Process for anodizing aluminum

Assignee: Individual
•
Filing: 1976-01-21
•
Granted: 1977-12-27
•
Expires: 1996-01-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Aluminum foil in the form of a continuous web for example, is anodically oxidized by first coating one side of the web with a material such as a polymeric material which is inert to the anodizing conditions and then electrolytically anodizing the uncoated side of the web. The laminate formed which can be used as a base plate for presensitized and wipe-on lithographic printing places includes an aluminium foil coated on one side with an inert material and having an anodically oxidized layer on the other side which is formed after the one side is coated with the inert material.

Inventors

  • 👤 Howard A. Fromson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 14:56
CPC Classifications
B; B41; B41N; B41N3/00; B41N3/03; B41N3/034; C; C25; C25D; C25D11/00; C25D11/02; C25D11/04; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31678; Y10T428/31692; Y10T428/31703

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 62 words
In a process wherein aluminum foil is anodically oxidized, the improvement which comprises bonding a member narrower than the aluminum foil to one side thereof, encapsulating said member by coating, prior to anodizing, the bonded side of the aluminum foil with a polymeric material which is inert to the anodizing conditions and thereafter electrolytically anodizing the uncoated side of said aluminum foil.
Claim 2
Dependent Claim 62 words
In a process wherein aluminum foil is anodically oxidized, the improvement which comprises bonding a member narrower than the aluminum foil to one side thereof, encapsulating said member by coating, prior to anodizing, the bonded side of the aluminum foil with a polymeric material which is inert to the anodizing conditions and thereafter electrolytically anodizing the uncoated side of said aluminum foil.
Claim 3
Dependent Claim 32 words
Process of claim 1 wherein the aluminum foil is in the form of a continuous web which is continuously bonded to a continuous web of said member via an inert polymeric material.
Claim 4
Dependent Claim 12 words
Process of claim 2 wherein said member is a paper base material.
Claim 5
Dependent Claim 60 words
Process for continuously anodically oxidizing an aluminum web which comprises continuously bonding the aluminum web to a second web which is narrower than the aluminum web, encapsulating the second web by continuously coating the bonded side of the aluminum web with a polymeric material inert to the anodizing conditions and then electrolytically anodizing the uncoated side of the aluminum web.
Claim 6
Dependent Claim 60 words
Process for continuously anodically oxidizing an aluminum web which comprises continuously bonding the aluminum web to a second web which is narrower than the aluminum web, encapsulating the second web by continuously coating the bonded side of the aluminum web with a polymeric material inert to the anodizing conditions and then electrolytically anodizing the uncoated side of the aluminum web.

References Cited (Backward Citations)

US2538317A Cited
DE1214510B Cited
US3270401A Cited
US3647645A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-12-26 1981-06-27 1981-12-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-12-26 1985-06-27 1985-12-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-12-26 1989-06-27 1989-12-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag