Abstract

Abstract In an electrochemical cell, such as a sodium sulphur cell, having a solid ceramic sodium-ion permeable electrolyte forming part of the boundary of a sodium-containing region, to seal this region, the ceramic electrolyte or a ceramic extension thereof is sealed to a metal housing or metal closure element using glass with the glass-to-metal interface protected against the effect of sodium vapour by a niobium coating over the metal in the region where the interface is exposed to the sodium or this interface is protected from such exposure by niobium foil.

Inventors

  • 👤 Roger J. Bones

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 06:31
CPC Classifications
H; H01; H01M; H01M10/00; H01M10/36; H01M10/39; H01M10/3909; Y; Y02; Y02E; Y02E60/00; Y02E60/10; Y02P; Y02P70/00; Y02P70/50

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 103 words
In an electrochemical device having a sodium-containing region partially bounded by a sodium-ion permeable solid ceramic electrolyte element and having the sodium-containing region sealed by a sodium-resistant glass seal joining the ceramic electrolyte element or a ceramic extension thereof to a metal member, the improvement which comprises providing a protective layer of film of niobium secured to said metal member in the region thereof exposed to the sodium in said sodium-containing region, and extending into said glass seal to protect at least the periphery of the interface between said glass seal and said metal member which is subjected to exposure to the sodium.
Claim 2
Dependent Claim 103 words
In an electrochemical device having a sodium-containing region partially bounded by a sodium-ion permeable solid ceramic electrolyte element and having the sodium-containing region sealed by a sodium-resistant glass seal joining the ceramic electrolyte element or a ceramic extension thereof to a metal member, the improvement which comprises providing a protective layer of film of niobium secured to said metal member in the region thereof exposed to the sodium in said sodium-containing region, and extending into said glass seal to protect at least the periphery of the interface between said glass seal and said metal member which is subjected to exposure to the sodium.
Claim 3
Dependent Claim 66 words
In an electrochemical device as claimed in claim 1 having also a steel housing partially bounding said sodium-containing region, the improvement which comprises providing said metal member as an intermediate metal member between said housing and said glass seal, said intermediate metal member being formed of a nickel alloy having a coefficient of thermal expansion similar to that of said glass and said ceramic electrolyte element.
Claim 4
Dependent Claim 22 words
In an electrochemical device as claimed in claim 2, the improvement which comprises forming said intermediate member of a nickel-iron corrosion-resistant alloy.
Claim 5
Dependent Claim 21 words
In an electrochemical device as claimed in claim 3, the improvement wherein said nickel-iron alloy in Nilo 42 or Nilo K.
Claim 6
Dependent Claim 103 words
In an electrochemical cell having a sodium-containing region partially bounded by a sodium-ion permeable solid ceramic electrolyte element and having the sodium-containing region sealed by a sodium-resistant glass seal joining the ceramic electrolyte element or a ceramic extension thereof to a metal member, the improvement which comprises providing a coating of niobium over the surface of said metal member at least in the region of the periphery of the interface between said glass seal and said metal member which is subjected to exposure to sodium to prevent sodium vapour reaching any region of direct contact between said glass seal and said metal member.
Claim 7
Dependent Claim 103 words
In an electrochemical cell having a sodium-containing region partially bounded by a sodium-ion permeable solid ceramic electrolyte element and having the sodium-containing region sealed by a sodium-resistant glass seal joining the ceramic electrolyte element or a ceramic extension thereof to a metal member, the improvement which comprises providing a coating of niobium over the surface of said metal member at least in the region of the periphery of the interface between said glass seal and said metal member which is subjected to exposure to sodium to prevent sodium vapour reaching any region of direct contact between said glass seal and said metal member.
Claim 8
Dependent Claim 112 words
In an electrochemical cell having a sodium-containing region partially bounded by a sodium-ion permeable solid ceramic electrolyte element and having the sodium-containing region sealed by a sodium-resistant glass seal joining the ceramic electrolyte element or a ceramic extension thereof to a metal member, the improvement which comprises providing a film of niobium secured to said metal member in the region thereof exposed to the sodium in said sodium containing region, said film extending into said glass seal to form a sealed region within said sodium-containing region, said sealed region including the periphery of the interface between said glass seal and said metal member to protect said periphery from exposure to said sodium.
Claim 9
Dependent Claim 112 words
In an electrochemical cell having a sodium-containing region partially bounded by a sodium-ion permeable solid ceramic electrolyte element and having the sodium-containing region sealed by a sodium-resistant glass seal joining the ceramic electrolyte element or a ceramic extension thereof to a metal member, the improvement which comprises providing a film of niobium secured to said metal member in the region thereof exposed to the sodium in said sodium containing region, said film extending into said glass seal to form a sealed region within said sodium-containing region, said sealed region including the periphery of the interface between said glass seal and said metal member to protect said periphery from exposure to said sodium.
Claim 10
Dependent Claim 122 words
A sodium sulphur cell having a solid sodium-ion permeable ceramic electrolyte element separating a sodium compartment from a cathodic reactant compartment wherein the sodium compartment is at least partially bounded by a metal housing and is sealed by sealing means between the electrolyte and the housing, said sealing means including glass as a bonding agent between the ceramic electrolyte element or a ceramic extension thereof and said metal housing or an intermediate metal member attached to said housing and wherein a protective niobium coating or foil is provided over the metal to protect the interface between said glass and said metal housing or intermediate metal member at least in the region where said interface is exposed to sodium from the sodium compartment.
Claim 11
Dependent Claim 122 words
A sodium sulphur cell having a solid sodium-ion permeable ceramic electrolyte element separating a sodium compartment from a cathodic reactant compartment wherein the sodium compartment is at least partially bounded by a metal housing and is sealed by sealing means between the electrolyte and the housing, said sealing means including glass as a bonding agent between the ceramic electrolyte element or a ceramic extension thereof and said metal housing or an intermediate metal member attached to said housing and wherein a protective niobium coating or foil is provided over the metal to protect the interface between said glass and said metal housing or intermediate metal member at least in the region where said interface is exposed to sodium from the sodium compartment.
Claim 12
Dependent Claim 42 words
A sodium cell as claimed in claim 7 wherein said protective metal coating is provided over a base metal member having a coefficient of expansion similar to that of said coating material, said base metal member being secured in said metal housing.
Claim 13
Dependent Claim 40 words
A sodium sulphur cell as claimed in claim 7 wherein the electrolyte is a beta-alumina tube with an alpha-alumina flange secured to the beta-alumina tube and wherein said alpha-alumina flange is sealed to a cylindrical housing by said sealing means.
Claim 14
Dependent Claim 74 words
A sodium sulphur cell as claimed in claim 7 wherein the sodium compartment is an annular region around the outside of the beta-alumina tube within an outer cylindrical steel housing and wherein a nickel-iron corrosion-resistant ring welded to the open end of the housing and extending downwardly therein, has a coating of niobium at least in the region of the ring where the interface between said ring and said glass is exposed to sodium.
Claim 15
Dependent Claim 22 words
A sodium sulphur cell as claimed in claim 10 wherein said coating is a niobium coating of 10 to 200 microns thickness.
Claim 16
Dependent Claim 113 words
A sodium sulphur cell as claimed in claim 7 wherein the sodium compartment is an annular region around the outside of the beta-alumina tube within an outer cylindrical steel housing and wherein a nickel-iron corrosion-resistant ring welded to the open end of the housing and extending downwardly therein has niobium foil secured along one edge of the foil to the ring in a part thereof which is exposed to the sodium, the foil extending around the surface of the ring, so as to extend into the glass and thereby cover the surface of the ring at the region of the interface between said ring and said glass which is exposed to the sodium.
Claim 17
Dependent Claim 88 words
A sodium sulphur cell as claimed in claim 7 wherein an annular alpha-alumina flange is secured to the open end of a beta-alumina electrolyte tube, said alpha-alumina flange having an annular groove therein, and wherein a metal member is provided which is secured to the end of a cylindrical steel housing for the cell, said metal member extending into said annular groove and being secured by glass in that groove, said metal member, where it extends into the groove, being protected by said niobium plating or niobium foil.

References Cited (Backward Citations)

US3441446A Cited
US3421945A Cited
US3468709A Cited
US3756856A Cited
US3982959A Cited
US3946751A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-02-13 1981-08-15 1982-02-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-02-13 1985-08-15 1986-02-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-02-13 1989-08-15 1990-02-14 $7700.00 Window Closed / Lapsed