← Back to Patent Explorer
US4056400A Expired / Lapsed US ⏱️ 0.0 years remaining

Oxidation products of cellulose, hemicellulose and lignin

Assignee: Individual
•
Filing: 1975-07-28
•
Granted: 1977-11-01
•
Expires: 1995-07-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A composition which consists essentially of a mixture of oligomeric and polymeric oxidation products of cellulose, hemicellulose and lignin containing carboxy, ether and hydroxy groups as obtained by the direct oxidation of a woody plant material, preferably in an aqueous suspension thereof, using alkali hypohalite in a one stage oxidation procedure or nitrogen dioxide, alkali periodate or lead tetraacetate followed by alkali chlorite or alkali hypochlorite in a two stage oxidation procedure. The resulting oxidation products as obtained by one of these specific processes are especially valuable as additives to a surface active detergent or cleaning agent.

Inventors

  • 👤 Michael Diamantoglou
  • 👤 Helmut Magerlein
  • 👤 Rainer Zielke
  • 👤 Emery George Philomena Cornelissens

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 03:00
CPC Classifications
C; C11; C11D; C11D3/00; C11D3/16; C11D3/38; C11D3/382; C08; C08H; C08H8/00; C11D3/20; C11D3/22; C11D3/222; C11D3/223

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 129 words
A process for the production of a mixture consisting primarily of oligomeric and polymeric oxidation products of cellulose, hemicellulose and lignin containing carboxy, ether and hydroxy groups which comprises: oxidizing a woody plant material in aqueous suspension in a single stage with alkali hypohalite as the essential oxidizing agent or in two stages with nitrogen dioxide, alkali periodate or lead tetraacetate as the essential oxidizing agent of the first stage and with alkali chlorite or alkali hypochlorite as the essential oxidizing agent in the second stage, the total amount of oxidizing agent being at least two parts by weight for each part by weight of said woody plant material; separating undissolved components; and precipitating the oxidation products from the aqueous medium by means of a water-miscible organic precipitating agent.
Claim 2
Dependent Claim 129 words
A process for the production of a mixture consisting primarily of oligomeric and polymeric oxidation products of cellulose, hemicellulose and lignin containing carboxy, ether and hydroxy groups which comprises: oxidizing a woody plant material in aqueous suspension in a single stage with alkali hypohalite as the essential oxidizing agent or in two stages with nitrogen dioxide, alkali periodate or lead tetraacetate as the essential oxidizing agent of the first stage and with alkali chlorite or alkali hypochlorite as the essential oxidizing agent in the second stage, the total amount of oxidizing agent being at least two parts by weight for each part by weight of said woody plant material; separating undissolved components; and precipitating the oxidation products from the aqueous medium by means of a water-miscible organic precipitating agent.
Claim 3
Dependent Claim 39 words
A process as claimed in claim 1 wherein the oxidation with an alkali hypohalite is carried out at a pH-value in the range of about 8 to 10 and in a temperature range of about 0° to 40° C.
Claim 4
Dependent Claim 17 words
A process as claimed in claim 2 wherein said temperature range is about 10° to 25° C.
Claim 5
Dependent Claim 16 words
A process as claimed in claim 1 wherein sodium hypochlorite is used as an oxidizing agent.
Claim 6
Dependent Claim 25 words
A process as claimed in claim 1 wherein the organic precipitating agent is a primary, secondary or tertiary alcohol of 1 to 4 carbon atoms.
Claim 7
Dependent Claim 29 words
A process as claimed in claim 1 wherein the two stage oxidation is carried out with nitrogen dioxide in the first stage and sodium hypochlorite in the second stage.
Claim 8
Dependent Claim 44 words
A process as claimed in claim 4 wherein the oxidation is carried out in a single stage with said sodium hypochlorite as the essential oxidizing agent at a pH-value of about 8 to 10 and at a temperature of about 0° to 40° C.
Claim 9
Dependent Claim 16 words
A process as claimed in claim 7 wherein said temperature is about 10° to 25° C.
Claim 10
Dependent Claim 20 words
A process as claimed in claim 1 wherein the total time of the oxidation is at least about 5 hours.
Claim 11
Dependent Claim 131 words
A process for the production of a mixture consisting primarly of oligomeric and polymeric oxidation products of cellulose, hemicellulose and lignin containing carboxy, ether and hydroxy groups which comprises oxidizing a woody plant material in a single stage with alkali hypohalite as the essential oxidizing agent or in two stages with nitrogen dioxide, alkali periodate or lead tetraacetate as the essential oxidizing agent of the first stage and with alkali chlorite or alkali hypochlorite as the essential oxidizing agent in the second stage with the proviso that halogen and an aqueous alkali hydroxide are simultaneously conducted into an initial aqueous suspension of the woody plant material being oxidized, the total amount of oxidizing agent being at least two parts by weight for each part by weight of said woody plant material.
Claim 12
Dependent Claim 131 words
A process for the production of a mixture consisting primarly of oligomeric and polymeric oxidation products of cellulose, hemicellulose and lignin containing carboxy, ether and hydroxy groups which comprises oxidizing a woody plant material in a single stage with alkali hypohalite as the essential oxidizing agent or in two stages with nitrogen dioxide, alkali periodate or lead tetraacetate as the essential oxidizing agent of the first stage and with alkali chlorite or alkali hypochlorite as the essential oxidizing agent in the second stage with the proviso that halogen and an aqueous alkali hydroxide are simultaneously conducted into an initial aqueous suspension of the woody plant material being oxidized, the total amount of oxidizing agent being at least two parts by weight for each part by weight of said woody plant material.
Claim 13
Dependent Claim 44 words
A process as claimed in claim 10 wherein the oxidation is carried out in a single stage with said sodium hypochlorite as the essential oxidizing agent at a pH-value of about 8 to 10 and at a temperature of about 0° to 40° C.
Claim 14
Dependent Claim 16 words
A process as claimed in claim 11 wherein said temperature is about 10° to 25° C.
Claim 15
Dependent Claim 21 words
A process as claimed in claim 11 wherein the total reaction time for the oxidation is about 5 to 10 hours.

References Cited (Backward Citations)

US2140863A Cited
US3878037A Cited
US3907632A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-10-31 1981-05-02 1981-11-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-10-31 1985-05-02 1985-11-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-10-31 1989-05-02 1989-11-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag