← Back to Patent Explorer
US4054729A Expired / Lapsed US ⏱️ 0.0 years remaining

Rechargeable high temperature electrochemical battery

Assignee: Westinghouse Electric Corp
•
Filing: 1976-10-27
•
Granted: 1977-10-18
•
Expires: 1996-10-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A rechargeable, high temperature, electrochemical cell is made, comprising an anode containing an intermetallic compound of magnesium with silicon or magnesium with boron, a cathode containing a metal sulfide and a contacting, fused halide salt electrolyte, containing magnesium ions disposed between the anode and cathode.

Inventors

  • 👤 Arnold O. Isenberg

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 15:28
CPC Classifications
H; H01; H01M; H01M4/00; H01M4/02; H01M4/36; H01M4/38; H01M4/46; H01M10/00; H01M10/36; H01M10/39; H01M10/399; Y; Y02; Y02E; Y02E60/00; Y02E60/10

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 55 words
A rechargeable, high temperature, electrochemical cell, comprising an anode containing a battery active material selected from the group consisting of intermetallic compounds of magnesium with silicon and magnesium with boron, a cathode containing a metal sulfide, and a contacting fused halide salt electrolyte containing magnesium ions therebetween, said anode and cathode having attached electrical connections.
Claim 2
Dependent Claim 55 words
A rechargeable, high temperature, electrochemical cell, comprising an anode containing a battery active material selected from the group consisting of intermetallic compounds of magnesium with silicon and magnesium with boron, a cathode containing a metal sulfide, and a contacting fused halide salt electrolyte containing magnesium ions therebetween, said anode and cathode having attached electrical connections.
Claim 3
Dependent Claim 87 words
The rechargeable, high temperature electrochemical cell of claim 1, wherein the anode has a porous metal fiber structure, the electrolyte is disposed in a heat resistant matrix material, said matrix material being in powder of fiber form, constituting between about 5 vol.% to about 50 vol. % of the electrolyte-matrix composition, and is selected from the group consisting of MgO, Al 2 O 3 ,CaF, BN, ZrO 2 and mixtures thereof, and the intermetallic compound is selected from the group consisting of magnesium silicide and magnesium boride.
Claim 4
Dependent Claim 32 words
The rechargeable, high temperature electrochemical cell of claim 1, wherein the cathode has a porous metal fiber structure having between about 10 vol.% to about 70 vol.% of sulfide materials disposed therein.
Claim 5
Dependent Claim 44 words
The rechargeable, high temperature electrochemical cell of claim 2, wherein the electrolyte contains Mg halide impregnated within a matrix material of ZrO 2 , and the metal sulfide is selected from the group consisting of iron sulfide, nickel sulfide, copper sulfide and mixtures thereof.
Claim 6
Dependent Claim 32 words
The rechargeable, high temperature, electrochemical cell of claim 4, wherein the metal sulfide consists of particles of iron sulfide having an average particle size of between about 0.1 micron to 50 microns.
Claim 7
Dependent Claim 55 words
The rechargeable, high temperature electrochemical cell of claim 5, wherein the electrolyte is selected from the group consisting of salt mixtures of MgCl 2 -- NaCl, MgCl 2 -- NaCl -- CaF 2 , MgCl 2 -- LiCl, and MgCl 2 -- NaCl -- KCl and the battery material in the anode comprises magnesium silicide.
Claim 8
Dependent Claim 14 words
A plurality of the cells of claim 5 electrically connected to form a battery.
Claim 9
Dependent Claim 119 words
A rechargeable, electrochemical cell, operating at a temperature of between about 400° C to about 650° C, comprising an anode containing a battery active material selected from the group consisting of intermetallic compounds of magnesium with silicon and magnesium with boron, a cathode containing iron sulfide, and a contacting molten halide salt electrolyte therebetween containing magnesium ions disposed in a matrix of heat resistant materials selected from the group consisting of MgO, Al 2 O 3 , CaF, BN, ZrO 2 and mixtures thereof in powder or fiber form, said matrix constituting between about 5 vol.% to about 50 vol.% of the electrolyte-matrix composition, all enclosed in a heat resistant container, said anode and cathode having attached electrical connections.
Claim 10
Dependent Claim 119 words
A rechargeable, electrochemical cell, operating at a temperature of between about 400° C to about 650° C, comprising an anode containing a battery active material selected from the group consisting of intermetallic compounds of magnesium with silicon and magnesium with boron, a cathode containing iron sulfide, and a contacting molten halide salt electrolyte therebetween containing magnesium ions disposed in a matrix of heat resistant materials selected from the group consisting of MgO, Al 2 O 3 , CaF, BN, ZrO 2 and mixtures thereof in powder or fiber form, said matrix constituting between about 5 vol.% to about 50 vol.% of the electrolyte-matrix composition, all enclosed in a heat resistant container, said anode and cathode having attached electrical connections.
Claim 11
Dependent Claim 39 words
The rechargeable, electrochemical cell of claim 8, wherein the anode has a porous metal fiber structure, and the cathode has a porous metal fiber structure having between about 10 vol.% to about 70 vol.% of iron sulfide disposed therein.
Claim 12
Dependent Claim 56 words
The rechargeable, electrochemical cell of claim 9, wherein the electrolyte is selected from the group consisting of molten salt mixtures of MgCl 2 -- NaCl, MgCl 2 -- NaCl -- CaF 2 , MgCl 2 -- NaCl -- LiCl, and MgCl 2 -- NaCl -- KCl and the battery material in the anode is magnesium silicide.
Claim 13
Dependent Claim 17 words
The rechargeable, electrochemical cell of claim 9, wherein the battery material on the anode is magnesium boride.

References Cited (Backward Citations)

US3607402A Cited
US3980495A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-10-17 1981-04-18 1981-10-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-10-17 1985-04-18 1985-10-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-10-17 1989-04-18 1989-10-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag