← Back to Patent Explorer
US4052325A Expired / Lapsed US ⏱️ 0.0 years remaining

Liquid electrographic developer composition containing redispersible polyester toner and process

Assignee: Eastman Kodak Co
•
Filing: 1976-06-28
•
Granted: 1977-10-04
•
Expires: 1996-06-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A liquid developer containing redispersible, readily heat-fixable toner particles and a process for using the same. The developer is characterized by toner particles containing certain linear polyesters which are physically inert to the liquid carrier vehicle of the liquid developer and which, advantageously, have a melting point in the range of from about 40° to about 150° C.

Inventors

  • 👤 Domenic Santilli

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 13:52
CPC Classifications
G; G03; G03G; G03G9/00; G03G9/08; G03G9/12; G03G9/13; G03G9/132; Y; Y10; Y10S; Y10S430/00; Y10S430/001; Y10S430/105

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 257 words
An electrographic liquid developer composition comprising a mixture of electrostatically-attractable, heat-fixable redispersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (a) present in an amount of from about 0.05 to about 15 weight percent of said developer composition, (b) having a melting point in the range of from about 40° to about 150° C, and (c) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear polyester physically inert with respect to said carrier liquid, said polyester having the formula ##STR6## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; R and R 2 , which may be the same or different, represent a member of the group selected from the divalent residue of an aliphatic, alicyclic, or aromatic diol upon removal of the two hydroxy groups from said diol; R 1 is a member selected from the group consisting of the divalent residue of a sulfonamido-free aliphatic, alicyclic or aromatic dicarboxylic acid upon removal of the two carboxy groups from said acid; and R 3 represents (i) a member selected from the same group as R 1 and may be the same as or different from R 1 or (ii) the divalent residue of a disulfonamido group-containing aromatic dicarboxylic acid upon removal of the two carboxyl groups from said acid, said disulfonamido group having a monovalent cation on the amido nitrogen atom thereof.
Claim 2
Dependent Claim 257 words
An electrographic liquid developer composition comprising a mixture of electrostatically-attractable, heat-fixable redispersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (a) present in an amount of from about 0.05 to about 15 weight percent of said developer composition, (b) having a melting point in the range of from about 40° to about 150° C, and (c) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear polyester physically inert with respect to said carrier liquid, said polyester having the formula ##STR6## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; R and R 2 , which may be the same or different, represent a member of the group selected from the divalent residue of an aliphatic, alicyclic, or aromatic diol upon removal of the two hydroxy groups from said diol; R 1 is a member selected from the group consisting of the divalent residue of a sulfonamido-free aliphatic, alicyclic or aromatic dicarboxylic acid upon removal of the two carboxy groups from said acid; and R 3 represents (i) a member selected from the same group as R 1 and may be the same as or different from R 1 or (ii) the divalent residue of a disulfonamido group-containing aromatic dicarboxylic acid upon removal of the two carboxyl groups from said acid, said disulfonamido group having a monovalent cation on the amido nitrogen atom thereof.
Claim 3
Dependent Claim 25 words
An electrographic liquid developer composition as defined in claim 1 wherein R 3 is a member selected from the same group as R 1 .
Claim 4
Dependent Claim 208 words
An electrographic liquid developer composition comprising a mixture of electrostatically-attractable, heat-fixable redispersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (a) present in an amount of from about 0.05 to about 15 weight percent of said developer composition, (b) having a melting point in the range of from about 40° to about 150° C, and (c) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear crystalline polyester inert with respect to said carrier liquid, said polyester having the formula ##STR7## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; R and R 2 , which may be the same or different, represent a member of the group selected from the divalent residue of an aliphatic, alicyclic, or aromatic diol upon removal of the two hydroxy groups from said diol; and R 1 and R 3 , which may be the same or different, represent a member selected from the group consisting of the divalent residue of a sulfonamido-free aliphatic, alicyclic or aromatic dicarboxylic acid upon removal of the two carboxyl groups from said acid.
Claim 5
Dependent Claim 208 words
An electrographic liquid developer composition comprising a mixture of electrostatically-attractable, heat-fixable redispersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (a) present in an amount of from about 0.05 to about 15 weight percent of said developer composition, (b) having a melting point in the range of from about 40° to about 150° C, and (c) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear crystalline polyester inert with respect to said carrier liquid, said polyester having the formula ##STR7## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; R and R 2 , which may be the same or different, represent a member of the group selected from the divalent residue of an aliphatic, alicyclic, or aromatic diol upon removal of the two hydroxy groups from said diol; and R 1 and R 3 , which may be the same or different, represent a member selected from the group consisting of the divalent residue of a sulfonamido-free aliphatic, alicyclic or aromatic dicarboxylic acid upon removal of the two carboxyl groups from said acid.
Claim 6
Dependent Claim 29 words
An electrographic liquid developer composition as defined in claim 3 wherein said toner particles have a melting point within the range of from about 60° to about 100° C.
Claim 7
Dependent Claim 36 words
An electrographic liquid developer composition as defined in claim 3 wherein said crystalline polyester is selected from the group consisting of poly(decamethylene sebacate), poly(nonamethylene terephthalate), poly(tetramethylene succinate:sebacate), poly(ethylene sebacate), poly(p-xylylene sebacate), poly(decamethylene adipate) and poly(ethylene suberate).
Claim 8
Dependent Claim 246 words
An electrographic liquid developer composition comprising a mixture of electrostatically-attractable redispersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (a) present in an amount of from about 0.1 to about 3 weight percent of said developer composition and (b) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear polyester physically inert with respect to said carrier liquid, said polyester having the formula ##STR8## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; and R and R 2 , which may be the same or different, represent a member of the group selected from the divalent residue of an aliphatic, alicyclic, or aromatic diol upon removal of the two hydroxy groups from said diol; and R 1 and R 3 , which may be the same or different, represent a member selected from the group consisting of the divalent residue of a sulfonamido-free aliphatic, alicyclic or aromatic dicarboxylic acid upon removal of the two carboxy groups from said acid, said toner particles contained in said developer composition having an average particle size within the range of from about 0.1 to about 10 microns and having a melting point within the range of from about 60° to about 100° C., and comprising from about 0.1 to about 33 percent by weight of a colorant.
Claim 9
Dependent Claim 246 words
An electrographic liquid developer composition comprising a mixture of electrostatically-attractable redispersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (a) present in an amount of from about 0.1 to about 3 weight percent of said developer composition and (b) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear polyester physically inert with respect to said carrier liquid, said polyester having the formula ##STR8## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; and R and R 2 , which may be the same or different, represent a member of the group selected from the divalent residue of an aliphatic, alicyclic, or aromatic diol upon removal of the two hydroxy groups from said diol; and R 1 and R 3 , which may be the same or different, represent a member selected from the group consisting of the divalent residue of a sulfonamido-free aliphatic, alicyclic or aromatic dicarboxylic acid upon removal of the two carboxy groups from said acid, said toner particles contained in said developer composition having an average particle size within the range of from about 0.1 to about 10 microns and having a melting point within the range of from about 60° to about 100° C., and comprising from about 0.1 to about 33 percent by weight of a colorant.
Claim 10
Dependent Claim 38 words
An electrographic liquid developer composition as defined in claim 6 wherein said linear polyester is selected from the group consisting of poly(decamethylene sebacate), poly(nonamethylene terephthalate), poly(ethylene terephthalate:isophthalate), poly(tetramethylene succinate:sebacate), poly(ethylene sebacate), poly(p-xylylene sebacate), poly(decamethylene adipate) and poly(ethylene suberate).
Claim 11
Dependent Claim 167 words
An electrographic liquid developer composition comprising a mixture of electrostatically-attractable redispersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (i) present in an amount of from about 0.1 to about 3 weight percent of said developer composition, (ii) having a melting point within the range of from about 60° to about 100° C. and (iii) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear crystalline polyester physically inert with respect to said carrier liquid, said polyester having the formula ##STR9## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; R and R 2 , which may be the same or different, represent a divalent residue of a aromatic diol; and R 1 and R 3 , which may be the same or different, represent a divalent residue of a sulfonamido-free aliphatic dicarboxylic acid.
Claim 12
Dependent Claim 167 words
An electrographic liquid developer composition comprising a mixture of electrostatically-attractable redispersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (i) present in an amount of from about 0.1 to about 3 weight percent of said developer composition, (ii) having a melting point within the range of from about 60° to about 100° C. and (iii) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear crystalline polyester physically inert with respect to said carrier liquid, said polyester having the formula ##STR9## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; R and R 2 , which may be the same or different, represent a divalent residue of a aromatic diol; and R 1 and R 3 , which may be the same or different, represent a divalent residue of a sulfonamido-free aliphatic dicarboxylic acid.
Claim 13
Dependent Claim 176 words
An electrographic liquid developer composition comprising a mixture of electrostatically-attractable redisersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (i) present in an amount of from about 0.1 to about 3 weight percent of said developer composition, (ii) having a melting point within the range of from about 60° to about 100° C, and (iii) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear polyester physically inert with respect to said carrier liquid, said polyester having the formula ##STR10## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; R and R 2 , which may be the same or different, represent a divalent residue of an alkylene glycol upon removal of the two hydroxy groups from said glycol and R 1 and R 3 , which may be the same or different, represent the divalent residue of a sulfonamido-free aliphatic dicarboxylic acid.
Claim 14
Dependent Claim 176 words
An electrographic liquid developer composition comprising a mixture of electrostatically-attractable redisersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (i) present in an amount of from about 0.1 to about 3 weight percent of said developer composition, (ii) having a melting point within the range of from about 60° to about 100° C, and (iii) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear polyester physically inert with respect to said carrier liquid, said polyester having the formula ##STR10## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; R and R 2 , which may be the same or different, represent a divalent residue of an alkylene glycol upon removal of the two hydroxy groups from said glycol and R 1 and R 3 , which may be the same or different, represent the divalent residue of a sulfonamido-free aliphatic dicarboxylic acid.
Claim 15
Dependent Claim 300 words
In an electrographic development process wherein an electrostatic charge pattern carried on a dielectric substrate is developed into a visible image by applying an electrographic liquid developer composition to said charge pattern, the improvement which comprises applying, as said liquid developer composition to said charge pattern, a composition comprising a mixture of electrostatically-attractable, heat-fixable redispersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (a) present in an amount of from about 0.05 to about 15 weight percent of said developer composition, (b) having a melting point in the range of from about 40° to about 150° C, and (c) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear polyester physically inert with respect to said carrier liquid, said polyester having the formula ##STR11## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; R and R 2 , which may be the same or different, represent a member of the group selected from the divalent residue of an aliphatic, alicyclic, or aromatic diol upon removal of the two hydroxy groups from said diol; R 1 is a member selected from the group consisting of the divalent residue of a sulfonamido-free aliphatic, alicyclic or aromatic dicarboxylic acid upon removal of the two carboxyl groups from said acid; and R 3 represents (i) a member selected from the same group as R 1 and may be the same as or different from R 1 or (ii) the divalent residue of a disulfonamido group-containing aromatic dicarboxylic acid upon removal of the two carboxyl groups from said acid, said disulfonamido group having a monovalent cation on the amido nitrogen atom thereof.
Claim 16
Dependent Claim 300 words
In an electrographic development process wherein an electrostatic charge pattern carried on a dielectric substrate is developed into a visible image by applying an electrographic liquid developer composition to said charge pattern, the improvement which comprises applying, as said liquid developer composition to said charge pattern, a composition comprising a mixture of electrostatically-attractable, heat-fixable redispersible toner particles in an electrically insulating liquid carrier having a volume resistivity greater than 10 10 ohm-cms. and a dielectric constant less than about 3.0, said toner particles (a) present in an amount of from about 0.05 to about 15 weight percent of said developer composition, (b) having a melting point in the range of from about 40° to about 150° C, and (c) comprising, in an amount greater than about 0.05 weight percent of said developer composition, a linear polyester physically inert with respect to said carrier liquid, said polyester having the formula ##STR11## wherein X represents a mole percentage value within the range of 0 to 100 mole percent; R and R 2 , which may be the same or different, represent a member of the group selected from the divalent residue of an aliphatic, alicyclic, or aromatic diol upon removal of the two hydroxy groups from said diol; R 1 is a member selected from the group consisting of the divalent residue of a sulfonamido-free aliphatic, alicyclic or aromatic dicarboxylic acid upon removal of the two carboxyl groups from said acid; and R 3 represents (i) a member selected from the same group as R 1 and may be the same as or different from R 1 or (ii) the divalent residue of a disulfonamido group-containing aromatic dicarboxylic acid upon removal of the two carboxyl groups from said acid, said disulfonamido group having a monovalent cation on the amido nitrogen atom thereof.

References Cited (Backward Citations)

US2899335A Cited
US3391014A Cited
US3590000A Cited
GB1266545A Cited
US3546180A Cited
US3557691A Cited
US3668127A Cited
US3856692A Cited
BE793247A Cited
US3826747A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-10-03 1981-04-04 1981-10-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-10-03 1985-04-04 1985-10-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-10-03 1989-04-04 1989-10-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag