Abstract

Abstract A method of reducing the switching time of certain semiconductor devices and particularly gain-operated semiconductor devices. The depth of maximum defect generation in a given type of semiconductor devices having a block PN junction is determined on irradiation with a given radiation source emitting particles with molecular weight of at least one (1), preferably protons or alpha particles; and the energy level of the radiation source adjusted to provide the depth of maximum defect generation adjacent a blocking PN junction of the type of semiconductor device. At least one semiconductor device of said given type of semiconductor device is positioned with a major surface thereof to be exposed to the adjusted radiation source, and thereafter irradiated with the adjusted radiation source to a given dosage level to reduce the switching time of the semiconductor device. Preferably, the semiconductor device is positioned and the energy level of the radiation source adjusted to irradiate through the major surface of the device closer the higher impurity region adjoining the blocking PN junction, and to provide the maximum defect generation in said higher impurity region adjoining the blocking PN junction but spaced from the PN junction beyond a depletion region formed at the PN junction on application of a specified blocking voltage across the PN junction of the semiconductor device.

Inventors

  • 👤 John Bartko
  • 👤 Kuan H. Sun

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 19:59
CPC Classifications
H; H10; H10P; H10P34/00; H10P34/40; Y; Y10; Y10S; Y10S148/00; Y10S148/093

Claims Analysis

Total Claims: 31
Claim 1
Independent Claim 128 words
A method of reducing the switching time of certain semiconductor devices comprising the steps of: A. determining the depth of maximum defect generation in a given type of semiconductor device having a blocking PN junction on irradiation with a given radiation source radiating particles with molecular weight of at least one; B. adjusting the energy level of said radiation source to provide the depth of maximum defect generation adjacent a blocking PN junction of said type of semiconductor device; C. positioning at least one semiconductor device of said given type with a major surface thereof to be exposed to said adjusted radiation source; and D. thereafter irradiating said semiconductor device with said adjusted radiation source to a given dosage level reducing the switching time of said semiconductor device.
Claim 2
Independent Claim 128 words
A method of reducing the switching time of certain semiconductor devices comprising the steps of: A. determining the depth of maximum defect generation in a given type of semiconductor device having a blocking PN junction on irradiation with a given radiation source radiating particles with molecular weight of at least one; B. adjusting the energy level of said radiation source to provide the depth of maximum defect generation adjacent a blocking PN junction of said type of semiconductor device; C. positioning at least one semiconductor device of said given type with a major surface thereof to be exposed to said adjusted radiation source; and D. thereafter irradiating said semiconductor device with said adjusted radiation source to a given dosage level reducing the switching time of said semiconductor device.
Claim 3
Dependent Claim 36 words
A method of reducing the switching time of certain semiconductor devices as set forth in claim 1 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 4
Dependent Claim 44 words
A method of reducing the switching time of certain semiconductor devices as set forth in claim 1 wherein: in step C, the semiconductor device is positioned to irradiate through a major surface thereof closer the higher impurity concentration region adjoining said blocking PN junction.
Claim 5
Dependent Claim 36 words
A method of reducing the switching time of ceratin semiconductor devices as set forth in claim 3 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 6
Dependent Claim 49 words
A method of reducing the switching time of certain semiconductor devices as set forth in claim 3 wherein: in step B, the energy level of said radiation source is adjusted to provide the depth of maximum defect generation in the higher impurity concentration region adjoining said blocking PN junction.
Claim 7
Dependent Claim 36 words
A method of reducing the switching time of certain semiconductor devices as set forth in claim 5 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 8
Dependent Claim 65 words
A method of reducing the switching time of certain semiconductor devices as set forth in claim 5 wherein: in step B, the energy level of said radiation source is adjusted to provide the depth of maximum defect generation in the higher impurity concentration region spaced adjacent a depletion region formed on application of a specified blocking voltage across said PN junction of the semiconductor device.
Claim 9
Dependent Claim 36 words
A method of reducing the switching time of certain semiconductor devices as set forth in claim 5 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 10
Independent Claim 129 words
A method of reducing the switching time of gain-operated semiconductor devices comprising the steps of: A. determining the depth of maximum defect generation in a given type of gain-operated semiconductor device having a blocking PN junction on irradiation with a given radiation source radiating particles with molecular weight of at least one; B. adjusting the energy level of said radiation source to provide the depth of maximum defect generation adjacent a blocking PN junction of said type of semiconductor device; C. positioning at least one semiconductor device of said given type with a major surface thereof to be exposed to said adjusted radiation source; and D. thereafter irradiating said semiconductor device with said adjusted radiation source to a given dosage level reducing the switching time of said semiconductor device.
Claim 11
Independent Claim 129 words
A method of reducing the switching time of gain-operated semiconductor devices comprising the steps of: A. determining the depth of maximum defect generation in a given type of gain-operated semiconductor device having a blocking PN junction on irradiation with a given radiation source radiating particles with molecular weight of at least one; B. adjusting the energy level of said radiation source to provide the depth of maximum defect generation adjacent a blocking PN junction of said type of semiconductor device; C. positioning at least one semiconductor device of said given type with a major surface thereof to be exposed to said adjusted radiation source; and D. thereafter irradiating said semiconductor device with said adjusted radiation source to a given dosage level reducing the switching time of said semiconductor device.
Claim 12
Dependent Claim 36 words
A method of reducing the switching time of gain-operated semiconductor devices as set forth in claim 9 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 13
Dependent Claim 44 words
A method of reducing the switching time of gain-operated semiconductor devices as set forth in claim 9 wherein: in step C, the semiconductor device is positioned to irradiate through a major surface thereof closer the higher impurity concentration region adjoining said blocking PN junction.
Claim 14
Dependent Claim 36 words
A method of reducing the switching time of gain-operated semiconductor devices as set forth in claim 11 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 15
Dependent Claim 49 words
A method of reducing the switching time of gain-operated semiconductor devices as set forth in claim 11 wherein: in step B, the energy level of said radiation source is adjusted to provide the depth of maximum defect generation in the higher impurity concentration region adjoining said blocking PN junction.
Claim 16
Dependent Claim 36 words
A method of reducing the switching time of gain-operated semiconductor devices as set forth in claim 5 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 17
Dependent Claim 65 words
A method of reducing the switching time of gain-operated semiconductor devices as set forth in claim 13 wherein: in step B, the energy level of said radiation source is adjusted to provide the depth of maximum defect generation in the high impurity concentration region spaced adjacent a depletion region formed on applications of a specified blocking voltage across said PN junction of the semiconductor device.
Claim 18
Dependent Claim 36 words
A method of reducing the switching time of gain-operated semiconductor devices as set forth in claim 15 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 19
Independent Claim 115 words
A method of reducing the turn-off time of thyristors comprising the steps of: A. determining the depth of maximum defect generation in a given type of thyristor on radiation with a given radiation source radiating particles with molecular weight of at least one; B. adjusting the energy level of said radiation source to provide the depth of maximum defect generation adjacent a blocking PN junction of said type of thyristor; C. positioning at least one thyristor of said given type with a major surface thereof to be exposed to said adjusted radiation source; and D. thereafter irradiating said thyristor with said adjusted radiation source to a dosage level reducing the turn-off time of said thyristor.
Claim 20
Independent Claim 115 words
A method of reducing the turn-off time of thyristors comprising the steps of: A. determining the depth of maximum defect generation in a given type of thyristor on radiation with a given radiation source radiating particles with molecular weight of at least one; B. adjusting the energy level of said radiation source to provide the depth of maximum defect generation adjacent a blocking PN junction of said type of thyristor; C. positioning at least one thyristor of said given type with a major surface thereof to be exposed to said adjusted radiation source; and D. thereafter irradiating said thyristor with said adjusted radiation source to a dosage level reducing the turn-off time of said thyristor.
Claim 21
Dependent Claim 34 words
A method of reducing the turn-off time of thyristors as set forth in claim 17 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 22
Dependent Claim 59 words
A method of reducing the turn-off time of thyristors as set forth in claim 18 wherein: in step D, the irradiating is to a dosage level between about 1 × 10 10 and about 5 × 10 11 protons per centimeter square or between about 1 × 10 9 and about 5 × 10 10 alphas per centimeter square.
Claim 23
Dependent Claim 43 words
A method of reducing the switching time of certain semiconductor devices as set forth in claim 17 wherein: in step C, the semiconductor device is positioned to irradiate through a major surface thereof closer the higher concentration region adjoining said blocking PN junction.
Claim 24
Dependent Claim 34 words
A method of reducing the turn-off time of thyristors as set forth in claim 20 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 25
Dependent Claim 60 words
A method of reducing the turn-off time of thyristors as set forth in claim 21 wherein: in step D, the irradiating is to a dosage level between about 1 × 10 10 and about 5 × 10 11 protons per centimeter square or between about 1 × 10 9 and about 5 × 10 10 alpha particles per centimeter square.
Claim 26
Dependent Claim 49 words
A method of reducing the switching time of certain semiconductor devices as set forth in claim 20 wherein: in step B, the energy level of said radiation source is adjusted to provide the depth of maximum defect generation in the higher impurity concentration region adjoining said blocking PN junction.
Claim 27
Dependent Claim 34 words
A method of reducing the turn-off time of thyristors as set forth in claim 23 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 28
Dependent Claim 60 words
A method of reducing the turn-off time of thyristors as set forth in claim 24 wherein: in step D, the irradiating is to a dosage level between about 1 × 10 10 and about 5 × 10 11 protons per centimeter square or between about 1 × 10 9 and about 5 × 10 10 alpha particles per centimeter square.
Claim 29
Dependent Claim 65 words
A method of reducing the switching time of certain semiconductor devices as set forth in claim 23 wherein: in step B, the energy level of said radiation source is adjusted to provide the depth of maximum defect generation in the higher impurity concentration region spaced adjacent a depletion region formed on application of a specified blocking voltage across said PN junction of the semiconductor device.
Claim 30
Dependent Claim 34 words
A method of reducing the turn-off time of thyristors as set forth in claim 26 wherein: in step A, said radiation source is selected from the group consisting of proton and alpha particle sources.
Claim 31
Dependent Claim 60 words
A method of reducing the turn-off time of thyristors as set forth in claim 27 wherein: in step D, the irradiating is to a dosage level between about 1 × 10 10 and about 5 × 10 11 protons per centimeter square or between about 1 × 10 9 and about 5 × 10 10 alpha particles per centimeter square.

References Cited (Backward Citations)

US3515956A Cited
US3736192A Cited
US3880675A Cited
US3881963A Cited
US3809582A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-10-31 1981-05-02 1981-11-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-10-31 1985-05-02 1985-11-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-10-31 1989-05-02 1989-11-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag