Patent US2220593A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4092283A Expired / Lapsed US ⏱️ 0.0 years remaining

Gravure ink binder for paper and process for preparing the same

Assignee: Arakawa Rinsan Kagaku Kogyo KK
•
Filing: 1975-06-23
•
Granted: 1978-05-30
•
Expires: 1995-06-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Gravure ink binder for paper comprising the reaction product of (a) cyclopentadiene, (b) alpha , beta -ethylenically unsaturated dicarboxylic acid or anhydride thereof, (c) resin acid and (d) metal compound, and having a softening point of 130 DEG C. to 240 DEG C. and acid value of not more than 100. The binder provides gravure inks for paper excellent in drying property and gloss.

Inventors

  • 👤 Toshio Oishi
  • 👤 Takashi Kitano
  • 👤 Hiroshi Sasaki
  • 👤 Tetuo Yamashita

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 17:16
CPC Classifications
C; C09; C09D; C09D11/00; C09D11/02; C09D11/10

Claims Analysis

Total Claims: 22
Claim 1
Independent Claim 139 words
A gravure ink binder for paper comprising the reaction product of (a) at least one member selected from the group consisting of cyclopentadiene, dicyclopentadiene and substitution products thereof where one or two hydrogens are replaced by methyl group, (b) 1 to 30 parts of at least one member selected from the group consisting of α,β-ethylenically unsaturated dicarboxylic acids and α,β-ethylenically unsaturated dicarboxylic acid anhydrides, (c) 5 to 100 parts of a resin acid, and (d) 0.05 to 11 parts of at least one metal compound selected from the group consisting of bivalent metal oxides, bivalent metal hydroxides and bivalent metal acetates, said reaction product having a softening point of 150° to 220° C. and an acid value of not more than 100, and said parts of (b), (c) and (d) being parts by weight per 100 parts of (a).
Claim 2
Dependent Claim 139 words
A gravure ink binder for paper comprising the reaction product of (a) at least one member selected from the group consisting of cyclopentadiene, dicyclopentadiene and substitution products thereof where one or two hydrogens are replaced by methyl group, (b) 1 to 30 parts of at least one member selected from the group consisting of α,β-ethylenically unsaturated dicarboxylic acids and α,β-ethylenically unsaturated dicarboxylic acid anhydrides, (c) 5 to 100 parts of a resin acid, and (d) 0.05 to 11 parts of at least one metal compound selected from the group consisting of bivalent metal oxides, bivalent metal hydroxides and bivalent metal acetates, said reaction product having a softening point of 150° to 220° C. and an acid value of not more than 100, and said parts of (b), (c) and (d) being parts by weight per 100 parts of (a).
Claim 3
Dependent Claim 18 words
The binder of claim 1, wherein said reaction product has an acid value of not more than 75.
Claim 4
Dependent Claim 12 words
The binder of claim 1, wherein said (a) is cyclopentadiene and/or dicyclopentadiene.
Claim 5
Dependent Claim 26 words
The binder of claim 1, wherein said (b) is at least one member selected from the group consisting of maleic acid, fumaric acid and maleic anhydride.
Claim 6
Dependent Claim 50 words
The binder of claim 1, wherein said resin acid is at least one member selected from the group consisting of rosin, rosin modified with maleic acid, rosin modified with fumaric acid, partial esterification product of rosin modified with maleic acid and partial esterification product of rosin modified with fumaric acid.
Claim 7
Dependent Claim 21 words
The binder of claim 1, wherein said resin acid is partial esterification product of pentaerythritol and rosin modified with maleic acid.
Claim 8
Dependent Claim 22 words
The binder of claim 1, wherein said resin acid is partial esterification product of diethylene glycol and rosin modified with fumaric acid.
Claim 9
Dependent Claim 21 words
The binder of claim 1, wherein said resin acid is partial esterification product of glycerin and rosin modified with fumaric acid.
Claim 10
Dependent Claim 29 words
The binder of claim 1, wherein said metal compound is at least one member selected from the group consisting of zinc oxide, calcium hydroxide, magnesium hydroxide and calcium acetate.
Claim 11
Dependent Claim 22 words
The binder of claim 1, wherein the amount of said (b) falls within the range of 3 to 28 parts by weight.
Claim 12
Dependent Claim 23 words
The binder of claim 1, wherein the amount of said resin acid falls within the range of 10 to 85 parts by weight.
Claim 13
Dependent Claim 23 words
The binder of claim 1, wherein the amount of said metal compound falls within the range of 0.1 to 10.5 parts by weight.
Claim 14
Dependent Claim 31 words
The binder of claim 1, in which said reaction product is further reacted with 0 to 30 parts by weight of an alcohol per 100 parts by weight of (a) employed.
Claim 15
Dependent Claim 25 words
The binder of claim 13, wherein said alcohol is a member selected from the group consisting of diethylene glycol, diethylene glycol monoethyl ether and pentaerythritol.
Claim 16
Dependent Claim 157 words
A process for preparing gravure ink binder for paper which comprises the steps of carrying out the heat-reaction between (a) at least one member selected from the group consisting of cyclopentadiene, dicyclopentadiene and substitution products thereof where one or two hydrogens are replaced by methyl group, (b) 1 to 30 parts of at least one member selected from the group consisting of α,β-ethylenically unsaturated dicarboxylic acids and α,β-ethylenically unsaturated dicarboxylic acid anhydrides, (c) 5 to 100 parts of a resin acid, and (d) 0.05 to 11 parts of at least one metal compound selected from the group consisting of bivalent metal oxides, bivalent metal hydroxides and bivalent metal acetates at a temperature of 190° to 300° C., and recovering the resulting reaction product having a softening point of 150° to 220° C. and an acid value of not more than 100, said parts of (b), (c) and (d) being parts by weight per 100 parts of (a).
Claim 17
Dependent Claim 157 words
A process for preparing gravure ink binder for paper which comprises the steps of carrying out the heat-reaction between (a) at least one member selected from the group consisting of cyclopentadiene, dicyclopentadiene and substitution products thereof where one or two hydrogens are replaced by methyl group, (b) 1 to 30 parts of at least one member selected from the group consisting of α,β-ethylenically unsaturated dicarboxylic acids and α,β-ethylenically unsaturated dicarboxylic acid anhydrides, (c) 5 to 100 parts of a resin acid, and (d) 0.05 to 11 parts of at least one metal compound selected from the group consisting of bivalent metal oxides, bivalent metal hydroxides and bivalent metal acetates at a temperature of 190° to 300° C., and recovering the resulting reaction product having a softening point of 150° to 220° C. and an acid value of not more than 100, said parts of (b), (c) and (d) being parts by weight per 100 parts of (a).
Claim 18
Dependent Claim 19 words
The process of claim 15, wherein said heat-reaction is carried out at a temperature of 200° to 270° C.
Claim 19
Dependent Claim 99 words
The process of claim 15, in which said resulting reaction product of (a), (b), (c) and (d) is subjected to the reaction with at least one alcohol selected from the group consisting of 2-ethylhexyl alcohol, ethylene glycol monomethyl ether, ethylene glycol monoethyl ether, ethylene glycol monobutyl ether, diethylene glycol monomethyl ether, diethylene glcyol monoethyl ether, diethylene glycol monobutyl ether, ethylene glycol, diethylene glycol, triethylene glycol, neopentyl alcohol, glycerin and pentaerythritol at a temperature of 180° to 270° C., the amount of said alcohol being selected from 0 to 30 parts by weight per 100 parts by weight of (a).
Claim 20
Dependent Claim 229 words
A process for preparing gravure ink binder for paper which comprises the steps of carrying out the heat-reaction between (a) at least one member selected from the group consisting of cyclopentadiene, dicyclopentadiene and substitution products thereof where one or two hydrogens are replaced by methyl group, (b) 1 to 30 parts of at least one member selected from the group consisting of α,β-ethylenically unsaturated dicarboxylic acids and α,β-ethylenically unsaturated dicarboxylic acid anhydrides, and (c) 5 to 100 parts of a resin acid at a temperature of 190° to 300° C., subjecting the resulting reaction product of (a), (b) and (c) to reaction with (d) 0.05 to 11 parts of at least one metal compound selected from the group consisting of bivalent metal oxides, bivalent metal hydroxides and bivalent metal acetates, in a solvent selected from the group consisting of benzene, toluene, xylene and mineral spirit in the presence of a catalytically effective amount of an organic acid catalyst selected from the group consisting of formic acid, acetic acid, latic acid, tartaric acid and citric acid at a temperature of 50° to 200° C., and recovering the resulting reaction product of (a), (b), (c) and (d) having a softening point of 150° to 220° C. and an acid value of not more than 100, said parts of (b), (c) and (d) being parts by weight per 100 parts of (a).
Claim 21
Dependent Claim 229 words
A process for preparing gravure ink binder for paper which comprises the steps of carrying out the heat-reaction between (a) at least one member selected from the group consisting of cyclopentadiene, dicyclopentadiene and substitution products thereof where one or two hydrogens are replaced by methyl group, (b) 1 to 30 parts of at least one member selected from the group consisting of α,β-ethylenically unsaturated dicarboxylic acids and α,β-ethylenically unsaturated dicarboxylic acid anhydrides, and (c) 5 to 100 parts of a resin acid at a temperature of 190° to 300° C., subjecting the resulting reaction product of (a), (b) and (c) to reaction with (d) 0.05 to 11 parts of at least one metal compound selected from the group consisting of bivalent metal oxides, bivalent metal hydroxides and bivalent metal acetates, in a solvent selected from the group consisting of benzene, toluene, xylene and mineral spirit in the presence of a catalytically effective amount of an organic acid catalyst selected from the group consisting of formic acid, acetic acid, latic acid, tartaric acid and citric acid at a temperature of 50° to 200° C., and recovering the resulting reaction product of (a), (b), (c) and (d) having a softening point of 150° to 220° C. and an acid value of not more than 100, said parts of (b), (c) and (d) being parts by weight per 100 parts of (a).
Claim 22
Dependent Claim 24 words
A gravure ink for paper comprising a varnish containing the binder of claim 1 dissolved in an aromatic hydrocarbon solvent and pigment dispersed therein.

References Cited (Backward Citations)

US3468829A Cited
US3475362A Cited
US3880788A Cited
US3935145A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-05-29 1981-11-28 1982-05-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-05-29 1985-11-28 1986-05-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-05-29 1989-11-28 1990-05-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag