US4065370A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method of ion plating a thin metallic strip for flashlamp starting
Assignee: United States Department of the Army
•
Filing: 1977-01-28
•
Granted: 1977-12-27
•
Expires: 1997-01-28
Abstract
Abstract A method of insuring efficient triggering of a laser flashlamp by ion plag to the outer surface of the quartz envelope of the flashlamp and an elongated thin electrically conductive strip which consists of an underlying thin layer of silver coated with a thin layer of nickel.
Inventors
- 👤 Lowell Noble
- 👤 James T. Gaspar
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-25 06:50
CPC Classifications
H; H01; H01S; H01S3/00; H01S3/09; H01S3/091; H01S3/0915; H01S3/092; C; C23; C23C; C23C14/00; C23C14/22; C23C14/24; C23C14/32; H01J; H01J61/00; H01J61/02; H01J61/54; H01J61/547
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
83 words
A method of insuring triggering of a laser flashlamp by application of an electrical impulse to an elongated metal strip permanently affixed to the outer surface of the quartz envelope of said flashlamp, comprising the steps of forming said metal strip by masking said flashlamp envelope to leave exposed an elongated region of said envelope, ion plating onto said exposed region of said envelope a thing layer of silver, and ion plating onto said plated layer of silver a thin layer of nickel.
Claim 2
Independent Claim
83 words
A method of insuring triggering of a laser flashlamp by application of an electrical impulse to an elongated metal strip permanently affixed to the outer surface of the quartz envelope of said flashlamp, comprising the steps of forming said metal strip by masking said flashlamp envelope to leave exposed an elongated region of said envelope, ion plating onto said exposed region of said envelope a thing layer of silver, and ion plating onto said plated layer of silver a thin layer of nickel.
Claim 3
Dependent Claim
19 words
The method of claim 1 wherein each of said layers has a thickness of at least 5000 Angstrom units.
Claim 4
Dependent Claim
59 words
The method of claim 1 wherein said ion plating steps include evaporating said layer material in a partially evacuated enclosure, ionizing said evaporated material in an inert gas plasma created by high voltage discharge into said gas and accelerating said ionized material to said flashlamp by the high voltage created within said enclosure between said flashlamp and said enclosure.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-12-26 | 1981-06-27 | 1981-12-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-12-26 | 1985-06-27 | 1985-12-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-12-26 | 1989-06-27 | 1989-12-27 | $7700.00 | Window Closed / Lapsed |