Abstract

Abstract A high efficiency pyrotechnically activated lithium-chlorine primary cell ving a high voltage output, high energy density, and a high rate of discharge comprises a porous graphite gas diffuser, a fused alkali metal salt electrolyte, a lithium anode in contact with the electrolyte, a lithium vapor barrier, and a cartridge containing a pyrotechnic material disposed within the anode, all of the components being stacked inside a container which serves as the cell case. The lithium vapor barrier comprises a porous metal ring impregnated with lithium-chloride and is designed to prevent vaporized lithium from penetrating the barrier, contacting the chlorine cover gas and exothermically reacting.

Inventors

  • 👤 Frederic M. Bowers
  • 👤 Judith H. Ambrus
  • 👤 Michael E. DeGraba

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 10:30
CPC Classifications
H; H01; H01M; H01M12/00; H01M12/04; H01M4/00; H01M4/02; H01M4/64; H01M4/66; H01M4/661; Y; Y02; Y02E; Y02E60/00; Y02E60/10

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 242 words
A pyrotechnically activated, high efficiency lithium-chlorine primary cell comprising: a cell case; a porous graphite wafer positioned within the cell case to provide a gas receiving chamber; a fused salt electrolyte contiguous to the porous graphite wafer; an anode comprising a metal shield which contains a lithium impregnated metal matrix, the anode being in contact with the electrolyte and insulated from the cell case by a refractory electrical insulator, wherein the metal of the shield and the metal of the matrix are selected from the group consisting of nickel and nickel alloys; a metal cartridge containing a pyrotechnic material, the cartridge being disposed within the anode, wherein the metal is selected from the group consisting of nickel and nickel alloys; a vapor barrier comprising a porous metal ring impregnated with lithium-chloride said barrier being disposed above said anode and contiguous with both said metal shield and said metal cartridge, wherein the metal of said ring is selected from the group consisting of nickel and nickel alloys; a source of Cl 2 gas; means to introduce the Cl 2 gas into the gas receiving chamber; and means to activate the pyrotechnic material; wherein, chlorine gas is introduced into the gas receiving chamber and passed through the porous graphite wafer as the pyrotechnic material is activated thereby providing sufficient heat to melt the electrolyte, and to heat the entire cell to its operating temperature, thus generating the flow of ions between the cell electrodes.
Claim 2
Dependent Claim 242 words
A pyrotechnically activated, high efficiency lithium-chlorine primary cell comprising: a cell case; a porous graphite wafer positioned within the cell case to provide a gas receiving chamber; a fused salt electrolyte contiguous to the porous graphite wafer; an anode comprising a metal shield which contains a lithium impregnated metal matrix, the anode being in contact with the electrolyte and insulated from the cell case by a refractory electrical insulator, wherein the metal of the shield and the metal of the matrix are selected from the group consisting of nickel and nickel alloys; a metal cartridge containing a pyrotechnic material, the cartridge being disposed within the anode, wherein the metal is selected from the group consisting of nickel and nickel alloys; a vapor barrier comprising a porous metal ring impregnated with lithium-chloride said barrier being disposed above said anode and contiguous with both said metal shield and said metal cartridge, wherein the metal of said ring is selected from the group consisting of nickel and nickel alloys; a source of Cl 2 gas; means to introduce the Cl 2 gas into the gas receiving chamber; and means to activate the pyrotechnic material; wherein, chlorine gas is introduced into the gas receiving chamber and passed through the porous graphite wafer as the pyrotechnic material is activated thereby providing sufficient heat to melt the electrolyte, and to heat the entire cell to its operating temperature, thus generating the flow of ions between the cell electrodes.
Claim 3
Dependent Claim 16 words
The cell of claim 1 wherein said porous metal ring is a compressed, sintered fibermetal mat.
Claim 4
Dependent Claim 16 words
The cell as claimed in claim 2 wherein said vapor barrier is about 1.5 mm thick.
Claim 5
Dependent Claim 17 words
A battery comprising a plurality of the pyrotechnically activated lithium-chlorine primary cells as claimed in claim 1.
Claim 6
Dependent Claim 260 words
In combination with a pyrotechnically activated lithium-chlorine primary cell of the type which includes: a cell case which comprises a cylindrical, dense graphite cell case, the walls of said cell case being line with a BN insulator; a porous graphite wafer positioned within the cell case to provide a gas receiving chamber; a LiCl--KCl eutectic fused salt electrolyte contiguous to the porous graphite wafer; an anode which comprises a nickel 200 cylinder containing a lithium impregnated nickel 200 compressed, sintered fibermetal mat, the anode being in intimate contact with the electrolyte and insulated from the cell case by the BN insulator; cylindrical graphite-line nickel 200 cartridge containing a mixture of aluminum, nickel and ferric oxide, the cartridge being concentrically disposed within and in intimate contact with the anode; a source of Cl 2 gas; an inlet to introduce the Cl 2 gas into the gas receiving chamber; and an electrical heating element to activate the pyrotechnic material; wherein, chlorine gas is introduced into the gas receiving chamber and passed through the porous graphite wafer as the pyrotechnic material is activated thereby providing sufficient heat to melt the electrolyte, and to heat the entire cell to its operating temperature, thus generating the flow of ions between the cell electrodes, and wherein the improvement comprises: a vapor barrier comprising a porous metal ring impregnated with lithium-chloride said barrier being disposed above said anode and contiguous with both said metal shield and said metal cartridge, and wherein the metal of said ring is selected from the group consisting of nickel and nickel alloys.
Claim 7
Dependent Claim 260 words
In combination with a pyrotechnically activated lithium-chlorine primary cell of the type which includes: a cell case which comprises a cylindrical, dense graphite cell case, the walls of said cell case being line with a BN insulator; a porous graphite wafer positioned within the cell case to provide a gas receiving chamber; a LiCl--KCl eutectic fused salt electrolyte contiguous to the porous graphite wafer; an anode which comprises a nickel 200 cylinder containing a lithium impregnated nickel 200 compressed, sintered fibermetal mat, the anode being in intimate contact with the electrolyte and insulated from the cell case by the BN insulator; cylindrical graphite-line nickel 200 cartridge containing a mixture of aluminum, nickel and ferric oxide, the cartridge being concentrically disposed within and in intimate contact with the anode; a source of Cl 2 gas; an inlet to introduce the Cl 2 gas into the gas receiving chamber; and an electrical heating element to activate the pyrotechnic material; wherein, chlorine gas is introduced into the gas receiving chamber and passed through the porous graphite wafer as the pyrotechnic material is activated thereby providing sufficient heat to melt the electrolyte, and to heat the entire cell to its operating temperature, thus generating the flow of ions between the cell electrodes, and wherein the improvement comprises: a vapor barrier comprising a porous metal ring impregnated with lithium-chloride said barrier being disposed above said anode and contiguous with both said metal shield and said metal cartridge, and wherein the metal of said ring is selected from the group consisting of nickel and nickel alloys.
Claim 8
Dependent Claim 16 words
The cell of claim 5 wherein said porous metal ring is a compressed, sintered, fibermetal mat.
Claim 9
Dependent Claim 14 words
The cell of claim 6 wherein said vapor barrier is about 1.5 mm thick.

References Cited (Backward Citations)

US3909297A Cited
US3972730A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-05-01 1981-10-31 1982-05-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-05-01 1985-10-31 1986-05-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-05-01 1989-10-31 1990-05-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag