Abstract

Abstract Articles of aluminium or aluminium alloys are pickled by placing them as anodes into a sulfuric acid bath containing no chromic acid or bichromate and connecting them by an electrical circuit including a D.C. potential source to a suitable cathode placed in the same bath, then imposing a certain control voltage from the potential source onto the anode and maintaining the resulting anode voltage at a substantially constant level during the whole pickling period. Means may be provided for continuously measuring the anode voltage and re-adjusting it to keep the voltage constant.

Inventors

  • 👤 Paul Frederik A. Bijlmer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 08:00
CPC Classifications
C; C25; C25F; C25F1/00; C25F1/02; C25F1/04; C25F7/00

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 135 words
The method of pickling aluminum articles which comprises the steps of: a. providing a pickling bath containing sulfuric acid without any chromic acid or bichromate oxidizing agent; b. positioning the aluminum article in the bath of step (a) and measuring the potential between said article and the bath; c. imposing a control voltage between said article and a cathode positioned in said bath in spaced relation to the article, said control voltage having a value at least sufficient to raise the potential of said article near to zero volts but said control voltage having a value less than 1 volt; d. maintaining said control voltage substantially constant for a time sufficient to produce microscopic pits of about 200μ in diameter in the surface of said article; and then e. recovering said article from the bath.
Claim 2
Independent Claim 135 words
The method of pickling aluminum articles which comprises the steps of: a. providing a pickling bath containing sulfuric acid without any chromic acid or bichromate oxidizing agent; b. positioning the aluminum article in the bath of step (a) and measuring the potential between said article and the bath; c. imposing a control voltage between said article and a cathode positioned in said bath in spaced relation to the article, said control voltage having a value at least sufficient to raise the potential of said article near to zero volts but said control voltage having a value less than 1 volt; d. maintaining said control voltage substantially constant for a time sufficient to produce microscopic pits of about 200μ in diameter in the surface of said article; and then e. recovering said article from the bath.
Claim 3
Dependent Claim 29 words
The method as defined in claim 1 wherein the control voltage imposed in step (c) establishes the potential of the article at a value of from -100 to +200mV.
Claim 4
Dependent Claim 23 words
The method as defined in claim 2 wherein the bath of step (a) contains sulfuric acid in concentration of 100-300 grams per liter.
Claim 5
Dependent Claim 21 words
The method as defined in claim 3 wherein the bath of step (a) is maintained at a temperature of 50°-60° C.
Claim 6
Dependent Claim 16 words
The method as defined in claim 4 wherein the time of step (d) is 10-30 minutes.
Claim 7
Dependent Claim 15 words
The process as claimed in claim 1, wherein said article is an aluminium alloy article.
Claim 8
Dependent Claim 22 words
The process as claimed in claim 1, wherein said article is an article of aluminium-copper alloy coated with a layer of aluminium.
Claim 9
Dependent Claim 37 words
The process as claimed in claim 1, wherein step d) is effected by continuously measuring the resulting voltage between said anode and said pickling bath and re-adjusting said voltage where necessary by means of said control voltage.

References Cited (Backward Citations)

US2040618A Cited
US3694334A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-08-15 1981-02-14 1981-08-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-08-15 1985-02-14 1985-08-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-08-15 1989-02-14 1989-08-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag