← Back to Patent Explorer
US4062907A Expired / Lapsed US ⏱️ 0.0 years remaining

Polyester hot melt adhesive

Assignee: Eastman Chemical Co
•
Filing: 1976-11-15
•
Granted: 1977-12-13
•
Expires: 1996-11-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Polyesters useful as hot melt adhesives are prepared from selected dicarboxylic acids and selected diols, which include a critical range of polyoxyethylene glycols. In a first embodiment of the invention, the polyester is prepared from terephthalic acid, isophthalic acid, adipic acid, 1,4-butanediol, ethylene glycol, and 20 to 45 weight percent of the selected polyoxyethylene glycols. In a second embodiment of the invention, the polyester is prepared from terephthalic acid, acipic acid, 1,6-hexanediol, ethylene glycol, and 2 to 40 weight percent of the selected polyoxyethylene glycols.

Inventors

  • 👤 Bobby J. Sublett

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 20:57
CPC Classifications
C; C08; C08G; C08G63/00; C08G63/68; C08G63/685; C08G63/6854; C09; C09J; C09J167/00

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 136 words
A polyester having an inherent viscosity of at least 0.5 consisting essentially of A. a dicarboxylic acid component which is 1. 25 to 65 mole percent terephthalic acid, 2. 10 to 25 mole percent isophthalic acid, 3. 25 to 50 mole percent adipic acid, B. a diol component which is 1. 60 to 25 mole percent 1,4-butanediol, 2. 40 to 75 mole percent ethylene glycol, and 3. 20 to 45 weight percent, based on the weight of the polyester, of a polyoxyethylene glycol selected from the group consisting of ##STR5## where x is in the range of 1 to 127 and y is in the range of 1 to 110, ##STR6## where x is in the range of 16 to 612, and (c) H(OCH.sub.2 CH.sub.2).sub.x --OH where x is in the range of 4 to 180.
Claim 2
Dependent Claim 136 words
A polyester having an inherent viscosity of at least 0.5 consisting essentially of A. a dicarboxylic acid component which is 1. 25 to 65 mole percent terephthalic acid, 2. 10 to 25 mole percent isophthalic acid, 3. 25 to 50 mole percent adipic acid, B. a diol component which is 1. 60 to 25 mole percent 1,4-butanediol, 2. 40 to 75 mole percent ethylene glycol, and 3. 20 to 45 weight percent, based on the weight of the polyester, of a polyoxyethylene glycol selected from the group consisting of ##STR5## where x is in the range of 1 to 127 and y is in the range of 1 to 110, ##STR6## where x is in the range of 16 to 612, and (c) H(OCH.sub.2 CH.sub.2).sub.x --OH where x is in the range of 4 to 180.
Claim 3
Dependent Claim 57 words
A polyester having an inherent viscosity of at least 0.5 consisting essentially of A. a dicarboxylic acid component which is 1. 40 to 60 mole percent terephthalic acid, 2. 15 to 25 mole percent isophthalic acid, 3. 25 to 40 mole percent adipic acid, B. a diol component which is 1. 60 to 40 mole percent 1,4-butanediol,
Claim 4
Dependent Claim 57 words
A polyester having an inherent viscosity of at least 0.5 consisting essentially of A. a dicarboxylic acid component which is 1. 40 to 60 mole percent terephthalic acid, 2. 15 to 25 mole percent isophthalic acid, 3. 25 to 40 mole percent adipic acid, B. a diol component which is 1. 60 to 40 mole percent 1,4-butanediol,
Claim 5
Dependent Claim 78 words
40 to 60 mole percent ethylene glycol, and 3. 30 to 40 weight percent, based on the weight of the polyester, of a polyoxyethylene glycol selected from the group consisting of ##STR7## where x is in the range of 1 to 127 and y is in the range of 1 to 110, ##STR8## where x is in the range of 16 to 612, and (c) H(OCH.sub.2 CH.sub.2).sub.x --OH where x is in the range of 4 to 180.
