← Back to Patent Explorer
US4104173A Expired / Lapsed US ⏱️ 0.0 years remaining

Gelling agents for hydrocarbon compounds

Assignee: GE Chemicals Inc
•
Filing: 1975-08-20
•
Granted: 1978-08-01
•
Expires: 1995-08-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In complete, non-stoichiometric aluminum salts of alkyl orthophosphates, when neutralized with a second basic compound, form pseudo double salts which are capable of gelling hydrocarbons when present in low concentrations. The resulting gelled hydrocarbons are useful in cracking or fracturing treatments of oil wells, and exhibit reduced fluid friction in high shear flow systems.

Inventors

  • 👤 Robert L. Gay
  • 👤 Richard J. Schlott
  • 👤 James E. Burroughs

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 15:57
CPC Classifications
C; C07; C07F; C07F9/00; C07F9/02; B; B01; B01J; B01J23/00; B01J23/38; B01J23/54; B01J23/56; B01J23/64; B01J23/656; B01J23/6567; C07F9/06; C07F9/08; C09; C09K; C09K8/00; C09K8/60; C09K8/62; C09K8/64; C10; C10L; C10L7/00; C10L7/02; Y; Y10; Y10S; Y10S507/00; Y10S507/922

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 195 words
A method of making a gelled hydrocarbon composition comprising the steps of (a) preparing a mixture of alkyl acid orthophosphates by reacting phosphorus pentoxide with a mixture of at least two alcohols wherein at least one alcohol is selected from the group consisting of C 1 to C 5 n-alkanols and at least one alcohol is selected from the group consisting of C 6 to C 18 alkanols and C 6 to C 18 alkenols, (b) reacting said mixture of alkyl acid orthophosphates with a basic aluminum compound selected from the group consisting of hydrated alumina and aluminum alkoxides in a ratio of from 2.67 to 8 gram atoms of phosphorus per gram atom of aluminum to produce a partial aluminum salt of the alkyl acid orthophosphates, (c) adding from 0.1 to about 10 parts by weight of said partial aluminum salt to 100 parts by weight of a liquid hydrocarbon, and (d) adding thereto sufficient amount of a second base selected from the group consisting of alkali metal hydroxides, alkali metal oxides, ammonium hydroxide, alkaline earth metal hydroxides, alkaline earth metal oxides, and alkali metal salts of weak acids to neutralize the remaining acidity.
Claim 2
Independent Claim 195 words
A method of making a gelled hydrocarbon composition comprising the steps of (a) preparing a mixture of alkyl acid orthophosphates by reacting phosphorus pentoxide with a mixture of at least two alcohols wherein at least one alcohol is selected from the group consisting of C 1 to C 5 n-alkanols and at least one alcohol is selected from the group consisting of C 6 to C 18 alkanols and C 6 to C 18 alkenols, (b) reacting said mixture of alkyl acid orthophosphates with a basic aluminum compound selected from the group consisting of hydrated alumina and aluminum alkoxides in a ratio of from 2.67 to 8 gram atoms of phosphorus per gram atom of aluminum to produce a partial aluminum salt of the alkyl acid orthophosphates, (c) adding from 0.1 to about 10 parts by weight of said partial aluminum salt to 100 parts by weight of a liquid hydrocarbon, and (d) adding thereto sufficient amount of a second base selected from the group consisting of alkali metal hydroxides, alkali metal oxides, ammonium hydroxide, alkaline earth metal hydroxides, alkaline earth metal oxides, and alkali metal salts of weak acids to neutralize the remaining acidity.
Claim 3
Dependent Claim 23 words
The method of claim 1 further comprising diluting said gelled hydrocarbon composition with from 1 to about 1,000 volumes of a liquid hydrocarbon.
Claim 4
Dependent Claim 239 words
A liquid hydrocarbon composition comprising a liquid hydrocarbon and a minor amount of a gelling agent consisting of the pseudo double salts of alkyl acid orthophosphates with aluminum and a second ion selected from the group consisting of alkali metal, alkaline earth metal and ammonium ions, said pseudo double salt prepared by the steps of (a) preparing a mixture of alkyl acid orthophosphates by reacting phosphorus pentoxide with a mixture of at least two alcohols wherein at least one alcohol is selected from the group consisting of C 1 to C 5 n-alkanols and at least one alcohol is selected from the group consisting of C 6 to C 18 alkanols and C 6 to C 18 alkenols, (b) reacting said mixture of alkyl acid orthophosphates with a basic aluminum compound selected from the group consisting of hydrated of alumina and aluminum alkoxides in a ratio of from 2.67 to 8 gram atoms of phosphorus per gram atom of aluminum to produce a partial aluminum salt of the alkyl acid orthophosphates, (c) adding from 0.1 to about 10 parts by weight of said partial aluminum salt to 100 parts by weight of a liquid hydrocarbon, and (d) adding thereto sufficient amount of a second base selected from the group consisting of alkali metal hydroxides, alkali metal oxides, ammonium hydroxide, alkaline earth metal hydroxides, alkaline earth metal oxides, and alkali metal salts of weak acids to neutralize the remaining acidity.
Claim 5
Dependent Claim 239 words
A liquid hydrocarbon composition comprising a liquid hydrocarbon and a minor amount of a gelling agent consisting of the pseudo double salts of alkyl acid orthophosphates with aluminum and a second ion selected from the group consisting of alkali metal, alkaline earth metal and ammonium ions, said pseudo double salt prepared by the steps of (a) preparing a mixture of alkyl acid orthophosphates by reacting phosphorus pentoxide with a mixture of at least two alcohols wherein at least one alcohol is selected from the group consisting of C 1 to C 5 n-alkanols and at least one alcohol is selected from the group consisting of C 6 to C 18 alkanols and C 6 to C 18 alkenols, (b) reacting said mixture of alkyl acid orthophosphates with a basic aluminum compound selected from the group consisting of hydrated of alumina and aluminum alkoxides in a ratio of from 2.67 to 8 gram atoms of phosphorus per gram atom of aluminum to produce a partial aluminum salt of the alkyl acid orthophosphates, (c) adding from 0.1 to about 10 parts by weight of said partial aluminum salt to 100 parts by weight of a liquid hydrocarbon, and (d) adding thereto sufficient amount of a second base selected from the group consisting of alkali metal hydroxides, alkali metal oxides, ammonium hydroxide, alkaline earth metal hydroxides, alkaline earth metal oxides, and alkali metal salts of weak acids to neutralize the remaining acidity.
Claim 6
Dependent Claim 170 words
A pseudo double salt of an alkyl acid orthophosphate prepared by the steps of (a) preparing a mixture of alkyl acid orthophosphates by reacting phosphorus pentoxide with a mixture of at least two alcohols wherein at least one alcohol is selected from the group consisting of C 1 to C 5 n-alkanols and at least one alcohol is selected from the group consisting of C 6 to C 18 alkanols and C 6 to C 18 alkenols, (b) reacting said mixture of alkyl acid orthophosphates with a basic aluminum compound selected from the group consisting of hydrated alumina and aluminum alkoxides in a ratio of from 2.67 gram atoms of phosphorus per gram atom of aluminum to produce a partial aluminum salt of the alkyl acid orthophosphates, and (c) adding thereto sufficient amount of a second base selected from the group consisting of alkali metal hydroxides, alkali metal oxides, ammonium hydroxide, alkaline earth metal hydroxides, alkaline earth oxides, and alkali metal salts of weak acids to neutralize the remaining acidity.
Claim 7
Dependent Claim 170 words
A pseudo double salt of an alkyl acid orthophosphate prepared by the steps of (a) preparing a mixture of alkyl acid orthophosphates by reacting phosphorus pentoxide with a mixture of at least two alcohols wherein at least one alcohol is selected from the group consisting of C 1 to C 5 n-alkanols and at least one alcohol is selected from the group consisting of C 6 to C 18 alkanols and C 6 to C 18 alkenols, (b) reacting said mixture of alkyl acid orthophosphates with a basic aluminum compound selected from the group consisting of hydrated alumina and aluminum alkoxides in a ratio of from 2.67 gram atoms of phosphorus per gram atom of aluminum to produce a partial aluminum salt of the alkyl acid orthophosphates, and (c) adding thereto sufficient amount of a second base selected from the group consisting of alkali metal hydroxides, alkali metal oxides, ammonium hydroxide, alkaline earth metal hydroxides, alkaline earth oxides, and alkali metal salts of weak acids to neutralize the remaining acidity.
Claim 8
Dependent Claim 42 words
The pseudo double salt of claim 4 wherein the neutralization Step C is carried out in the presence of from 9 parts by weight to 4,000 parts by weight of a liquid hydrocarbon per 1 part by weight of partial aluminum salt.

References Cited (Backward Citations)

US4038207A Cited
US4007128A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-07-31 1982-01-30 1982-08-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-07-31 1986-01-30 1986-08-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-07-31 1990-01-30 1990-08-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag