Process for forming an electrically insulating seal between a metal lead and a metal cover

Assignee: GTE Sylvania Inc
•
Filing: 1976-11-19
•
Granted: 1977-09-13
•
Expires: 1996-11-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A metal body, for example, a cover for hermetically sealed electrochemical cells, is relatively flexible and electrically conductive. An aperture is provided within the body to receive an electrically insulating material, such as glass, which mounts a terminal or metal lead, for the cell. In the process for producing the seal, the body is positioned with the lead therein and a sealing glass is placed thereabout. The assembly is fired at a temperature high enough to achieve melting of said sealing glass and effecting a between the body, lead and glass to form a glass-to-metal seal. At least one surface of the lead is then ground to be flush with the glass and then the assembly is refired to heal cracks formed in the glass by the grinding operation.

Inventors

  • 👤 Paul C. Shaffer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 08:39
CPC Classifications
H; H01; H01B; H01B17/00; H01B17/26; H01B17/30; H01B17/303; H01B17/305; H01M; H01M50/00; H01M50/10; H01M50/183; H01M50/186; H01M50/19; H01M50/191; Y; Y02; Y02E; Y02E60/00; Y02E60/10; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49204; Y10T29/49208; Y10T29/4921; Y10T29/49211

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 94 words
A process for producing a glass-to-metal seal in an apertured metal body which comprises the steps of: positioning said apertured metal body; positioning a metal lead substantially centrally located within said aperture; placing a sealing glass in said aperture; firing said body, lead and sealing glass at a temperature high enough to achieve melting of said sealing glass and effecting a bond between said body, said lead and said glass to form said glass-to-metal; grinding at least one surface of said lead flush with said glass; and refiring said body and said glass-to-metal seal.
Claim 2
Dependent Claim 94 words
A process for producing a glass-to-metal seal in an apertured metal body which comprises the steps of: positioning said apertured metal body; positioning a metal lead substantially centrally located within said aperture; placing a sealing glass in said aperture; firing said body, lead and sealing glass at a temperature high enough to achieve melting of said sealing glass and effecting a bond between said body, said lead and said glass to form said glass-to-metal; grinding at least one surface of said lead flush with said glass; and refiring said body and said glass-to-metal seal.
Claim 3
Dependent Claim 18 words
The process of claim 1 wherein said firing is accomplished at a temperature of at least 800° C.
Claim 4
Dependent Claim 18 words
The process of claim 2 wherein said refiring is accomplished at a temperature of at least 750° C.
Claim 5
Dependent Claim 24 words
The process of claim 3 wherein said refiring is for a time long enough to heal cracks formed in said seal by said grinding.

References Cited (Backward Citations)

CA807605A Cited
US2898668A Cited
US3083249A Cited
US3225132A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-09-12 1981-03-14 1981-09-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-09-12 1985-03-14 1985-09-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-09-12 1989-03-14 1989-09-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag