filing: 1977-09-19
•
Granted: 1978-10-24
•
Expires: 1997-09-19
Abstract
Abstract The present invention is a method for preparing a colloidal dispersion of selenium by the locus control process. In one embodiment the method involves adding hydrazine to a solution containing submicron sized domains of a soluble second phase which domains bear a plurality of pendant acid groups to form a salt between the hydrazine and pendant acid groups. Addition of selenous acid to the solution results in reduction of the selenium contained therein to zero valent selenium which selenium is produced in the form of a stable colloidal dispersion.
Inventors
- 👤 Thomas W. Smith
- 👤 Wolfgang H. H. Gunther
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 20:04
CPC Classifications
B; B01; B01J; B01J13/00; B01J13/0004; B01J13/0008; B01J13/0013; B82; B82Y; B82Y30/00; C; C01; C01B; C01B19/00; C01B19/02; G; G03; G03G; G03G5/00; G03G5/02; G03G5/04; G03G5/08; G03G5/087; C01P; C01P2004/00; C01P2004/60; C01P2004/62; C01P2004/64
Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
120 words
A method of forming a stable, colloidal dispersion of selenium which comprises: (a) providing a solution of a solvent containing submicron domains of a soluble second phase, the domains being comprised of a hydrazine substituted poly (acrylic acid) and being capable of reducing selenous acid or alkyl selenite to selenium; (b) adding selenous acid or an alkyl selenite corresponding to the following formula: ##STR3## wherein R 2 and R 3 are independently H or alkyl of 1 to 20 carbon atoms and R 4 is an alkylene radical of 1 to 20 carbon atoms, to the solution to reduce the selenium in the selenous acid or alkyl selenite to zero valent selenium and thereby form the colloidal dispersion of selenium.
Claim 2
Independent Claim
120 words
A method of forming a stable, colloidal dispersion of selenium which comprises: (a) providing a solution of a solvent containing submicron domains of a soluble second phase, the domains being comprised of a hydrazine substituted poly (acrylic acid) and being capable of reducing selenous acid or alkyl selenite to selenium; (b) adding selenous acid or an alkyl selenite corresponding to the following formula: ##STR3## wherein R 2 and R 3 are independently H or alkyl of 1 to 20 carbon atoms and R 4 is an alkylene radical of 1 to 20 carbon atoms, to the solution to reduce the selenium in the selenous acid or alkyl selenite to zero valent selenium and thereby form the colloidal dispersion of selenium.
Claim 3
Dependent Claim
15 words
The method of claim 1 wherein the second phase is a hydrazine substituted poly(acrylic acid).
Claim 4
Independent Claim
130 words
A method of forming a stable, colloidal dispersion of selenium which comprises: (a) providing a solution of a solvent containing submicron domains of a soluble second phase, the domains being comprised of a hydrazine substituted copolymer of (styrene/acrylic acid), or a copolymer of (styrene/methacrylic acid) and said domains being capable of reducing selenous acid or alkyl selenite to selenium; (b) adding selenous acid or an alkyl selenite corresponding to the following formula: ##STR4## wherein R 2 and R 3 are independently H or alkyl of 1 to 20 carbon atoms and R 4 is an alkylene radical of 1 to 20 carbon atoms to the solution to reduce the selenium in the selenous acid or alkyl selenite to zero valent selenium and thereby form the colloidal dispersion of the selenium.
Claim 5
Independent Claim
130 words
A method of forming a stable, colloidal dispersion of selenium which comprises: (a) providing a solution of a solvent containing submicron domains of a soluble second phase, the domains being comprised of a hydrazine substituted copolymer of (styrene/acrylic acid), or a copolymer of (styrene/methacrylic acid) and said domains being capable of reducing selenous acid or alkyl selenite to selenium; (b) adding selenous acid or an alkyl selenite corresponding to the following formula: ##STR4## wherein R 2 and R 3 are independently H or alkyl of 1 to 20 carbon atoms and R 4 is an alkylene radical of 1 to 20 carbon atoms to the solution to reduce the selenium in the selenous acid or alkyl selenite to zero valent selenium and thereby form the colloidal dispersion of the selenium.
Claim 6
Independent Claim
126 words
A method of forming a stable, colloidal dispersion of selenium which comprises: (a) providing a solution of a solvent containing submicron domains of a soluble second phase, the domains being comprised of a homo or copolymer of an unsaturated carboxylic acid, and said domains being capable of reducing selenous acid or alkyl senenite to selenium; (b) adding selenous acid or an alkyl selenite corresponding to the following formula: ##STR5## wherein R 2 and R 3 are independently H or alkyl of 1 to 20 carbon atoms and R 4 is an alkylene radical of 1 to 20 carbon atoms, to the solution to reduce the selenium in the selenous acid or alkyl selenite to zero valent selenium and thereby form the colloidal dispersion of the selenium.
Claim 7
Independent Claim
126 words
A method of forming a stable, colloidal dispersion of selenium which comprises: (a) providing a solution of a solvent containing submicron domains of a soluble second phase, the domains being comprised of a homo or copolymer of an unsaturated carboxylic acid, and said domains being capable of reducing selenous acid or alkyl senenite to selenium; (b) adding selenous acid or an alkyl selenite corresponding to the following formula: ##STR5## wherein R 2 and R 3 are independently H or alkyl of 1 to 20 carbon atoms and R 4 is an alkylene radical of 1 to 20 carbon atoms, to the solution to reduce the selenium in the selenous acid or alkyl selenite to zero valent selenium and thereby form the colloidal dispersion of the selenium.
Claim 8
Dependent Claim
20 words
The method of claim 4 wherein the soluble second phase is a homo or copolymer of an unsaturated carboxylic acid.
Claim 9
Independent Claim
130 words
A method of forming a stable, colloidal dispersion of selenium which comprises: (a) providing a solution of a solvent containing submicron domains of a soluble second phase, the domains being comprised of a hydrazine substituted poly(2-methyl-2-acrylamido propane-sulfonic acid), p-styrene sulfonic acid or vinyl sulfonic acid, and said domains being capable of reducing selenous acid or alkyl selenite to selenium; (b) adding selenous acid or an alkyl selenite corresponding to the following formula: ##STR6## wherein R 2 and R 3 are independently H or alkyl of 1 to 20 carbon atoms and R 4 is an alkylene radical of 1 to 20 carbon atoms, to the solution to reduce the selenium in the selenous acid or alkyl selenite to zero valent selenium and thereby form the colloidal dispersion of the selenium.
Claim 10
Independent Claim
130 words
A method of forming a stable, colloidal dispersion of selenium which comprises: (a) providing a solution of a solvent containing submicron domains of a soluble second phase, the domains being comprised of a hydrazine substituted poly(2-methyl-2-acrylamido propane-sulfonic acid), p-styrene sulfonic acid or vinyl sulfonic acid, and said domains being capable of reducing selenous acid or alkyl selenite to selenium; (b) adding selenous acid or an alkyl selenite corresponding to the following formula: ##STR6## wherein R 2 and R 3 are independently H or alkyl of 1 to 20 carbon atoms and R 4 is an alkylene radical of 1 to 20 carbon atoms, to the solution to reduce the selenium in the selenous acid or alkyl selenite to zero valent selenium and thereby form the colloidal dispersion of the selenium.
References Cited (Backward Citations)
US3130012A
Cited
US3962113A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-10-23 | 1982-04-24 | 1982-10-24 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-10-23 | 1986-04-24 | 1986-10-24 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-10-23 | 1990-04-24 | 1990-10-24 | $7700.00 | Window Closed / Lapsed |