← Back to Patent Explorer
US4073760A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of packaging asphalt material and improved product resulting therefrom

Assignee: H C PRICE Co
•
Filing: 1976-07-23
•
Granted: 1978-02-14
•
Expires: 1996-07-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of providing asphalt base coating material for pipe and a novel container for holding the coating material are the subject of the present application. An asphalt coating material comprising 10% to 25% by weight asphalt and 75% to 90% by weight sand-lime aggregate is used to coat the weld joints of pipe previously coated with similar material along its length for corrosion protection. The weld joint coating material is delivered to a coating station in easy to handle small size containers. The containers comprise no more than about 5% of the weight of the material contained thereby and are constructed primarily from a material containing at least one of the members of the group consisting of polyethylene, polypropylene and polyethylene-polypropylene copolymer. The containers are placed in a chopper where they are reduced in size along with the coating material. The chopped mixture of particles are then melted and stirred until a relatively even mixture of a flowable liquid is presented.

Inventors

  • 👤 Robert J. Harris
  • 👤 Gail T. Sikes

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 22:36
CPC Classifications
E; E01; E01C; E01C19/00; E01C19/02; E01C19/10; E01C19/1059; E01C19/1068; C; C08; C08L; C08L95/00

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 149 words
A method of providing asphalt base coating material for pipe wherein said material comprises about 10% to 25% by weight asphalt and about 75% to 90% by weight aggregate, said method comprising: supplying said coating material in a plurality of individual containers, each of which has a weight of no more than about 5% of the weight of the coating material contained thereby, and each of said containers being constructed primarily from a material containing at least one member of the group consisting of polyethylene, polypropylene, and polyethylene-polypropylene copolymer; chopping said containers and said coating material to reduce the size thereof and present a mixture of said container and said coating material particles; raising the temperature of said mixture to melt said particles and present a flowable liquid; and stirring said liquid to distribute the melted container particles throughout the melted coating material particles and present a coating composition.
Claim 2
Independent Claim 149 words
A method of providing asphalt base coating material for pipe wherein said material comprises about 10% to 25% by weight asphalt and about 75% to 90% by weight aggregate, said method comprising: supplying said coating material in a plurality of individual containers, each of which has a weight of no more than about 5% of the weight of the coating material contained thereby, and each of said containers being constructed primarily from a material containing at least one member of the group consisting of polyethylene, polypropylene, and polyethylene-polypropylene copolymer; chopping said containers and said coating material to reduce the size thereof and present a mixture of said container and said coating material particles; raising the temperature of said mixture to melt said particles and present a flowable liquid; and stirring said liquid to distribute the melted container particles throughout the melted coating material particles and present a coating composition.
Claim 3
Dependent Claim 23 words
A method as set forth in claim 1, wherein said temperature raising step comprises elevating said temperature to about 300° to 400° F.
Claim 4
Dependent Claim 20 words
A method as set forth in claim 1, wherein said chopping step comprises shredding said containers and said coating material.
Claim 5
Dependent Claim 51 words
A method as set forth in claim 3, wherein said container comprises about 10% to 15% by weight polyethylene, about 10% to 15% by weight polypropylene-polyethylene copolymer and about 70% to 80% polypropylene, and the total weight of said container comprises about 1.7% by weight of the coating material contained thereby.

References Cited (Backward Citations)

US2918940A Cited
US3853800A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-02-13 1981-08-15 1982-02-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-02-13 1985-08-15 1986-02-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-02-13 1989-08-15 1990-02-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag