Abstract
Abstract The invention relates to a controlled density fill material and a method of using such fill material in, for examples, the backfilling of sewers, embankments, structures and utility trenches. The material includes Portland cement, fly ash and aggregates. The material, while having some properties of both, is neither a soil nor a concrete.
Inventors
- 👤 William E. Brewer
- 👤 Franklin V. Zimmer
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 02:34
CPC Classifications
E; E02; E02D; E02D17/00; E02D17/18; C; C04; C04B; C04B18/00; C04B18/04; C04B18/06; C04B18/08; C04B2111/00; C04B2111/00474; C04B2111/00663; C04B2111/00706; Y; Y02; Y02W; Y02W30/00; Y02W30/50; Y02W30/91
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
106 words
A method of backfilling a conduit wherein the conduit is installed in a trench, the method comprising installing the conduit, placing controlled density fill material over the conduit without compacting such fill material, such controlled density fill material consisting essentially of 2% to 6% be weight of Portland cement, 2 to 10% by weight of flyash, 70 to 90% be weight of aggregate and 5 to 15 % by weight of water, the fill material being sufficiently placeable and flowable that tamping or vibrating is unnecessary and having a concrete comparison 28-day compressive strength of less than 1400 psi, whereby the material may be easily re-excavated.
Claim 2
Independent Claim
106 words
A method of backfilling a conduit wherein the conduit is installed in a trench, the method comprising installing the conduit, placing controlled density fill material over the conduit without compacting such fill material, such controlled density fill material consisting essentially of 2% to 6% be weight of Portland cement, 2 to 10% by weight of flyash, 70 to 90% be weight of aggregate and 5 to 15 % by weight of water, the fill material being sufficiently placeable and flowable that tamping or vibrating is unnecessary and having a concrete comparison 28-day compressive strength of less than 1400 psi, whereby the material may be easily re-excavated.
Claim 3
Dependent Claim
48 words
A method of backfilling according to claim 1, wherein the controlled density fill material consists essentially of 2 to 5% by weight of Portland cement, 2 to 9% by weight of fly ash, 74 to 86% by weight or aggregate and 8 to 13% by weight of water.
Claim 4
Dependent Claim
46 words
A method of backfilling a conduit, according to claim 1, wherein the controlled density fill material consists essentially or about 4% by weight of Portland cement about 2.6% by weight of fly ash, about 82.4% by weight of aggregate and about 11% be weight of water.
Claim 5
Dependent Claim
25 words
A method of back-filling according to claim 1, wherein such cured fill material has a 28-day compressive strength of between 100 psi and 300 psi.
Claim 6
Dependent Claim
26 words
A method of back-filling, according to claim 1, wherein said fly ash is finely divided fly ash which is collected by electrostatic precipitators or mechanical collectors.
References Cited (Backward Citations)
US2250107A
Cited
US2414734A
Cited
US2527766A
Cited
US2622989A
Cited
US2945769A
Cited
US3719511A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-09-26 | 1981-03-28 | 1981-09-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-09-26 | 1985-03-28 | 1985-09-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-09-26 | 1989-03-28 | 1989-09-27 | $7700.00 | Window Closed / Lapsed |