Abstract

Abstract A cyclic electrolytic process for the manufacture of hydrogen from carbonaceous material such as coal, agricultural wastes and garbage to produce commercial hydrogen. An alakli metal sulfate is reduced to an alkali metal sulfide by reaction of the sulfate and carbonaceous fuel at an elevated temperature. The sulfide and impurities derived from the fuel are digested with an aqueous solution to dissolve the sulfide and separate out the impurities. The solution of the alkali sulfide is added to electrolytic cells in which an electric current is utilized to generate hydrogen at the cathode while oxidizing the sulfide substantially to sulfate at the anode. The cell electrolyte temperature is greater than 150° C and less than 350° C. Under these conditions the polarization problem encountered in hydrogen/oxygen cells is substantially avoided. The alkali sulfate is then separated from the electrolyte stream exiting from the electrolytic cells, reduced again by burning with fuel and recycled to the electrolytic cell.

Inventors

  • 👤 Robert Spitzer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 19:19
CPC Classifications
C; C25; C25B; C25B1/00; C25B1/01; C25B1/02

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 124 words
A cyclic electrolytic process of utilizing the energy of dirty carbonaceous fuels to produce commercial hydrogen which comprises: (a) reducing an alkali sulfate to alkali sulfide by reaction of the sulfate and dirty fuel at an elevated temperature, (b) digesting the sulfide and impurities derived from said dirty fuel with aqueous solution, or water, to dissolve the sulfide, and separate out said impurities, (c) adding the solution of said alkali sulfide to an electrolytic cell in which an electric current is utilized to generate hydrogen at the cathode while oxidizing sulfide substantially to sulfate at the anode, (d) separating alkali sulfate from an electrolyte stream exiting from said electrolytic cells, and (e) recycling the alkali sulfate to the reducing procedure of said step (a).
Claim 2
Dependent Claim 124 words
A cyclic electrolytic process of utilizing the energy of dirty carbonaceous fuels to produce commercial hydrogen which comprises: (a) reducing an alkali sulfate to alkali sulfide by reaction of the sulfate and dirty fuel at an elevated temperature, (b) digesting the sulfide and impurities derived from said dirty fuel with aqueous solution, or water, to dissolve the sulfide, and separate out said impurities, (c) adding the solution of said alkali sulfide to an electrolytic cell in which an electric current is utilized to generate hydrogen at the cathode while oxidizing sulfide substantially to sulfate at the anode, (d) separating alkali sulfate from an electrolyte stream exiting from said electrolytic cells, and (e) recycling the alkali sulfate to the reducing procedure of said step (a).
Claim 3
Dependent Claim 21 words
The method of claim 1 in which the cell electrolyte temperature is greater than 150° C and less than 400° C.
Claim 4
Dependent Claim 28 words
The process of claim 2 in which the electrolytic cell is maintained at a pressure above the vapor pressure of the electrolyte and up to about 200 atmospheres.
Claim 5
Dependent Claim 16 words
The method of claim 3 in which said pressure is about between 20 to 200 atmospheres.
Claim 6
Dependent Claim 18 words
The method of claim 3 in which the electrolyte concentration of sulfate is about between 20 to 30%.
Claim 7
Dependent Claim 21 words
The method of claim 1 in which the concentration of alkali sulfate is maintained above its saturation point in the electrolyte.
Claim 8
Dependent Claim 29 words
The method of claim 6 in which the electrolyte is maintained at about a steady concentration of sulfide and sulfate by continuously adding alkali sulfide and removing alkali sulfate.
Claim 9
Dependent Claim 13 words
The method of claim 1 in which the alkali sulfate is sodium sulfate.
Claim 10
Dependent Claim 13 words
The method of claim 1 in which the alkali sulfate is potassium sulfate.
Claim 11
Dependent Claim 12 words
The method of claim 1 in which the dirty fuel is coal.
Claim 12
Dependent Claim 13 words
The method of claim 1 in which the dirty fuel is coal char.
Claim 13
Dependent Claim 15 words
The method of claim 1 in which the dirty fuel is agricultural waste or garbage.
Claim 14
Dependent Claim 25 words
The method of claim 1 in which the electrolyte concentration of sulfide is greater than 5% and less than 35% expressed as sodium sulfide equivalence.
Claim 15
Dependent Claim 40 words
The method of claim 1 in which the alkali sulfate is intimately mixed with said fuel at an elevated pressure to prepared a solid form which is heated by contact with heated gases to effect reduction of said alkali sulfate.

References Cited (Backward Citations)

US3409520A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-03-27 1981-09-26 1982-03-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-03-27 1985-09-26 1986-03-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-03-27 1989-09-26 1990-03-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag