Abstract A method for making a disposable model for a precision investment casting, which comprises casting a naphthalene or para-dichlorobenzene-containing modeling material into a pattern mold at a temperature of 150 DEG C or less, preferably 80 to 150 DEG C and further preferably at a casting speed of 5 to 0.1 kg/second; the modeling material being optionally admixed with a resin selected from the group consisting of polystyrene, polyethylene, polyvinyl acetate and a mixture thereof as a reinforcing material or comprising a mixture of naphthalene or paradichlorobenzene (preferably 80 to 30% by weight), a wax (preferably 20 to 70% by weight) and the resin as mentioned above (preferably 0.5 to 15% by weight on the basis of the whole weight of the modeling material).
Inventors
👤 Ken Ugata
👤 Yasuji Morita
👤 Yasuharu Mine
👤 Hiroshi Izaki
Bibliographic Details
Application Number—
JurisdictionUS
Data Sourcegoogle_patents
Last Synchronized2026-10-26 15:55
CPC Classifications
B; B22; B22C; B22C7/00; B22C7/02
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
44 words
A method for making a disposable model for a precision investment casting, which comprises casting a modeling material consisting essentially of naphthalene or para-dichlorobenzene into a pattern mold at a temperature of 80°-150° C and at a casting speed of 5 to 0.1 kg/second.
Claim 2
Independent Claim
44 words
A method for making a disposable model for a precision investment casting, which comprises casting a modeling material consisting essentially of naphthalene or para-dichlorobenzene into a pattern mold at a temperature of 80°-150° C and at a casting speed of 5 to 0.1 kg/second.
Claim 3
Independent Claim
86 words
A method for making a disposable model for a precision inventment casting, which comprises casting a modeling material consisting essentially of naphthalene or para-dichlorobenzene and a resin selected from the group consisting of polystyrene, polyethylene, polyvinyl acetate and mixtures thereof, said resin being contained in an amount of 20% by weight of less on the basis of the whole weight of the modeling material, into a pattern mold at a temperature of 80° to 150° C and at a casting speed of 5 to 0.1 kg/second.
Claim 4
Independent Claim
86 words
A method for making a disposable model for a precision inventment casting, which comprises casting a modeling material consisting essentially of naphthalene or para-dichlorobenzene and a resin selected from the group consisting of polystyrene, polyethylene, polyvinyl acetate and mixtures thereof, said resin being contained in an amount of 20% by weight of less on the basis of the whole weight of the modeling material, into a pattern mold at a temperature of 80° to 150° C and at a casting speed of 5 to 0.1 kg/second.
Claim 5
Dependent Claim
31 words
The method according to claim 2, wherein the resin is contained in an amount of 0.5 to 15% by weight on the basis of the whole weight of the modeling material.