Abstract

Abstract A tire sealant composition which possesses the added ability of operating as a tire balancing composition is provided. Such composition comprises a fibrous component of asbestos fibers and a polyvinyl alcohol-containing liquid component. The composition has a viscosity of about 1000 to about 2200 cps at 100° F.

Inventors

  • 👤 Jerry B. Kent
  • 👤 Peter P. Augostini

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 11:29
CPC Classifications
B; B29; B29D; B29D30/00; B29D30/06; B29D30/0681; B29D30/0685; B29C; B29C73/00; B29C73/16; B29C73/163; B29D30/0601; B29D30/0633; B60; B60C; B60C19/00; B60C19/003; C; C08; C08K; C08K7/00; C08K7/02; C08K7/04; C08K7/10; C08K7/12; C09; C09J; C09J129/00; C09J129/02; C09J129/04; B29D2030/0634; B29D2030/0635; B29D2030/0637; B29D2030/0686; B29D2030/0698; B29L; B29L2030/00; C08L; C08L2666/00; C08L2666/54; Y; Y10; Y10T; Y10T152/00; Y10T152/10; Y10T152/10495; Y10T152/10666; Y10T152/10675; Y10T152/10684

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 102 words
A tire sealing and balancing composition having a viscosity of from about 1000 to about 2200 cps at 100° F., said composition comprising from about 2% to about 8% by weight of a fibrous component containing asbestos fibers of from about 0.01 to about 3.0 inches in length and fiberglass fibers of about 0.25 inches to 0.125 inches in length the ratio of asbestos fibers to fiberglass fibers being from about 20:1 to about 100:1 and an aqueous solution of a water soluble polyvinyl alcohol wherein the ratio by weight of polyvinyl alcohol to water is from about 0.5:100 to about 5.0:100.
Claim 2
Dependent Claim 102 words
A tire sealing and balancing composition having a viscosity of from about 1000 to about 2200 cps at 100° F., said composition comprising from about 2% to about 8% by weight of a fibrous component containing asbestos fibers of from about 0.01 to about 3.0 inches in length and fiberglass fibers of about 0.25 inches to 0.125 inches in length the ratio of asbestos fibers to fiberglass fibers being from about 20:1 to about 100:1 and an aqueous solution of a water soluble polyvinyl alcohol wherein the ratio by weight of polyvinyl alcohol to water is from about 0.5:100 to about 5.0:100.
Claim 3
Dependent Claim 50 words
The tire sealing composition of claim 1 further characterized in that the polyvinyl alcohol is from 98.0% to 98.8% hydrolyzed polyvinyl acetate and, in a 4% by weight aqueous solution, has a viscosity of 28-32 cps as measured with a Brookfield viscometer, Model LVF, #1 spindle, 60 rpm, 20° C.
Claim 4
Dependent Claim 48 words
The tire sealing composition of claim 1 further characterized in that the polyvinyl alcohol is from 87.0% to 89.0% hydrolyzed polyvinyl acetate, and a 4% solution of same has a viscosity of 28-32 cps as measured with a Brookfield viscometer, Model LVF, #1 spindle, 60 rpm, 20° C.
Claim 5
Dependent Claim 27 words
The tire sealing component of claim 2 further characterized in that the ratio by weight of polyvinyl alcohol to water is from about 0.5:100 to about 5.0:100.
Claim 6
Dependent Claim 27 words
The tire sealing component of claim 2 further characterized in that the ratio by weight of polyvinyl alcohol to water is from about 0.5:100 to about 1.0:100.
Claim 7
Dependent Claim 18 words
The tire sealing component of claim 5 further characterized in that the liquid component contains an antifreeze additive.
Claim 8
Dependent Claim 35 words
The tire sealing component of claim 6 further characterized in that the antifreeze additive is ethylene or diethylene glycol, the ratio by volume of said additive to water being from about 40:60 to about 60:40.
Claim 9
Dependent Claim 27 words
The tire sealing component of claim 3 further characterized in that the ratio by weight of polyvinyl alcohol to water is from about 0.5:100 to about 5.0:100.
Claim 10
Dependent Claim 25 words
The tire sealing component of claim 2 further characterized in that the ratio by weight of polyvinyl alcohol is from about 0.5:100 to about 1.0:100.
Claim 11
Dependent Claim 18 words
The tire sealing component of claim 9 further characterized in that the liquid component contains an antifreeze additive.
Claim 12
Dependent Claim 35 words
The tire sealing component of claim 10 further characterized in that the antifreeze additive is ethylene or diethylene glycol, the ratio by volume of said additive to water being from about 40:60 to about 60:40.
Claim 13
Dependent Claim 26 words
The tire sealing component of claim 1 further characterized in that it also contains potassium dichromate, sodium tetraborate pentahydrate or mixtures thereof as a rust preventative.
Claim 14
Dependent Claim 25 words
The tire sealing component of claim 1 further characterized in that the liquid component contains from 0.05 to about 1.5 percent, as an anti-foaming agent.

References Cited (Backward Citations)

US2622044A Cited
US2693438A Cited
US3034998A Cited
US3249568A Cited
US3282874A Cited
US3167522A Cited
US3352696A Cited
US3860539A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-07-17 1982-01-16 1982-07-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-07-17 1986-01-16 1986-07-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-07-17 1990-01-16 1990-07-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag