Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
175 words
A method for the production of colorless polyester amides from monomer starting materials selected from the group consisting of dicarboxylic acids, esters of dicarboxylic acids, primary diamines, polyhydric alcohols and aminocarboxylic acids; esters of dicarboxylic acids, primary diamines and aminocarboxylic acids; dicarboxylic acids, esters of dicarboxylic acids, primary diamines and lactams; esters of dicarboxylic acids, primary diamines and lactams; dicarboxylic acids, esters of dicarboxylic acids, primary diamines and aminocarboxylic acids; or esters of dicarboxylic acids, primary diamines, polyhydric alcohols and aminocarboxylic acids comprising: (a) condensing said starting materials in a first condensing stage in the presence of about 3 to 20 percent by weight of added water based on the total weight of polyamide forming starting materials under a pressure of about 14 to 25 bar and at a temperature of about 220°-300° C: (b) removing said water from said first condensing stage; and (c) in a second condensing stage completely condensing said starting materials at a reduced pressure of about 0.91 to 100 mbar and at a temperature of about 230° to 300° C.
Claim 2
Independent Claim
175 words
A method for the production of colorless polyester amides from monomer starting materials selected from the group consisting of dicarboxylic acids, esters of dicarboxylic acids, primary diamines, polyhydric alcohols and aminocarboxylic acids; esters of dicarboxylic acids, primary diamines and aminocarboxylic acids; dicarboxylic acids, esters of dicarboxylic acids, primary diamines and lactams; esters of dicarboxylic acids, primary diamines and lactams; dicarboxylic acids, esters of dicarboxylic acids, primary diamines and aminocarboxylic acids; or esters of dicarboxylic acids, primary diamines, polyhydric alcohols and aminocarboxylic acids comprising: (a) condensing said starting materials in a first condensing stage in the presence of about 3 to 20 percent by weight of added water based on the total weight of polyamide forming starting materials under a pressure of about 14 to 25 bar and at a temperature of about 220°-300° C: (b) removing said water from said first condensing stage; and (c) in a second condensing stage completely condensing said starting materials at a reduced pressure of about 0.91 to 100 mbar and at a temperature of about 230° to 300° C.
Claim 3
Dependent Claim
19 words
The method of claim 1, wherein a temperature of 250°-280° C is employed in the first and second stages.
Claim 4
Dependent Claim
20 words
The method of claim 2, wherein a reduced pressure of 0.1 - 30 mbar is utilized in the second stage.
Claim 5
Dependent Claim
16 words
The method of claim 3, wherein said pressure of said first stage is about 16-20 bar.
Claim 6
Dependent Claim
21 words
The method of claim 1, wherein said first stage is carried out for a period of about 1 to 12 hours.
Claim 7
Dependent Claim
37 words
The method of claim 4, wherein said first stage is carried out for a period of about 6 to 10 hours and said second stage is carried out for a period of about 2 to 8 hours.