US4114956A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Transporting iron ore slurries
Assignee: Chevron USA Inc
•
Filing: 1976-02-05
•
Granted: 1978-09-19
•
Expires: 1996-02-05
Abstract
Abstract Method of transporting iron ore by forming an aqueous slurry containing by volume 20 to 45 percent iron ore; from 0.02 to 0.4 percent by weight based on iron ore in the slurry of a dispersant; and from 0.01 to 0.2 percent by weight based on water in the slurry of an organic polymer and moving the slurry through a pipeline.
Inventors
- 👤 Harley Y. Jennings, Jr.
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-04 01:52
CPC Classifications
B; B65; B65G; B65G53/00; B65G53/04; B65G53/30; Y; Y10; Y10T; Y10T137/00; Y10T137/0318; Y10T137/0391
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
105 words
A method of pipelining iron ore comprising forming an aqueous slurry of iron ore particles of from 20 to 45 percent by volume, from 0.02 to 0.4 percent by weight based on iron ore content of the slurry of an ionic dispersant to contact the iron ore particles to impart negative charges thereon and from 0.01 to 0.2 percent by weight based on water content of the slurry of a nonionic organic polymer to increase the carrying capacity of the slurry for coarse iron ore particles, moving said slurry through a pipeline and recovering the iron ore particles from the slurry at a downline location.
Claim 2
Independent Claim
105 words
A method of pipelining iron ore comprising forming an aqueous slurry of iron ore particles of from 20 to 45 percent by volume, from 0.02 to 0.4 percent by weight based on iron ore content of the slurry of an ionic dispersant to contact the iron ore particles to impart negative charges thereon and from 0.01 to 0.2 percent by weight based on water content of the slurry of a nonionic organic polymer to increase the carrying capacity of the slurry for coarse iron ore particles, moving said slurry through a pipeline and recovering the iron ore particles from the slurry at a downline location.
Claim 3
Dependent Claim
36 words
The method of claim 1 further characterized in that the organic polymer is high molecular weight water-soluble polyacrylamide in an amount of from 0.01 to 0.05 percent by weight based on water content of the slurry.
Claim 4
Dependent Claim
31 words
The method of claim 1 further characterized in that the organic polymer is guar gum in an amount of from 0.05 to 0.2 percent based on water content of the slurry.
Claim 5
Dependent Claim
51 words
The method of claim 1 further characterized in that all of the iron ore particles pass a 10 mesh screen, 95 percent of the particles pass a 65 mesh screen, 80 percent of the particles pass a 200 mesh screen and 70 percent of the particles pass a 325 mesh screen.
Claim 6
Dependent Claim
32 words
The method of claim 1 further characterized in that the dispersant is lignosulfonate in an amount of from 0.05 to 0.2 percent by weight based on iron ore content of the slurry.
Claim 7
Dependent Claim
32 words
The method of claim 2 further characterized in that the dispersant is lignosulfonate in an amount of from 0.05 to 0.2 percent by weight based on iron ore content of the slurry.
Claim 8
Dependent Claim
32 words
The method of claim 3 further characterized in that the dispersant is lignosulfonate in an amount of from 0.05 to 0.2 percent by weight based on iron ore content of the slurry.
Claim 9
Dependent Claim
14 words
The method of claim 1 further characterized in that the iron ore is hematite.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-09-18 | 1982-03-20 | 1982-09-19 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-09-18 | 1986-03-20 | 1986-09-19 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-09-18 | 1990-03-20 | 1990-09-19 | $7700.00 | Window Closed / Lapsed |