Abstract

Abstract Disclosed herein are rubber modified fire retardant polymer compositions based on interpolymers of styrene, maleic anhydride and a brominated monomer such as tribromophenyl acrylate, which have been formulated with various additives. These compositions, which have a UL-94 rating of at least V-1, are especially useful for use in radio and T.V. cabinets, furniture, appliance housings and other similar applications.

Inventors

  • 👤 Yoon C. Lee

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 23:09
CPC Classifications
C; C08; C08K; C08K3/00; C08K3/18; C08K3/20; C08K3/22; C08K3/2279; C08K3/01; C08K3/016

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 206 words
A composition of matter comprising: A. from 48 to 94 percent by weight based on the total weight of the molding composition of a polyblend of: a. a matrix polymer of 1. from 55 to 85 percent by weight of a styrene monomer; 2. from 5 to 25 percent by weight of a maleic anhydride monomer; and 3. from 10 to 20 percent by weight of a brominated monomer selected from the group consisting of bromophenyl acrylates, bromophenyl methacrylates, bromoneopentyl acrylate and bromoneopentyl methacrylates with the proviso that the amount of bromine in the polymer is at least 6 percent by weight and b. a rubber component wherein the amount of rubber in the polyblend is in the range of from 1 to 30 percent by weight based on the weight of the polyblend; B. from 3 to 12 percent by weight based on the total weight of the molding composition of a metal oxide; C. from 3 to 25 percent by weight based on the total weight of the molding composition of a smoke suppressant which is selected from the group consisting of smoke suppressing hydrates, carbonates and borates, and D. from 0 to 15 percent by weight of a brominated aromatic fire retardant additive.
Claim 2
Dependent Claim 206 words
A composition of matter comprising: A. from 48 to 94 percent by weight based on the total weight of the molding composition of a polyblend of: a. a matrix polymer of 1. from 55 to 85 percent by weight of a styrene monomer; 2. from 5 to 25 percent by weight of a maleic anhydride monomer; and 3. from 10 to 20 percent by weight of a brominated monomer selected from the group consisting of bromophenyl acrylates, bromophenyl methacrylates, bromoneopentyl acrylate and bromoneopentyl methacrylates with the proviso that the amount of bromine in the polymer is at least 6 percent by weight and b. a rubber component wherein the amount of rubber in the polyblend is in the range of from 1 to 30 percent by weight based on the weight of the polyblend; B. from 3 to 12 percent by weight based on the total weight of the molding composition of a metal oxide; C. from 3 to 25 percent by weight based on the total weight of the molding composition of a smoke suppressant which is selected from the group consisting of smoke suppressing hydrates, carbonates and borates, and D. from 0 to 15 percent by weight of a brominated aromatic fire retardant additive.
Claim 3
Dependent Claim 24 words
A composition of matter as in claim 1 wherein the styrene monomer is selected from the group consisting of styrene, alpha-methyl styrene or chlorostyrene.
Claim 4
Dependent Claim 16 words
A composition of matter as in claim 2 wherein the brominated monomer contains three bromine atoms.
Claim 5
Dependent Claim 15 words
A composition of matter as in claim 2 wherein the brominated monomer is tribromophenyl acrylate.
Claim 6
Dependent Claim 15 words
A composition of matter as in claim 2 wherein the brominated monomer is tribromoneopentyl methacrylate.
Claim 7
Dependent Claim 15 words
A composition of matter as in claim 1 wherein the metal oxide is antimony oxide.
Claim 8
Dependent Claim 37 words
A composition of matter as in claim 1 wherein the smoke suppressant is selected from the group consisting of magnesium carbonate, dawsonite, and mixtures thereof wherein the ratio of magnesium carbonate to dawsonite is at least 1:1.
Claim 9
Dependent Claim 25 words
A composition of matter as in claim 1 which further contains from 3 to 12 percent by weight of a brominated aromatic fire retardant additive.
Claim 10
Dependent Claim 28 words
A composition of matter as in claim 1 wherein the rubber component is a chlorinated rubber selected from the group consisting of polyepichlorohydrin, polychloroprene and chlorinated polyethylene rubbers.
Claim 11
Dependent Claim 256 words
A composition of matter comprising: A. from 61 to 90 percent by weight based on the total weight of the molding composition of a polyblend of: a. a matrix polymer of 1. from 60 to 83 percent by weight of a styrene monomer selected from the group consisting of styrene, alpha-methyl styrene or chlorostyrene and mixtures thereof; 2. from 7 to 20 percent by weight of a maleic anhydride monomer; and 3. from 10 to 20 percent by weight of a brominated monomer selected from the group consisting of tribromophenyl acrylate, tribromophenyl methacrylate, tribromoneopentyl acrylate and tribromoneopentyl methacrylate, with the proviso that the amount of bromine in the polymer is at least 6 percent by weight; and b. a rubber component wherein the amoung of rubber in the polyblend is in the range of from 5 to 20 percent by weight based on the weight of the polyblend and is a chlorinated rubber selected from the group consisting of polyepichlorohydrin, polychloroprene and chlorinated polyethylene rubbers; B. from 4 to 12 percent by weight based on the total weight of the molding composition of brominated aromatic fire retardant additive; C. from 3 to 12 percent by weight based on the total weight of the molding composition of antimony oxide; and D. from 3 to 15 percent by weight based on the total weight of the molding composition of a smoke suppressant which is selected from the group consisting of magnesium carbonate, dawsonite and mixtures thereof wherein the ratio of magnesium carbonate to dawsonite is at least 1:1.
Claim 12
Dependent Claim 256 words
A composition of matter comprising: A. from 61 to 90 percent by weight based on the total weight of the molding composition of a polyblend of: a. a matrix polymer of 1. from 60 to 83 percent by weight of a styrene monomer selected from the group consisting of styrene, alpha-methyl styrene or chlorostyrene and mixtures thereof; 2. from 7 to 20 percent by weight of a maleic anhydride monomer; and 3. from 10 to 20 percent by weight of a brominated monomer selected from the group consisting of tribromophenyl acrylate, tribromophenyl methacrylate, tribromoneopentyl acrylate and tribromoneopentyl methacrylate, with the proviso that the amount of bromine in the polymer is at least 6 percent by weight; and b. a rubber component wherein the amoung of rubber in the polyblend is in the range of from 5 to 20 percent by weight based on the weight of the polyblend and is a chlorinated rubber selected from the group consisting of polyepichlorohydrin, polychloroprene and chlorinated polyethylene rubbers; B. from 4 to 12 percent by weight based on the total weight of the molding composition of brominated aromatic fire retardant additive; C. from 3 to 12 percent by weight based on the total weight of the molding composition of antimony oxide; and D. from 3 to 15 percent by weight based on the total weight of the molding composition of a smoke suppressant which is selected from the group consisting of magnesium carbonate, dawsonite and mixtures thereof wherein the ratio of magnesium carbonate to dawsonite is at least 1:1.

References Cited (Backward Citations)

US2894926A Cited
US3766249A Cited
GB1402958A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-09-12 1981-03-14 1981-09-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-09-12 1985-03-14 1985-09-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-09-12 1989-03-14 1989-09-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag