← Back to Patent Explorer
US4070498A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of manufacturing fluorescent screen of color picture tube

Assignee: Hitachi Ltd
•
Filing: 1976-07-30
•
Granted: 1978-01-24
•
Expires: 1996-07-30
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for manufacturing a fluorescent screen of a color picture tube by the steps of forming a coating of opto-hardening material on the inner surface of the faceplate of the panel of a color picture tube and exposing to a light and hardening selectively the coating thereby to form a matrix of stripes of the opto-hardening material, in which the selective exposure is performed by projecting a light derived from a light source having a predetermined width from each of at least two positions which are separated from the inner surface of the faceplate by a predetermined distance and also separated from each other onto the coating of the opto-hardening material formed on the faceplate through a slot of a predetermined width of a mask located between the inner surface of the faceplate and the light source, whereby the width of the stripe changes little even when the luminous intensity of the light source changes.

Inventors

  • 👤 Masahiro Nishizawa
  • 👤 Takehiko Ueyama

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 20:17
CPC Classifications
H; H01; H01J; H01J9/00; H01J9/20; H01J9/22; H01J9/227; H01J9/2271; H01J9/2272

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 252 words
A method for manufacturing the fluorescent screen of a color picture tube including the steps of forming a coating of opto-hardening material on the inner surface of the faceplate of the panel of a color picture tube and exposing to a light and hardening selectively the coating thereby to form a matrix of stripes of opto-hardening material, in which said selective exposure is performed by projecting a light derived from a light source having a predetermined width from each of at least two positions onto said coating of opto-hardening material formed on said faceplate through a slot with a predetermined width of a shadow mask located between said inner surface of said faceplate and said positions whereby the inclination of the energy level distribution curve of said projected light is steep around the portion where the energy level is equal to that required to harden said coating, said positions being separated from said inner surface of said faceplate by a predetermined distance and spaced from each other in a direction parallel to the width of said slot and by a distance selected so that the light-exposed area on said coating obtained by light projection from said light source located at one of said positions overlaps with the light-exposed area obtained by light projection from said light source located at the other position, and selecting a light energy of said projected light such that the coating is hardened at only an area where the light projections from all of said positions are applied.
Claim 2
Independent Claim 252 words
A method for manufacturing the fluorescent screen of a color picture tube including the steps of forming a coating of opto-hardening material on the inner surface of the faceplate of the panel of a color picture tube and exposing to a light and hardening selectively the coating thereby to form a matrix of stripes of opto-hardening material, in which said selective exposure is performed by projecting a light derived from a light source having a predetermined width from each of at least two positions onto said coating of opto-hardening material formed on said faceplate through a slot with a predetermined width of a shadow mask located between said inner surface of said faceplate and said positions whereby the inclination of the energy level distribution curve of said projected light is steep around the portion where the energy level is equal to that required to harden said coating, said positions being separated from said inner surface of said faceplate by a predetermined distance and spaced from each other in a direction parallel to the width of said slot and by a distance selected so that the light-exposed area on said coating obtained by light projection from said light source located at one of said positions overlaps with the light-exposed area obtained by light projection from said light source located at the other position, and selecting a light energy of said projected light such that the coating is hardened at only an area where the light projections from all of said positions are applied.
Claim 3
Dependent Claim 87 words
A manufacturing method of the fluorescent screen of a color picture tube according to claim 1, in which said light source having a predetermined width is located at one of said two positions and projects the light beam onto the coating of opto-hardening material through said slot and then said light source is moved to the other position and projects the light beam onto the same coating through the same slot, while the projection of the light beam is interrupted during the movement of said light source.

References Cited (Backward Citations)

US3993487A Cited
US3936302A Cited
US3779760A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-01-23 1981-07-25 1982-01-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-01-23 1985-07-25 1986-01-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-01-23 1989-07-25 1990-01-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag