Abstract

Abstract A method for the rapid determination of corrosion rates on a metallic material immersed in an electrolyte employs an electrochemical cell including at least one electrode of the material whose corrosion rate is to be determined and at least one other electrode also immersed in the same electrolyte. External forcing and measuring circuits are provided by means of which a first potential may be impressed across the immersed electrodes and the resulting current flow measured; the same circuits are also employed to impress a second potential and to measure the resulting current. Both said first and second potentials are so selected that they lie within the characteristic of the corroding cell governed by the exponential Tafel relationship. The freely corroding current for the test electrode is then determined by extrapolating the Tafel curve to zero impressed potential. The freely corroding current is then manipulated graphically or mathematically to give the corrosion rate in appropriate units.

Inventors

  • 👤 Wayne M. Gauntt
  • 👤 Earl L. Pye

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 23:08
CPC Classifications
G; G01; G01N; G01N17/00; G01N17/02

Claims Analysis

Total Claims: 23
Claim 1
Independent Claim 261 words
A method for determining the freely corroding current density of a metallic substance immersed in an electrolyte, comprising the steps of: providing a working electrode formed of said substance, providing a counter electrode formed of a conductive material, providing a reference electrode formed of a conductive substance, immersing said three electrodes in said electrolyte, establishing by external means a first potential difference, not less than 50 millivolts in magnitude, across said working and reference electrodes, measuring the current flow induced by said first potential difference through said counter electrode after the elapse of a predetermined first time period, said first time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said first potential difference, measuring said first potential between said working and reference electrodes, recording said current and said potential difference, establishing by said external means a second potential difference, substantially higher in magnitude than said first potential difference, between said working and reference electrodes, recording said second potential difference and the current resulting therefrom after the elapse of a second pre-determined time period, said second time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said second potential difference, converting said current measurements into current density measurements, deriving the linear equation passing through the pair of coordinate points represented by the measured first and second potential differences and by the logarithms of the corresponding measured current densities, and determining, by means of said equation, the freely corroding current density at zero applied potential difference.
Claim 2
Independent Claim 261 words
A method for determining the freely corroding current density of a metallic substance immersed in an electrolyte, comprising the steps of: providing a working electrode formed of said substance, providing a counter electrode formed of a conductive material, providing a reference electrode formed of a conductive substance, immersing said three electrodes in said electrolyte, establishing by external means a first potential difference, not less than 50 millivolts in magnitude, across said working and reference electrodes, measuring the current flow induced by said first potential difference through said counter electrode after the elapse of a predetermined first time period, said first time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said first potential difference, measuring said first potential between said working and reference electrodes, recording said current and said potential difference, establishing by said external means a second potential difference, substantially higher in magnitude than said first potential difference, between said working and reference electrodes, recording said second potential difference and the current resulting therefrom after the elapse of a second pre-determined time period, said second time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said second potential difference, converting said current measurements into current density measurements, deriving the linear equation passing through the pair of coordinate points represented by the measured first and second potential differences and by the logarithms of the corresponding measured current densities, and determining, by means of said equation, the freely corroding current density at zero applied potential difference.
Claim 3
Dependent Claim 35 words
The method of claim 1 wherein said first potential difference is selected in the range between 50 and 200 millivolts and said second potential difference is selected in the range between 100 and 400 millivolts.
Claim 4
Dependent Claim 13 words
The method of claim 2, wherein said conductive substance is said metallic substance.
Claim 5
Dependent Claim 17 words
The method of claim 1 wherein said conductive material of the counter electrode is said metallic substance.
Claim 6
Dependent Claim 15 words
The method of claim 4, wherein, additionally, said conductive substance is also said metallic substance.
Claim 7
Dependent Claim 17 words
The method of claim 1, wherein said pre-determined time periods are between ten seconds and fifty seconds.
Claim 8
Dependent Claim 22 words
The method of claim 1, wherein said conductive substance is selected from the following materials: platinum, calomel, copper/copper sulphate, and silver/silver chloride.
Claim 9
Dependent Claim 37 words
The method of claim 1, wherein said linear equation is solved by plotting said pair of coordinate points on graph paper and extending a straight line there through to its intercept on the logarithmic current density axis.
Claim 10
Independent Claim 301 words
A method for determining the freely corroding current density of a metallic substance immersed in an electrolyte, comprising the steps of: providing a first working electrode formed of said substance, providing a second working electrode formed of said metallic substance, providing a counter electrode formed of a conductive material, providing a reference electrode formed of a conductive substance, immersing said four electrodes in said electrolyte, establishing by external means a first potential difference, selected in the range between 50 and 200 millivolts, across said first working and said reference electrodes, measuring the current flow induced by said first potential difference through said counter electrode after the elapse of a predetermined first time period, said first time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said first potential difference, measuring said first potential difference between said first working and said reference electrodes, recording said first potential difference and said current induced thereby, establishing by said external means a second potential difference, substantially higher in magnitude than said first potential difference and selected in the range between 100 and 400 millivolts, across said second working and said reference electrodes, measuring and recording said second potential difference and the current flow resulting therefrom through said counter electrode after the elapse of a second pre-determined time period, said second time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said second potential difference, converting said current measurements into current density measurements, deriving the linear equation passing through the pair of coordinate points represented by the measured first and second potential differences and by the logarithms of the corresponding measured current densities, and determining, by means of said equation, the freely corroding current density at zero applied potential difference.
Claim 11
Independent Claim 301 words
A method for determining the freely corroding current density of a metallic substance immersed in an electrolyte, comprising the steps of: providing a first working electrode formed of said substance, providing a second working electrode formed of said metallic substance, providing a counter electrode formed of a conductive material, providing a reference electrode formed of a conductive substance, immersing said four electrodes in said electrolyte, establishing by external means a first potential difference, selected in the range between 50 and 200 millivolts, across said first working and said reference electrodes, measuring the current flow induced by said first potential difference through said counter electrode after the elapse of a predetermined first time period, said first time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said first potential difference, measuring said first potential difference between said first working and said reference electrodes, recording said first potential difference and said current induced thereby, establishing by said external means a second potential difference, substantially higher in magnitude than said first potential difference and selected in the range between 100 and 400 millivolts, across said second working and said reference electrodes, measuring and recording said second potential difference and the current flow resulting therefrom through said counter electrode after the elapse of a second pre-determined time period, said second time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said second potential difference, converting said current measurements into current density measurements, deriving the linear equation passing through the pair of coordinate points represented by the measured first and second potential differences and by the logarithms of the corresponding measured current densities, and determining, by means of said equation, the freely corroding current density at zero applied potential difference.
Claim 12
Dependent Claim 22 words
The method of claim 9, wherein said conductive substance is selected from the following materials: platinum, calomel, copper/copper sulphate, and silver/silver chloride.
Claim 13
Dependent Claim 17 words
The method of claim 9 whrein said conductive material of the counter electrode is said metallic substance.
Claim 14
Dependent Claim 68 words
The method of claim 9, including the additional steps of: providing a second counter electrode of a conductive material, immersing said second counter electrode in said electrolyte, establishing said second potential difference across said second working and said reference electrodes, and measuring and recording said second potential difference and the current flow resulting therefrom through said second counter electrode after the elapse of said second predetermined time period.
Claim 15
Dependent Claim 30 words
The method of claim 12 wherein said conductive material of said first and second counter electrodes is the same as said metallic substance of said first and second working electrodes.
Claim 16
Dependent Claim 20 words
The method of claim 9, wherein said predetermined time periods are intermediate between ten seconds and fifty seconds in duration.
Claim 17
Independent Claim 263 words
A method for determining the freely corroding current density of a metallic substance immersed in an electrolyte, comprising the steps of: providing a working electrode formed of said substance, providing a counter electrode formed of a conductive material, immersing said two electrodes in said electrolyte, establishing by external means a first potential difference, not less than 50 millivolts in magnitude, across said working and counter electrodes, measuring the current flow induced by said first potential difference through said working electrode after the elapse of a predetermined first time period, said first time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said first potential difference, measuring said first potential difference between said working and said counter electrodes, recording said first potential difference and said current induced thereby, establishing by said external means a second potential difference, substantially higher in magnitude than said first potential difference, between said working and said counter electrodes, recording said second potential difference, and the current flow through said working electrode induced thereby after the elapse of a second pre-determined time period, said second time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said second potential difference, converting said current measurements into current density measurements, deriving the linear equation passing through the pair of coordinate points represented by said measured first and second potential difference and by the logarithms of the corresponding measured current densities, and determining, by means of said equation, the freely corroding current density at zero applied potential difference.
Claim 18
Independent Claim 263 words
A method for determining the freely corroding current density of a metallic substance immersed in an electrolyte, comprising the steps of: providing a working electrode formed of said substance, providing a counter electrode formed of a conductive material, immersing said two electrodes in said electrolyte, establishing by external means a first potential difference, not less than 50 millivolts in magnitude, across said working and counter electrodes, measuring the current flow induced by said first potential difference through said working electrode after the elapse of a predetermined first time period, said first time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said first potential difference, measuring said first potential difference between said working and said counter electrodes, recording said first potential difference and said current induced thereby, establishing by said external means a second potential difference, substantially higher in magnitude than said first potential difference, between said working and said counter electrodes, recording said second potential difference, and the current flow through said working electrode induced thereby after the elapse of a second pre-determined time period, said second time period being substantially shorter than the time required to establish equilibrium current flow upon the imposition of said second potential difference, converting said current measurements into current density measurements, deriving the linear equation passing through the pair of coordinate points represented by said measured first and second potential difference and by the logarithms of the corresponding measured current densities, and determining, by means of said equation, the freely corroding current density at zero applied potential difference.
Claim 19
Dependent Claim 35 words
The method of claim 15 wherein said first potential difference is selected in the range between 50 and 200 millivolts and said second potential difference is selected in the range between 100 and 400 millivolts.
Claim 20
Dependent Claim 17 words
The method of claim 16 wherein said conductive material of the counter electrode is said metallic substance.
Claim 21
Dependent Claim 22 words
The method of claim 15, wherein said conductive material is selected from the following group: platinum, calomel, copper/copper sulphate, and silver/silver chloride.
Claim 22
Dependent Claim 36 words
The method of claim 15 wherein said linear equation is solved by plotting said pair of coordinate points on graph paper and extending a straight line therethrough to its intercept of the logarithmic current density axis.
Claim 23
Dependent Claim 20 words
The method of claim 15, wherein said predetermined time periods are selected in the range between 10 and 50 seconds.

References Cited (Backward Citations)

US3855101A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-10-31 1981-05-02 1981-11-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-10-31 1985-05-02 1985-11-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-10-31 1989-05-02 1989-11-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag