Abstract

Abstract There are disclosed furfuryl alcohol copolymers of a polyester prepolymer of maleic acid or anhydride and a polyhydric alcohol which incorporate tungsten and/or molybdenum metal atoms. The metal atoms are incorporated into the copolymers by reacting the polyester prepolymer with a reaction product of tungsten or molybdenum and pyrrolidine.

Inventors

  • 👤 Robert C. Shaffer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 15:19
CPC Classifications
C; C08; C08G; C08G63/00; C08G63/68; C08K; C08K3/00; C08K3/02; C08K3/04; C08K3/08

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 58 words
A copolymer of furfuryl alcohol and a polyester prepolymer which is a condensation product of a slight stoichiometric excess of maleic acid or anhydride and a polyhydric alcohol, said copolymer containing tungsten and/or molybdenum metal atoms, said polyester prepolymer having been reacted with a complex which is a reaction product of tungsten carbonyl and/or molybdenum carbonyl with pyrrolidine.
Claim 2
Dependent Claim 58 words
A copolymer of furfuryl alcohol and a polyester prepolymer which is a condensation product of a slight stoichiometric excess of maleic acid or anhydride and a polyhydric alcohol, said copolymer containing tungsten and/or molybdenum metal atoms, said polyester prepolymer having been reacted with a complex which is a reaction product of tungsten carbonyl and/or molybdenum carbonyl with pyrrolidine.
Claim 3
Dependent Claim 29 words
A copolymer as defined in claim 1 wherein from about 30 to 150 parts by weight of said reaction product is reacted with 100 parts by weight of polyester.
Claim 4
Dependent Claim 38 words
A copolymer as defined in claim 1 wherein said metal is present in said copolymer in such a manner as to remain in the charred resin product without volitilizing and to show no evidence of metal particle agglomeration.
Claim 5
Dependent Claim 55 words
A method for producing a copolymer as defined in claim 1 which comprises first reacting a tungsten carbonyl and/or a molybdenum carbonyl with pyrrolidine, subsequently reacting the resultant product with a polyester prepolymer of maleic acid or anhydride and a polyhydric alcohol, and then reacting this product with furfuryl alcohol to form a thermosetting copolymer.

References Cited (Backward Citations)

US3370026A Cited
US3519698A Cited
US3544530A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-05-01 1981-10-31 1982-05-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-05-01 1985-10-31 1986-05-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-05-01 1989-10-31 1990-05-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag