Abstract

Abstract Disclosed is a process wherein a conversion coated zinc or zinc alloy surface is post-treated with an aqueous solution comprising at least 0.02 g/l titanium ion and at least 0.1 g/l of an adjuvant selected from phosphoric acid, phytic acid, tannin, the salts and esters of the foregoing, and hydrogen peroxide.

Inventors

  • 👤 Yasunobu Matsushima
  • 👤 Kuniji Yashiro
  • 👤 Hideaki Kaneko
  • 👤 Masanori Suzuki

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 06:26
CPC Classifications
C; C23; C23C; C23C22/00; C23C22/82; C23C22/83

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 64 words
A chromium-free process for treating an oxide or phosphate conversion coated zinc or zinc alloy surface comprising contacting the surface with an aqueous post-treatment solution comprising at least 0.02 g/l of titanium ion and at least 0.1 g/l of at least one adjuvant selected from the group consisting of phosphoric acid, phytic acid, tannin, the salts or esters of the foregoing and hydrogen peroxide.
Claim 2
Dependent Claim 64 words
A chromium-free process for treating an oxide or phosphate conversion coated zinc or zinc alloy surface comprising contacting the surface with an aqueous post-treatment solution comprising at least 0.02 g/l of titanium ion and at least 0.1 g/l of at least one adjuvant selected from the group consisting of phosphoric acid, phytic acid, tannin, the salts or esters of the foregoing and hydrogen peroxide.
Claim 3
Dependent Claim 23 words
The process of claim 1 wherein the post-treatment solution is adjusted to a pH value in the range of about 2 to 6.
Claim 4
Dependent Claim 11 words
The process of claim 1 wherein the surface is subsequently painted.
Claim 5
Dependent Claim 21 words
The process of claim 1 wherein the titanium ion concentration in the post-treatment solution is not in excess of 5 g/l.
Claim 6
Dependent Claim 15 words
The process of claim 4 wherein the titanium concentration is between 0.05 and 2.5 g/l.
Claim 7
Dependent Claim 20 words
The process of claim 1 wherein the adjuvant concentration in the post-treatment solution is not in excess of 10 g/l.
Claim 8
Dependent Claim 15 words
The process of claim 6 wherein the adjuvant concentration is between 0.2 and 5 g/l.

References Cited (Backward Citations)

US3101286A Cited
US3682713A Cited
US3975214A Cited
US3895970A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-08-28 1982-02-27 1982-08-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-08-28 1986-02-27 1986-08-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-08-28 1990-02-27 1990-08-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag