Abstract

Abstract A method for increasing the tolerance of hydrocarbon polymer sulfonate surfactant materials to divalent ions especially calcium when such materials are injected into subterranean formations containing high divalent cation contents which comprises contacting the hydrocarbon polymer sulfonate surfactant with an oxidizing agent at oxidizing conditions. The specific hydrocarbon polymer sulfonate surfactants disclosed are those produced from lower aliphatic olefins such as isobutylene, butene-1, butene-2 or propylene or other similar olefinic materials which have been polymerized to average equivalent molecular weights of from about 350 to 675 or higher. The preferred oxidizing agent is hydrogen peroxide.

Inventors

  • 👤 Edward F. McCarthy

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 13:43
CPC Classifications
C; C09; C09K; C09K8/00; C09K8/58; C09K8/584; Y; Y10; Y10S; Y10S507/00; Y10S507/935; Y10S507/936

Claims Analysis

Total Claims: 18
Claim 1
Independent Claim 173 words
In a method of flooding an oil-bearing subterranean formation with a solubilized oil-water mixture which is injected into the formation and displaced towards at least one production means wherein the mixture comprises: from about 2 to about 50 weight percent of a surfactant comprising an aliphatic hydrocarbon polymer sulfonate having an average equivalent molecular weight of from about 250 to about 675 and containing a sulfite salt; a cosurfactant selected from the group consisting of water-soluble alcohol, oil-soluble alcohol having no more than 10 carbon atoms and a 2 to 12 mole ethylene oxide adduct of an alcohol having from 4 to 10 carbon atoms or mixtures thereof, the weight ratio of cosurfactant to sulfonate ranging from about 1:5 to about 10:1; and from about 98 to about 50 weight percent of an aqueous sodium chloride containing brine solution; wherein the improvement increases the tolerance of said surfactant to calcium cation containing brines and comprises contacting said sulfonate with hydrogen peroxide at oxidation conditions to effect oxidation of the sulfite in the surfactant.
Claim 2
Dependent Claim 173 words
In a method of flooding an oil-bearing subterranean formation with a solubilized oil-water mixture which is injected into the formation and displaced towards at least one production means wherein the mixture comprises: from about 2 to about 50 weight percent of a surfactant comprising an aliphatic hydrocarbon polymer sulfonate having an average equivalent molecular weight of from about 250 to about 675 and containing a sulfite salt; a cosurfactant selected from the group consisting of water-soluble alcohol, oil-soluble alcohol having no more than 10 carbon atoms and a 2 to 12 mole ethylene oxide adduct of an alcohol having from 4 to 10 carbon atoms or mixtures thereof, the weight ratio of cosurfactant to sulfonate ranging from about 1:5 to about 10:1; and from about 98 to about 50 weight percent of an aqueous sodium chloride containing brine solution; wherein the improvement increases the tolerance of said surfactant to calcium cation containing brines and comprises contacting said sulfonate with hydrogen peroxide at oxidation conditions to effect oxidation of the sulfite in the surfactant.
Claim 3
Dependent Claim 27 words
The method of claim 1 further characterized in that said polymer sulfonate is selected from the group consisting of alkali metal or ammonium or mixtures thereof sulfonates.
Claim 4
Dependent Claim 53 words
The method of claim 2 further characterized in that the polymer sulfonate has an average equivalent molecular wieght of from about 400 to about 450 and the hydrocarbon portion of the sulfonate is derived from the polymerization of monomers selected from the group consisting of isobutylene, butene-1, butene-2, or propylene or mixtures thereof.
Claim 5
Dependent Claim 28 words
The method of claim 2 further characterized in that the hydrocarbon portion of the sulfonate is derived from the polymerization of a mixture comprising isobutylene, butene-1, and butene-2.
Claim 6
Dependent Claim 38 words
The method of claim 1 further characterized in that said polymer sulfonate has an average equivalent molecular weight of from about 350-575 with its hydrocarbon portion derived from the polymerization of a mixture comprising isobutylene, butene-1 and butene-2.
Claim 7
Dependent Claim 26 words
The method of claim 5 further characterized in that said sulfonate is selected from the group consisting of alkali, metal or ammonium sulfonates or mixtures thereof.
Claim 8
Dependent Claim 49 words
The method of claim 6 further characterized in that said surfactant comprises from about 8 to about 13 weight percent hydrocarbon oil, from about 47 to about 52 weight percent sulfonate, from about 23 to about 29 weight percent water and less than about 16 weight percent inorganic salts.
Claim 9
Dependent Claim 27 words
The method of claim 7 further characterized in that said surfactant constitutes from about 6 weight percent to about 12 weight percent of the solubilized oil-water mixture.
Claim 10
Dependent Claim 28 words
The method of claim 1 further characterized in that said sulfite comprises a material selected from the group consisting of sodium sulfite and ammonium sulfite or mixtures thereof.
Claim 11
Dependent Claim 27 words
The method of claim 9 further characterized in that said polymer sulfonate is selected from the group consisting of alkali metal or ammonium or mixtures thereof sulfonates.
Claim 12
Dependent Claim 53 words
The method of claim 10 further characterized in that the polymer sulfonate has an average equivalent molecular weight of from about 400 to about 450 and the hydrocarbon portion of the sulfonate is derived from the polymerization of monomers selected from the group consisting of isobutylene, butene-1, butene-2, or propylene or mixtures thereof.
Claim 13
Dependent Claim 28 words
The method of claim 10 further characterized in that the hydrocarbon portion of the sulfonate is derived from the polymerization of a mixture comprising isobutylene, butene-1, and butene-2.
Claim 14
Dependent Claim 37 words
The method of claim 9 further characterized in that said polymer sulfonate has an average molecular weight of from about 350-575 with its hydrocarbon portion derived from the polymerization of a mixture comprising isobutylene, butene-1 and butene-2.
Claim 15
Dependent Claim 49 words
The method of claim 13 further characterized in that said surfactant comprises from about 8 to about 13 weight percent hydrocarbon oil, from about 47 to about 52 weight percent sulfonate, from about 23 to about 29 weight percent water and less than about 16 weight percent inorganic salts.
Claim 16
Dependent Claim 27 words
The method of claim 1 further characterized in that said surfactant constitutes from about 6 weight percent to about 12 weight percent of the solubilized oil-water mixture.
Claim 17
Dependent Claim 38 words
The method of claim 1 further characterized in that said surfactant comprises the product of neutralization of polybutene sulfonic acid and a base selected from the group consisting of ammonia, ammonium hydroxide and sodium hydroxide or mixtures thereof.
Claim 18
Dependent Claim 23 words
The method of claim 16 further characterized in that said product of neutralization contains water, unsulfonated polybutene and inorganic sulfate and sulfite salts.

References Cited (Backward Citations)

US2653970A Cited
US3424693A Cited
US3428654A Cited
US3535339A Cited
US3644499A Cited
US3714062A Cited
US3954849A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-05-15 1981-11-14 1982-05-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-05-15 1985-11-14 1986-05-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-05-15 1989-11-14 1990-05-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag