Patent US4219520A successfully refreshed from Google Patents.
US4112222A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method of preparing hydroxypropylated starch derivatives
Assignee: Ingredion Inc
•
Filing: 1977-01-07
•
Granted: 1978-09-05
•
Expires: 1997-01-07
Abstract
Abstract An improved method for producing granular, cold-water dispersible hydroxypropylated starch derivatives comprises reacting a granular starch base with propylene oxide in the presence of sodium acetate or another water-soluble salt of a selected carboxylic acid. The resulting starch product, which upon purification is free of toxic by-products and has no perceptible off-taste, finds use as a thickener in food as well as in non-food applications.
Inventors
- 👤 Wadym Jarowenko
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-05 06:45
CPC Classifications
C; C08; C08B; C08B31/00; C08B31/08; C08B31/12
Claims Analysis
Total Claims: 26
Claim 1
Independent Claim
149 words
In a method for producing a granular, cold-water dispersible hydroxypropylated starch ether which comprises reacting a granular starch base having a moisture content of 6-20% based on the weight of the starch with about 15-50% propylene oxide by weight, said reaction being carried out for about 4.5-24 hours at a temperature of about 70°-100° C. and at a pressure of about 10-100 p.s.i.g., the improvement comprising the steps of: (a) impregnating said starch base with about 0.25-5.0%, based on the weight of the dry starch base, of a catalyst salt in aqueous solution form, said salt being a water-soluble alkali or alkali earth salt of a carboxylic acid which is unsubstituted or alkyl- or hydroxy-substituted, having no more than 20 carbon atoms in total, and, if aliphatic, having 1 to 6 carbon atoms in its primary carbon chain; and (b) conducting said reaction in the presence of said salt.
Claim 2
Dependent Claim
149 words
In a method for producing a granular, cold-water dispersible hydroxypropylated starch ether which comprises reacting a granular starch base having a moisture content of 6-20% based on the weight of the starch with about 15-50% propylene oxide by weight, said reaction being carried out for about 4.5-24 hours at a temperature of about 70°-100° C. and at a pressure of about 10-100 p.s.i.g., the improvement comprising the steps of: (a) impregnating said starch base with about 0.25-5.0%, based on the weight of the dry starch base, of a catalyst salt in aqueous solution form, said salt being a water-soluble alkali or alkali earth salt of a carboxylic acid which is unsubstituted or alkyl- or hydroxy-substituted, having no more than 20 carbon atoms in total, and, if aliphatic, having 1 to 6 carbon atoms in its primary carbon chain; and (b) conducting said reaction in the presence of said salt.
Claim 3
Dependent Claim
19 words
The method of claim 1 wherein said carboxylic acid is an aliphatic monocarboxylic acid, dicarboxylic acid or tricarboxylic acid.
Claim 4
Dependent Claim
21 words
The method of claim 2 wherein said carboxylic acid is selected from the group consisting of ascorbic, citric and tartaric acid.
Claim 5
Dependent Claim
12 words
The method of claim 2 wherein said carboxylic acid is acetic acid.
Claim 6
Dependent Claim
14 words
The method of claim 1 wherein said salt is sodium acetate or potassium acetate.
Claim 7
Dependent Claim
26 words
The method of claim 1 wherein said starch base is impregnated with about 0.50-1.50%, based on the weight of the dry starch base, of said salt.
Claim 8
Dependent Claim
30 words
The method of claim 1 wherein said reaction is carried out for about 5.0-10 hours at a temperature of about 90°-98° C. and at a pressure of about 30-35 p.s.i.g.
Claim 9
Dependent Claim
18 words
The method of claim 1 wherein said starch base is reacted with about 20-30% propylene oxide by weight.
Claim 10
Dependent Claim
22 words
The method of claim 1 wherein said starch base has a moisture content of 10-17% based on the weight of the starch.
Claim 11
Dependent Claim
48 words
The method of claim 1 wherein said catalyst salt is a sodium or potassium salt, said carboxylic acid being selected from the group consisting of acetic, ascorbic, citric and tartaric acid, and said starch base impregnated with said salt is reacted with about 20-25% propylene oxide by weight.
Claim 12
Dependent Claim
19 words
The method of claim 1 wherein said salt is added directly to an aqueous slurry of said starch base.
Claim 13
Dependent Claim
19 words
The method of claim 1 wherein said salt is formed in situ in a slurry of said starch base.
Claim 14
Dependent Claim
41 words
The method of claim 12 wherein said salt is formed in situ by addition of said acid or an acid-producing material to said starch base, followed by addition of an alkali or alkali earth base to a pH of about 7-10.
Claim 15
Dependent Claim
14 words
The method of claim 13 wherein said acid-producing material is a lactone or anhydride.
Claim 16
Dependent Claim
27 words
The method of claim 13 wherein said salt is formed in situ by addition of said alkali or alkali earth base to a pH of about 7-8.
Claim 17
Dependent Claim
76 words
The method of claim 12 wherein said salt is formed in situ by alternate addition of an alkali or alkali earth base and an acid-producing material to said starch base until said starch base is substituted with up to about 3% by weight of the anionic constituent of said salt and a final pH of 7-10 is obtained, with the slurried substituted starch base being thereafter filtered and dried without washing prior to conducting said reaction.
Claim 18
Dependent Claim
12 words
The method of claim 16 wherein said acid-producing material is an anhydride.
Claim 19
Dependent Claim
35 words
The method of claim 12 wherein after formation of said salt in situ, said slurried starch base is filtered and dried to a moisture content of about 6-20% by weight prior to conducting said reaction.
Claim 20
Dependent Claim
21 words
The method of claim 18 wherein said slurried starch base is dried to a moisture content of about 10-17% by weight.
Claim 21
Dependent Claim
21 words
The method of claim 1 wherein, after said reaction, the starch product is recovered by adjusting the pH to about 3.5-7.0.
Claim 22
Dependent Claim
27 words
The method of claim 20 wherein, after pH adjustment, said starch product is washed with a water-alcohol mixture having a water content of about 10-50% by weight.
Claim 23
Dependent Claim
13 words
The method of claim 21 wherein said water-alcohol mixture is a water-ethanol mixture.
Claim 24
Dependent Claim
21 words
The method of claim 1 wherein said salt is added as a salt-containing solution to said starch base in dry form.
Claim 25
Independent Claim
187 words
A method of producing a granular cold-water dispersible hydroxypropylated starch ether comprising the steps of: (a) impregnating a granular starch base with about 0.25-5.0%, based on the weight of the dry starch base, of a catalyst salt in aqueous solution form, such that said impregnated starch base has a pH of 7-10, said salt being a water-soluble alkali or alkali earth salt of a carboxylic acid which is unsubstituted or alkyl- or hydroxy-substituted, said salt having no more than 20 carbons in total, and, if aliphatic, having from 1 to 6 carbon atoms in its primary carbon chain; (b) drying said impregnated starch base to a moisture content of about 6-20% by weight; (c) reacting said dried starch base without aging thereof with 15-50% by weight of propylene oxide, said reaction being carried out for about 4.5-24 hours at a temperature of about 70°-100° C. and at a pressure of about 10-100 p.s.i.g.; (d) recovering said reacted starch by adjusting the pH to about 3.5-7.0; and (e) washing said reacted starch with a water-alcohol mixture having a water content of about 10-50% and drying said washed starch.
Claim 26
Independent Claim
187 words
A method of producing a granular cold-water dispersible hydroxypropylated starch ether comprising the steps of: (a) impregnating a granular starch base with about 0.25-5.0%, based on the weight of the dry starch base, of a catalyst salt in aqueous solution form, such that said impregnated starch base has a pH of 7-10, said salt being a water-soluble alkali or alkali earth salt of a carboxylic acid which is unsubstituted or alkyl- or hydroxy-substituted, said salt having no more than 20 carbons in total, and, if aliphatic, having from 1 to 6 carbon atoms in its primary carbon chain; (b) drying said impregnated starch base to a moisture content of about 6-20% by weight; (c) reacting said dried starch base without aging thereof with 15-50% by weight of propylene oxide, said reaction being carried out for about 4.5-24 hours at a temperature of about 70°-100° C. and at a pressure of about 10-100 p.s.i.g.; (d) recovering said reacted starch by adjusting the pH to about 3.5-7.0; and (e) washing said reacted starch with a water-alcohol mixture having a water content of about 10-50% and drying said washed starch.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-09-04 | 1982-03-06 | 1982-09-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-09-04 | 1986-03-06 | 1986-09-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-09-04 | 1990-03-06 | 1990-09-05 | $7700.00 | Window Closed / Lapsed |