Claims Analysis
Total Claims: 19
Claim 1
Independent Claim
52 words
A method for recovering nickel from waste materials containing nickel which comprises the steps of (a) subjecting a mixture of the waste material and a nickel-containing ore to oxidizing conditions at an elevated temperature, (b) melting the oxidized mixture, (c) subjecting the melt to reducing conditions, and (d) recovering the desired nickel.
Claim 2
Independent Claim
52 words
A method for recovering nickel from waste materials containing nickel which comprises the steps of (a) subjecting a mixture of the waste material and a nickel-containing ore to oxidizing conditions at an elevated temperature, (b) melting the oxidized mixture, (c) subjecting the melt to reducing conditions, and (d) recovering the desired nickel.
Claim 3
Dependent Claim
22 words
The method of claim 1 wherein the mixture of waste nickel and ore is melted at a temperature of about 1600°-1700° C.
Claim 4
Dependent Claim
24 words
The method of claim 2 wherein a reducing agent containing silicon or carbon is added to the melted mixture of waste nickel and ore.
Claim 5
Dependent Claim
14 words
The method of claim 1 wherein the waste nickel is a spent nickel catalyst.
Claim 6
Dependent Claim
18 words
The method of claim 4 wherein the spent nickel catalyst is recovered from hydrogenation of fatty organic compounds.
Claim 7
Independent Claim
77 words
A method of improving the nickel content of ferronickel obtained from ores containing nickel and iron which comprises (a) oxidizing amixture of spent nickel catalyst and the ore containing nickel and iron at an elevated temperature, (b) heating the mixture at a temperature sufficient to melt the oxidized ore and nickel catalyst (c) adding a reducing agent to the melt, (d) vigorously mixing the melt and reducing agent whereby ferronickel is formed, and (e) recovering the ferronickel.
Claim 8
Independent Claim
77 words
A method of improving the nickel content of ferronickel obtained from ores containing nickel and iron which comprises (a) oxidizing amixture of spent nickel catalyst and the ore containing nickel and iron at an elevated temperature, (b) heating the mixture at a temperature sufficient to melt the oxidized ore and nickel catalyst (c) adding a reducing agent to the melt, (d) vigorously mixing the melt and reducing agent whereby ferronickel is formed, and (e) recovering the ferronickel.
Claim 9
Dependent Claim
21 words
The method of claim 6 wherein the mixture in step a) comprises from about 1 to about 10% of spent catalyst.
Claim 10
Dependent Claim
20 words
The method of claim 6 wherein the ore is dried and size graded prior to mixing with the spent catalyst.
Claim 11
Dependent Claim
26 words
The method of claim 6 wherein the oxidation of the mixture of ore and catalyst is conducted at a temperature of up to about 925°-955° C.
Claim 12
Dependent Claim
22 words
The method of claim 6 wherein the reducing agent added to the melt in step (c) is silicon, a ferrosilicon or carbon.
Claim 13
Dependent Claim
14 words
The method of claim 10 wherein the ferrosilicon agent contains from about 45-55% silicon.
Claim 14
Dependent Claim
21 words
The method of claim 6 wherein the spent catalyst is a nickel catalyst recovered from hydrogenation, alkylation, hydroalkylation, or cracking reactions.
Claim 15
Dependent Claim
29 words
The method of claim 11 wherein the catalyst is a spent nickel catalyst recovered from the hydrogenation of oils and has a fuel value of up to 11,000 BTU/lb.
Claim 16
Independent Claim
126 words
A method of improving the recovery of ferronickel from ores containing nickel and iron utilizing spent nickel catalysts containing fuel values which comprises (a) advancing and oxidizing the ore in a multiple hearth oxidizing furnace at an elevated temperature, (b) feeding the spent nickel catalyst into the furnace at about the mid point of the advancement of the ore through the multiple hearth furnace whereby the fuel values of the catalyst are used to raise or maintain the temperature within the furnace and any oxidizable nickel in the catalyst is oxidized to nickel oxide, (c) removing the oxidized ore and catalyst mixture from the furnace, (d) melting the oxidized mixture, (e) subjecting the melted mixture to reducing conditions to form ferronickel, and (f) recovering the ferronickel.
Claim 17
Independent Claim
126 words
A method of improving the recovery of ferronickel from ores containing nickel and iron utilizing spent nickel catalysts containing fuel values which comprises (a) advancing and oxidizing the ore in a multiple hearth oxidizing furnace at an elevated temperature, (b) feeding the spent nickel catalyst into the furnace at about the mid point of the advancement of the ore through the multiple hearth furnace whereby the fuel values of the catalyst are used to raise or maintain the temperature within the furnace and any oxidizable nickel in the catalyst is oxidized to nickel oxide, (c) removing the oxidized ore and catalyst mixture from the furnace, (d) melting the oxidized mixture, (e) subjecting the melted mixture to reducing conditions to form ferronickel, and (f) recovering the ferronickel.
Claim 18
Dependent Claim
27 words
The method of claim 14 wherein the multiple hearth furnace is a ten hearth Herreschaft furnace and the spent nickel catalyst is fed to the fifth hearth.
Claim 19
Dependent Claim
42 words
The method of claim 14 wherein the normal fuel input to the furnace is reduced by up to about 60% and the desired temperature within the furnace is maintained by controlling the feed rate of the spent nickel catalyst to the furnace.