Patent US4932447A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4089710A Expired / Lapsed US ⏱️ 0.0 years remaining

Phosphating method with control in response to conductivity change

Assignee: Imperial Chemical Industries Ltd
•
Filing: 1976-04-19
•
Granted: 1978-05-16
•
Expires: 1996-04-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of controlling a continuous process of phosphating metal surfaces in which an acidic zinc phosphate solution is brought to the steady state and there maintained in response to conductivity change, as phosphating proceeds, by addition of replenishments (a) acidic zinc phosphate and (b) alkali metal ion in a definite ratio of addition rates.

Inventors

  • 👤 Brian Alfred Cooke

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 10:19
CPC Classifications
C; C23; C23C; C23C22/00; C23C22/73; C23C22/77

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 196 words
In a method of applying a zinc phosphate coating to a continuous metal surface or to a series of metal surfaces wherein (1) a metal surface is treated with an acidic phosphating solution which comprises zinc, phosphate and alkali metal ions, (2) the acidic phosphating solution is replenished as coating proceeds by additions of an acidic material (a) comprising zinc phosphate ions, and of an alkaline material (b) comprising alkali metal ions, and (3) the composition of the acidic phosphating solution when in the steady state is such that a consistent and satisfactory coating is produced on the metal surface, and can be maintained substantially constant, as coating proceeds, by additions of materials (a) and (b) in a definite ratio of addition rates, the improvement which consists in commencing to treat a metal surface or metal surfaces in a phosphating solution which is already in said steady state, and thereafter making additions to the acidic phophating solution of materials (a) and (b) so as to maintain constant its electrolytic conductivity at a given temperature, the addition rates of (a) and (b) made in response to any change in conductivity being in the same said definite ratio.
Claim 2
Dependent Claim 196 words
In a method of applying a zinc phosphate coating to a continuous metal surface or to a series of metal surfaces wherein (1) a metal surface is treated with an acidic phosphating solution which comprises zinc, phosphate and alkali metal ions, (2) the acidic phosphating solution is replenished as coating proceeds by additions of an acidic material (a) comprising zinc phosphate ions, and of an alkaline material (b) comprising alkali metal ions, and (3) the composition of the acidic phosphating solution when in the steady state is such that a consistent and satisfactory coating is produced on the metal surface, and can be maintained substantially constant, as coating proceeds, by additions of materials (a) and (b) in a definite ratio of addition rates, the improvement which consists in commencing to treat a metal surface or metal surfaces in a phosphating solution which is already in said steady state, and thereafter making additions to the acidic phophating solution of materials (a) and (b) so as to maintain constant its electrolytic conductivity at a given temperature, the addition rates of (a) and (b) made in response to any change in conductivity being in the same said definite ratio.
Claim 3
Dependent Claim 42 words
A method according to claim 1 wherein the desired optimum composition of the acidic phosphating solution when in the steady state is determined by the analysis of a working acidic phosphating solution which provides a desired phosphate coating by a conventional procedure.
Claim 4
Dependent Claim 23 words
A method according to claim 1 wherein the acidic solution is replenished as coating proceeds by materials additional to materials (a) and (b).
Claim 5
Dependent Claim 16 words
A method according to claim 1 wherein the acidic phosphating solution also comprises a depolarising oxidant.
Claim 6
Dependent Claim 21 words
A method according to claim 1 wherein the acidic phosphating solution comprises zinc, phosphate, alkali metal, chlorate and optionally nitrate ions.
Claim 7
Dependent Claim 14 words
A method according to claim 1 wherein the metal surface comprises a ferrous metal.

References Cited (Backward Citations)

GB606382A Cited
US3338755A Cited
US3312189A Cited
US3369928A Cited
US3525651A Cited
US3607453A Cited
US3758349A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-05-15 1981-11-14 1982-05-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-05-15 1985-11-14 1986-05-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-05-15 1989-11-14 1990-05-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag