Method of inhibiting corrosion

Assignee: Individual
•
Filing: 1976-09-29
•
Granted: 1978-09-05
•
Expires: 1996-09-29
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of retarding corrosion of metal parts in an aqueous-containing fluid system which comprises, adding to the aqueous-containing fluid system a mixture of a water-soluble cation of mercury and a water-soluble cation of a Group IB or Group IIB metal.

Inventors

  • 👤 Ramon A. Bannister

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 10:31
CPC Classifications
C; C23; C23F; C23F11/00; C23F11/08; C23F11/18; C23F11/187

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 66 words
A method of inhibiting corrosion of metals which contact aqueous containing fluids which comprises, adding to the fluid a synergistic mixture of water soluble cations in a corrosion inhibiting amount, said synergistic mixture consisting essentially of a mercuric cation and a metal cation selected from the group consisting of Group IB metals, Group IIB metals, and lead; and contacting the metal with the corrosion inhibiting fluid.
Claim 2
Independent Claim 66 words
A method of inhibiting corrosion of metals which contact aqueous containing fluids which comprises, adding to the fluid a synergistic mixture of water soluble cations in a corrosion inhibiting amount, said synergistic mixture consisting essentially of a mercuric cation and a metal cation selected from the group consisting of Group IB metals, Group IIB metals, and lead; and contacting the metal with the corrosion inhibiting fluid.
Claim 3
Dependent Claim 15 words
The method according to claim 1 wherein said fluid is an aqueous chloride-ion containing fluid.
Claim 4
Dependent Claim 26 words
The method according to claim 2 wherein said water-soluble mercuric ion is a member of the group consisting of mercuric nitrate, mercuric acetate and mercuric cyanide.
Claim 5
Dependent Claim 41 words
The method according to claim 3 wherein the concentration of mercuric ion is from 2 parts per million to 5,000 parts per million and the concentration of water-soluble metal cation is from 1 part per million to 50,000 parts per million.
Claim 6
Dependent Claim 25 words
The method according to claim 3 wherein said water-soluble metal cation is selected from the group consisting of zinc, cadmium, copper, gold, silver and lead.
Claim 7
Dependent Claim 23 words
The method according to claim 1 wherein said metal is selected from the group consisting of stainless steel, carbon steel, iron and aluminum.
Claim 8
Dependent Claim 33 words
The method according to claim 3 wherein the concentration of mercuric ion is from 10 ppm. to 1,000 ppm. and the concentration of water-soluble metal cation is from 5 ppm. to 10,000 ppm.

References Cited (Backward Citations)

US3151087A Cited
US3880585A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-09-04 1982-03-06 1982-09-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-09-04 1986-03-06 1986-09-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-09-04 1990-03-06 1990-09-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag