Improved method of beneficiating clay by removal of titanium and iron impurities
Assignee: JM Huber Corp
•
Filing: 1977-01-21
•
Granted: 1978-05-09
•
Expires: 1997-01-21
Abstract
Abstract A method of beneficiating kaolin clay by the addition of non-dispersing neutral salts to assist in the removal of discolored impurities, such as titanium and iron bearing minerals from a clay slurry. This process is capable of producing clays having a brightness in the 90- 95 range.
Inventors
- 👤 Robert N. Maynard
- 👤 Bobby R. Skipper
- 👤 Nathan Millman
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-27 21:39
CPC Classifications
C; C01; C01B; C01B33/00; C01B33/20; C01B33/36; C01B33/38; C01B33/42; C01B33/26; C01B33/40; C01B33/46; C04; C04B; C04B33/00; C04B33/02; C04B33/04
Claims Analysis
Total Claims: 3
Claim 1
Independent Claim
190 words
An improved method for beneficiating an East Georgio kaolin clay, said method comprising the steps of: 1. treating an aqueous suspension of the kaolin clay be adding to the aqueous kaolin clay suspension a peptizing agent selected from the group consisting of polyphosphates, carbonates, silicates, alkalies, basic salts, and combinations thereof, in an amount in excess of that required to obtain minimum Brookfield viscosity of the kaolin clay-water-dispersant system as defined by measurement at 60% solids with a Brookfield viscometer at 10 r.p.m. using a No. 1 spindle; 2. further treating the aqueous suspension of the East Georgia kaolin clay by adding to the aqueous clay suspension from 4 pounds to 15 pounds per ton of kaolin clay of a non-dispersing neutral salt selected from the group consisting of sodium chloride, potassium chloride, sodium nitrate, sodium sulfate, and combinations thereof; 3. separating the contaminants from the clay by sedimentation within the aqueous kaolin clay slurry at a kaolin clay solids content in excess of 20 percent by weight and recovering a clay product having a brightness in the range of from 91 to 95 after bleaching of said clay product.
Claim 2
Dependent Claim
190 words
An improved method for beneficiating an East Georgio kaolin clay, said method comprising the steps of: 1. treating an aqueous suspension of the kaolin clay be adding to the aqueous kaolin clay suspension a peptizing agent selected from the group consisting of polyphosphates, carbonates, silicates, alkalies, basic salts, and combinations thereof, in an amount in excess of that required to obtain minimum Brookfield viscosity of the kaolin clay-water-dispersant system as defined by measurement at 60% solids with a Brookfield viscometer at 10 r.p.m. using a No. 1 spindle; 2. further treating the aqueous suspension of the East Georgia kaolin clay by adding to the aqueous clay suspension from 4 pounds to 15 pounds per ton of kaolin clay of a non-dispersing neutral salt selected from the group consisting of sodium chloride, potassium chloride, sodium nitrate, sodium sulfate, and combinations thereof; 3. separating the contaminants from the clay by sedimentation within the aqueous kaolin clay slurry at a kaolin clay solids content in excess of 20 percent by weight and recovering a clay product having a brightness in the range of from 91 to 95 after bleaching of said clay product.
Claim 3
Dependent Claim
13 words
The method of claim 1 wherein the neutral non-dispersing salt is sodium chloride.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-05-08 | 1981-11-07 | 1982-05-09 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-05-08 | 1985-11-07 | 1986-05-09 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-05-08 | 1989-11-07 | 1990-05-09 | $7700.00 | Window Closed / Lapsed |