Abstract
Abstract Recovery of ethylene terephthalate polymer from waste material is accomplished by glycolysis of the polyester to form bis-(2-hydroxyethyl)terephthalate for repolymerization. Formation of objectionable diethylene glycol is inhibited when glycolysis is accomplished by heating the polyester in a reaction mixture with bis-(2-hydroxyethyl)terephthalate, ethylene glycol and sodium acetate trihydrate, and water is introduced continuously into the reaction mixture during depolymerization of the polyester.
Inventors
- 👤 Abdul-Ilah Malik
- 👤 Elmer Edwin Most
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-30 21:16
CPC Classifications
C; C07; C07C; C07C67/00; C07C67/03; C08; C08J; C08J11/00; C08J11/04; C08J11/10; C08J11/18; C08J11/22; C08J11/24; C08J2367/00; C08J2367/02; Y; Y02; Y02W; Y02W30/00; Y02W30/50; Y02W30/62
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
102 words
In the process of depolymerizing waste ethylene terephthalate polyester of form bis-(2-hydroxyethyl)terephthalate and low molecular weight polymers thereof by glycolysis of the polyester waste with excess ethylene glycol at elevated temperatures; the improvement for inhibiting formation of glycol ethers which comprises preparing a reaction mixture of 1 part of the waste polyester in 0.88 to 3.6 parts bis-(2-hydroxyethyl)terephthalate, 0.1 to 0.5 part ethylene glycol and 0.000200 to 0.000500 part sodium acetate trihydrate, and heating the reaction mixture to depolymerize the polyester while continuously introducing 0.005 to 0.35 part per hour of water into the reaction mixture to inhibit formation of diethylene glycol.
Claim 2
Dependent Claim
102 words
In the process of depolymerizing waste ethylene terephthalate polyester of form bis-(2-hydroxyethyl)terephthalate and low molecular weight polymers thereof by glycolysis of the polyester waste with excess ethylene glycol at elevated temperatures; the improvement for inhibiting formation of glycol ethers which comprises preparing a reaction mixture of 1 part of the waste polyester in 0.88 to 3.6 parts bis-(2-hydroxyethyl)terephthalate, 0.1 to 0.5 part ethylene glycol and 0.000200 to 0.000500 part sodium acetate trihydrate, and heating the reaction mixture to depolymerize the polyester while continuously introducing 0.005 to 0.35 part per hour of water into the reaction mixture to inhibit formation of diethylene glycol.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-03-06 | 1981-09-05 | 1982-03-07 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-03-06 | 1985-09-05 | 1986-03-07 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-03-06 | 1989-09-05 | 1990-03-07 | $7700.00 | Window Closed / Lapsed |