Claim 6
Dependent Claim 78 words
40 to 60 mole percent ethylene glycol, and 3. 30 to 40 weight percent, based on the weight of the polyester, of a polyoxyethylene glycol selected from the group consisting of ##STR7## where x is in the range of 1 to 127 and y is in the range of 1 to 110, ##STR8## where x is in the range of 16 to 612, and (c) H(OCH.sub.2 CH.sub.2).sub.x --OH where x is in the range of 4 to 180.
Claim 7
Dependent Claim 128 words
A polyester having an inherent viscosity of at least 0.5 consisting essentially of A. a dicarboxylic acid component which is 1. 100 to 60 mole percent terephthalic acid, 2. 0 to 40 mole percent adipic acid, B. a diol component which is 1. 70 to 30 mole percent 1,6-hexanediol, 2. 30 to 70 mole percent ethylene glycol, and 3. 2 to 40 weight percent, based on the weight of the polyester, of a polyoxyethylene glycol selected from the group consisting of ##STR9## where x is in the range of 1 to 127 and y is in the range of 1 to 110, ##STR10## where x is in the range of 16 to 612, and (c) H(OCH.sub.2 CH.sub.2).sub.x --OH where x is in the range of 4 to 180.
Claim 8
Dependent Claim 128 words
A polyester having an inherent viscosity of at least 0.5 consisting essentially of A. a dicarboxylic acid component which is 1. 100 to 60 mole percent terephthalic acid, 2. 0 to 40 mole percent adipic acid, B. a diol component which is 1. 70 to 30 mole percent 1,6-hexanediol, 2. 30 to 70 mole percent ethylene glycol, and 3. 2 to 40 weight percent, based on the weight of the polyester, of a polyoxyethylene glycol selected from the group consisting of ##STR9## where x is in the range of 1 to 127 and y is in the range of 1 to 110, ##STR10## where x is in the range of 16 to 612, and (c) H(OCH.sub.2 CH.sub.2).sub.x --OH where x is in the range of 4 to 180.
Claim 9
Dependent Claim 128 words
A polyester having an inherent viscosity of at least 0.5 consisting essentially of A. a dicarboxylic acid component which is 1. 80 to 60 mole percent terephthalic acid, 2. 20 to 40 mole percent adipic acid, B. a diol component which is 1. 60 to 40 mole percent 1,6-hexanediol, 2. 40 to 60 mole percent ethylene glycol, and 3. 5 to 30 weight percent, based on the weight of the polyester, of a polyoxyethylene glycol selected from the group consisting of ##STR11## where x is in the range of 1 to 127 and y is in the range of 1 to 110, ##STR12## where x is in the range of 16 to 612, and (c) H(OCH.sub.2 CH.sub.2).sub.x --OH where x is in the range of 4 to 180.
Claim 10
Dependent Claim 128 words
A polyester having an inherent viscosity of at least 0.5 consisting essentially of A. a dicarboxylic acid component which is 1. 80 to 60 mole percent terephthalic acid, 2. 20 to 40 mole percent adipic acid, B. a diol component which is 1. 60 to 40 mole percent 1,6-hexanediol, 2. 40 to 60 mole percent ethylene glycol, and 3. 5 to 30 weight percent, based on the weight of the polyester, of a polyoxyethylene glycol selected from the group consisting of ##STR11## where x is in the range of 1 to 127 and y is in the range of 1 to 110, ##STR12## where x is in the range of 16 to 612, and (c) H(OCH.sub.2 CH.sub.2).sub.x --OH where x is in the range of 4 to 180.

References Cited (Backward Citations)

US3013914A Cited
US3423281A Cited
US3682863A Cited
US3669921A Cited
US3873639A Cited
US3932326A Cited
US3867479A Cited
US3948859A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-12-12 1981-06-13 1981-12-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-12-12 1985-06-13 1985-12-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-12-12 1989-06-13 1989-12-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag